MnO2 has shown great potential in the field of adsorption and has a good adsorption effect on heavy metal ions in aqueous solution, but there have been problems in the adsorption of heavy metal ions in high-concentration metal salt solutions. In this paper, different crystal forms of MnO2 (α-MnO2, β-MnO2, γ-MnO2, δ1-MnO2, δ2-MnO2, and ε-MnO2) were prepared and characterized by XRD, SEM, EDS, XPS, ZETA, and FT-IR. The reasons for the equi-acidity point pH change of MnO2 and the complex mechanism of surface hydroxylation on metal ions were discussed. The results showed that the equi-acidity point pHs of different crystalline MnO2 were different. The equi-acidity point pH decreased with the increase of reaction temperature and electrolyte concentration, but the reaction time had no effect on it. The equi-acidity point pHs of MnO2 were essentially equal to the equilibrium pH values of adsorption and desorption between surface hydroxyl and metal ions on them. The change of equi-acidity points was mainly due to the complexation of surface hydroxyl, and the equi-acidity point pHs depended on the content of surface hydroxyl and the size of the complexation ability. According to the equi-acidity point pH characteristics of MnO2, more hydroxyl groups could participate in the complexation reaction by repeatedly controlling the pH, so that MnO2 could adsorb heavy metals Co2+ and Ni2+ in high-concentration MnSO4 solution, and the adsorption rates of Co2+ and Ni2+ could reach 96.55 and 79.73%, respectively. The effects of MnO2 dosage and Mn2+ concentration on the adsorption performance were further investigated, and the products after MnO2 adsorption were analyzed by EDS and FT-IR. A new process for MnO2 to adsorb heavy metals Co2+ and Ni2+ in high-concentration MnSO4 solution was explored, which provided a reference for the deep purification of manganese sulfate solutions.
The recovery of valuable metals from spent lithium-ion batteries is beneficial to protect the environment and avoid resource depletion. Based on the synergistic effect of the reducing ability of oxalic acid and the acidic strength of sulfuric acid, this study was conducted to recover valuable metals from spent LiNi0.8Co0.1Mn0.1O2 lithium-ion battery cathode materials with the compound leaching agents of sulfuric acid and oxalic acid. Under the optimized conditions of sulfuric acid concentration at 2.5 mol·L−1, oxalic acid concentration at 20 g·L−1, liquid-to-solid ratio at 10 mL·g−1, reaction temperature at 85 °C, and reaction time at 100 min, the leaching rate of Li, Ni, Co, and Mn measured by ICP-OES was, respectively, 99.26%, 98.41%, 96.95%, and 97.54%. It was further validated that the valuable metals were almost completely leached when combined with the XRD and SEM-EDS analysis of spent cathode materials before and after leaching. The leaching of Li, Ni, Co, and Mn was all in accordance with the Avrami model with their activation energies of 31.96 kJ·mol−1, 41.01 kJ·mol−1, 47.57 kJ·mol−1, and 42.95 kJ·mol−1, indicating that the diffusion was the control of the Li leaching process, and the surface chemical reaction was the control of the other three metals. This work provides a new idea and method for the recycling of spent lithium-ion batteries.
Sodium-ion batteries have important application prospects in large-scale energy storage due to their advantages, such as safety, affordability, and abundant resources. Prussian blue analogs (PBAs) have a stable and open framework structure, making them a very promising cathode material. However, high-performance manganese-based Prussian blue cathode materials for sodium-ion batteries still suffer from significant challenges due to several key issues, such as a high number of vacancy defects and a high crystal water content. This article investigates the effects of the Fe-Mn molar ratio, Mn ion concentration, and reaction time on the electrochemical performance of MnHCF during the coprecipitation process. When Fe:Mn = 1:2, c(Mn2+) = 0.02 mol/L, and the reaction time is 12 h, the content of interstitial water molecules in the sample is low, and the Fe(CN)6 defects are few. At 0.1 C, the prepared electrode has a high initial discharge specific capacity (121.9 mAh g−1), and after 100 cycles at 0.2 C, the capacity retention rate is 65% (~76.2 mAh g−1). Meanwhile, the sample electrode exhibits excellent reversibility. The discharge capacity can still be maintained at around 75% when the magnification is restored from 5 C to 0.1 C. The improvement in performance is mainly attributed to two aspects: On the one hand, reducing the Fe(CN)6 defects and crystal water content is conducive to the diffusion and stable structure of N. On the other hand, reducing the reaction rate can significantly delay the crystallization of materials and optimize the nucleation process.
