Edoardo Zonta

Mr. Edoardo Zonta

Department of industrial engineering, University of Trento, Trento, Trentino-Alto Adige, Italy
orcid

Research Focus & Metrics

Academic Career Length

7Years (2020-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
24 October 2020 in Polymer Engineering & Science
Verified
Journal Article
Closed access
PDF file
EZEdoardo Zonta
Edoardo Zonta
FVFrancesco Valentini
Francesco Valentini
ADAndrea Dorigato
Andrea Dorigato
LFLuca Fambri
Luca Fambri
Alessandro PegorettiAlessandro Pegoretti
Alessandro Pegoretti

16 June 2023 in Molecules
Verified
Journal Article
Open access
PDF file
Giulia FrediGiulia Fredi
Giulia Fredi
EZEdoardo Zonta
Edoardo Zonta
ADAlessandro Dussin
Alessandro Dussin
Dimitrios BikiarisDimitrios Bikiaris
Dimitrios Bikiaris
George Z. PapageorgiouGeorge Z. Papageorgiou
George Z. Papageorgiou
Andrea DorigatoAndrea Dorigato
Andrea Dorigato
This work presents the successful preparation and characterization of polylactide/poly(propylene 2,5-furandicarboxylate) (PLA/PPF) and polylactide/poly(butylene 2,5-furandicarboxylate) (PLA/PBF) blends in form of bulk and fiber samples and investigates the influence of poly(alkylene furanoate) (PAF) concentration (0 to 20 wt%) and compatibilization on the physical, thermal, and mechanical properties. Both blend types, although immiscible, are successfully compatibilized by Joncryl (J), which improves the interfacial adhesion and reduces the size of PPF and PBF domains. Mechanical tests on bulk samples show that only PBF is able to effectively toughen PLA, as PLA/PBF blends with 5–10 wt% PBF showed a distinct yield point, remarkable necking propagation, and increased strain at break (up to 55%), while PPF did not show significant plasticizing effects. The toughening ability of PBF is attributed to its lower glass transition temperature and greater toughness than PPF. For fiber samples, increasing the PPF and PBF amount improves the elastic modulus and mechanical strength, particularly for PBF-containing fibers collected at higher take-up speeds. Remarkably, in fiber samples, plasticizing effects are observed for both PPF and PBF, with significantly higher strain at break values compared to neat PLA (up to 455%), likely due to a further microstructural homogenization, enhanced compatibility, and load transfer between PLA and PAF phases following the fiber spinning process. SEM analysis confirms the deformation of PPF domains, which is probably due to a “plastic–rubber” transition during tensile testing. The orientation and possible crystallization of PPF and PBF domains contribute to increased tensile strength and elastic modulus. This work showcases the potential of PPF and PBF in tailoring the thermo-mechanical properties of PLA in both bulk and fiber forms, expanding their applications in the packaging and textile industry.

29 January 2026 in ACS Omega
Verified
Journal Article
Open access
EZEdoardo Zonta
Edoardo Zonta
KCKatherine Giselle Benavides Cabrera
Katherine Giselle Benavides Cabrera
Andrea DorigatoAndrea Dorigato
Andrea Dorigato
Giulia FrediGiulia Fredi
Giulia Fredi
This work reports a novel, green, and scalable wet mixing approach to prepare bacterial cellulose (BC)/poly­(vinyl alcohol) (PVA)/chitosan (CH) composite films with precise control over barrier, mechanical, and antimicrobial properties, suitable for active food packaging. The resulting composites exhibit tunable water interaction, ultraviolet (UV) barrier, and mechanical properties dictated by the BC/PVA ratio. Increasing BC content reduces the water uptake, water solubility, water vapor permeability, and UV transmittance (60 wt %) introduces interfacial defects limiting deformability. Soil burial tests demonstrated composition-dependent biodegradation, reaching a weight loss higher than 30 wt % after 15 days. Incorporation of CH (5 wt %) improves film homogeneity and imparts antimicrobial activity, effectively extending strawberry shelf life. This processing method eliminates harsh solvents while enabling precise compositional control, yielding renewable films with composition-dependent performance for sustainable packaging applications.

29 October 2026 in Journal of Composites Science
Verified
Journal Article
Open access
PDF file
MPMarco Papparotto
Marco Papparotto
RMRoberto Miani
Roberto Miani
Pavel SolovyevPavel Solovyev
Pavel Solovyev
EZEdoardo Zonta
Edoardo Zonta
ASAlessandro Sorze
Alessandro Sorze
Giulia FrediGiulia Fredi
Giulia Fredi
Anionic polyamide 6 (aPA6) thermoplastic composites are known for their excellent mechanical and functional properties, including high strength, toughness, good processability, and gas-barrier capabilities. However, when exposed to the environment, they seem to lack proper mechanisms to resist degradation from radiation and atmospheric agents. For this reason, in this paper, the incorporation of a microscopic bio-based sulfonated lignin filler was investigated, aiming to improve UV shielding properties, which are expected to prolong the life cycle of the material and to decrease microplastic formation with extensive environmental benefits. In this work, anionic ring-opening polymerization (AROP) of ε-caprolactam (CL) was employed for the first time to produce aPA6/lignin microcomposites containing up to 5 wt% lignin in a simple in situ one-pot process. A marked increase in attenuation coefficient was observed in the UV range, up to 894% at 346 nm. Nuclear magnetic resonance (NMR) and microscopic characterization excluded chemical bonding between biofiller and matrix, resulting in a moderate decrease in mechanical performance (−21.4% in yield strength and −16.3% in stress at break). However, the absence of lignin–PA6 hybrids may be beneficial to the recyclability of the material. Overall, this study proved the benefits of introducing a widely available and environmentally friendly filler into recyclable high-performance composite materials, imparting further functional properties and anticipating novel applications.