Thin films of beryllium and gold that are several tens of nanometers thick were obtained, for the first time, on silicon and quartz substrates by the ion-beam method with tenfold alternation of deposition and partial sputtering of the nanosized metal layer. Scanning electron and atomic force microscopy indicate the predominant lateral growth of nanosized metal layers along the substrate surface. Optical spectra indicate the suppression of the localized plasmon resonance. The growth of the film occurs under the influence of the high-energy component of the sputtered metal atoms’ flux. The main role in the formation of the nanosized metal film is played by the processes of the elastic collision of incident metal atoms with the atoms of a substrate and a growing metal film. Metal films that are obtained by the tenfold application of the deposition–sputtering of a nanoscale metal layer are characterized by stronger adhesion to the substrate and have better morphological, electrical, and optical characteristics than those that are obtained by means of direct single deposition.
1 September 2019 in Journal of Magnetism and Magnetic Materials
Magnetoelectric properties of layered heterostructures (FM/PZT/FM) n (n≤ 3) obtained by ion-beam sputtering deposition of ferromagnetic metal (FM), where FM is the cobalt (Co) or permalloy Ni78Fe22, onto ferroelectric ceramic based on lead zirconate titanate (PZT) have been studied. The polished ferroelectric plates in thickness from 400 to 20 μm were subjected to finished treatment by ion-beam sputtering. After plasma activation they were covered by the ferromagnetic films from 1 to 6 μm in thickness. Enhanced characteristics of these structures were reached by means of both the thickness optimization of ferroelectric and ferromagnetic layers and obtaining of ferromagnetic/ferroelectric interfaces being free from defects and foreign impurities. Assuming on the basis of analysis of elastic stresses in the ferromagnetic film that the magnetoelectric effect forms within ferromagnetic/ferroelectric interface, the structures with 2–3 ferromagnetic layers were obtained. In layered heterostructure (Py/PZT/Py)3, the optimal thickness of ferromagnetic film was 2 μm, and outer and inner ferroelectric layers had 20 μm and 80 μm in thickness, respectively. For such structure the maximal magnetoelectric voltage coefficient of 250 mV/(cm Oe) was reached at a frequency 100 Hz in magnetic field of 0.25 T at room temperature. The structures studied can serve as energy-independent elements detecting the change of magnetic or electric fields in electronic devices based on magnetoelectric effect.