LiMn2O4, a significant cathode material for lithium-ion batteries, has garnered considerable attention due to its low cost and environmental friendliness. However, its widespread application is constrained by its rapid capacity degradation and short cycle life at elevated temperatures. To enhance the electrochemical performance of LiMn2O4, we employed a liquid-phase co-precipitation and calcination method to incorporate Cr3+ into the LiMn2O4 cathode material, successfully synthesizing a series of LiCrxMn2−xO4 (x = 0~0.06). The prepared Cr-doped samples exhibited an excellent spinel structure and a unique truncated octahedral morphology. Additionally, the substitution of Mn3+ in LiMn2O4 by Cr3+, coupled with the significantly higher Cr-O bond energy compared to Mn-O bond energy, enhanced the stability of the crystal structure and inhibited the Jahn–Teller effect. Experimental results demonstrated that the optimized LiCr0.04Mn1.96O4 displayed superior electrochemical performance, with a capacity retention rate of 93.24% after 500 cycles under a 0.5C current density; even at 50 °C, the capacity retention rate remained at 86.46% after 350 cycles under a 0.5C current density. The polyhedral morphology formed by Cr doping in LiMn2O4 offers an effective approach to achieving high-performance LiMn2O4 cathode materials.
The structure of Mn3O4 with an octahedron structure was similar to that of LiMn2O4, and the lithium manganate prepared with it had good electrochemical performance. During the preparation of octahedron Mn3O4, the effects of the pH regulator, temperature, and reaction pH on its morphology, specific surface area, and other properties were studied in this paper. LiMn2O4 was prepared from Octahedron Mn3O4 obtained by using better technology. The effects of calcination time and temperature on the physicochemical and electrochemical properties of LiMn2O4 were studied. The research results indicated that the optimal synthesis conditions for Mn3O4 were as follows: ammonia water was used as a pH regulator and complexing agent, reaction pH was 8, reaction temperature was 80 °C, reaction time was 12 h, and oxygen flow rate was 3 L∙min−1. The LiMn2O4 synthesized had a good octahedron morphology when the calcination temperature was 800 °C and the calcination time was 10 h. The first discharge-specific capacity was 121.9 mAh∙g−1 at a current density of 0.2 C, the discharge-specific capacity was 114.1 mAh∙g−1 after 100 cycles, and the capacity retention rate was 93.6%. Therefore, the lithium manganate prepared by using octahedron manganous oxide had good electrochemical reversibility and a good application prospect.
28 August 2023 in Russian Journal of Electrochemistry
Manganese sulfate solution would be affected by various factors in electrolytic production of manganese. When different electrolysis time was controlled, the effects of current density on the growth law of cathode manganese, the current efficiency, cell voltage and energy consumption in the electrodeposition process were studied. The results showed that too low or too high current density was not conducive to the growth of manganese grains. When the current density was about 450 A/m2, the manganese grains grew uniformly with spherical morphology and the cathode manganese sheet had high density. The α-manganese with good crystallinity and high density was obtained after electrodeposition for 10 h. Under this current density, the current efficiency of manganese deposition was high, the cell voltage was stable, and the energy consumption was low. The average current efficiency was 71.656%, the cell voltage fluctuated between 3.89 and 3.95 V, and the average energy consumption was 5.33 kW h/kg.