The air void content is one of the most important volumetric properties of asphalt matrixes, such as asphalt mixtures or mortars, because it can greatly affect the performance of the matrix. At the mixture level, there are standardized methods for measuring the air void content, which is an important design parameter of a mixture. However, at the mortar scale, no unified method has been proposed to determine the air void content corresponding to the asphalt mixture. Therefore, this research aims to, first, characterize the air void distribution within the mortar of an asphalt mixture and then develop an updated theoretical method for calculating the air void content of asphalt mortar. The internal structures of air voids from three commonly used asphalt mixtures with different gradations were captured using an industrial CT scanning technique and then morphologically characterized using the image analysis method. Three-dimensional models of the air voids were reconstructed, and the air void content calculated from the CT images was also verified by density tests. The scanning results show that the air void content and air void size fit the cumulative Weibull curve. The results show that the nominal maximum particle size (NMPS) of mortar and the mixture air void content were the main parameters that affected the mortar’s air voids. The mortar air void content had linear relationships with both the mixture air void content and the mixture asphalt aggregate ratio. The mortar air void content was more sensitive to the NMPS of the asphalt mixture compared with the air void content or asphalt aggregate ratio of the mixture. This research provides a quantitative method to calculate the air void content of asphalt mortar within a mixture, which may help in the matrix design of mortar.
The strength growth of a bitumen emulsion-based cold in-place recycling asphalt mixture (BE-CIR) is time-dependent and time-consuming due to the addition of water. There is a great difference between the curing conditions of specification in the laboratory and the in situ conditions, which often leads to a great discrepancy between the results of lab specimens and the field cores. The main objective of this paper is to evaluate the curing effect on laboratory BE-CIR considering field-water evaporation and heat-transfer conditions. Four different curing methods were designed by using different combinations of waterproof layers, heat insulation layers, and variable temperature modes. The variations in temperature indexes, moisture content, air void, and indirect tensile strength (ITS) with curing time were tested, and the mutual influence of these indicators was analyzed. Furthermore, the results of the laboratory samples were compared with the field cores. Testing results show that the performance of the BE-CIR mixture is significantly different from that with no treatment, which is manifested as higher moisture content and lower air void and ITS under the same curing time. The internal temperature of the mixture is the main factor affecting the variation of moisture content, especially on the first curing day. The air void of the mixture has a strong linear relationship with the moisture content. Moisture content and ITS under different curing methods showed similar trends and could be divided into two stages. Taking the field cores as a benchmark, it can be concluded that the field-water evaporation condition should be considered in the setting of indoor curing methods, while the heat transfer could not.
Cracking is one of the main distresses in asphalt pavement. At present, few studies have been conducted on the cracking performance of asphalt mixtures from the field due to the difficulty of sample collection. Therefore, this study aims to assess the cracking resistance of in-service asphalt pavement at intermediate temperature using a large number of field cores in Jiangsu province, China. A semi-circular bending (SCB) test at 25 °C was conducted on field-cored samples covering three asphalt layers from 16 in-service road sections that represent a combination of influencing factors, including air void, mixture type, service age, cumulative number of equivalent single-axle loads (ESALs), and overload rate. The flexibility index (FI) and tensile strength were calculated from the experimental data as cracking performance evaluation indices. According to the analysis of variance results, at the top layer, ESALs and service age had a strong influence on cracking resistance. The decline rate of FI became slower with increasing ESALs. The most rapid decline in crack resistance with service age occurred on medium-traffic-level sections that served for over 14 years. At the middle layer, the overload rate replaced service age as a significant factor for FI. At the bottom layer, the air void was the only significant factor affecting the cracking resistance. In general, as the depth of layer increased, the effect of traffic load and service age decreased, whereas the effect of material properties increased. In addition, the FI and tensile strength were more sensitive to traffic load and air void, respectively.
To better reveal the performance development of bitumen emulsion-based cold in-place recycling (BE-CIR) mixture over curing, a semi-sealed laboratory curing method was proposed in this research to simulate the in situ moisture evaporation process and cracking resistance of the BE-CIR specimen at different depths during a curing time of 28 days, which was also investigated by the semi-circular bending (SCB) test. The influencing factors of cement content (1.5% to 2.5%), initial moisture content (3.5% to 4.5%), curing temperature (25 °C to 45 °C) and relative humidity were investigated, and the significance of different factors affecting the performance development was also analyzed. The results indicate significant variations in cracking performance parameters at different depths, with the top part exhibiting notably higher tensile strength and fracture energy compared to the bottom part, and a gradient index (GI) is proposed to describe the difference. Cement content affected early tensile strength and fracture energy, while the initial moisture content affected the development rate of the performance. The influence of curing temperature was extensive, and as the temperature increased beyond 40 °C, the strength of the effect decreased. High humidity during the early stage of curing inhibited the strength formation and development of fracture energy. The performance development of the BE-CIR mixture is more significantly influenced by the moisture migration process, which is governed by curing temperature and relative humidity, as opposed to the cement content and initial moisture content.