LiMn2O4, a significant cathode material for lithium-ion batteries, has garnered considerable attention due to its low cost and environmental friendliness. However, its widespread application is constrained by its rapid capacity degradation and short cycle life at elevated temperatures. To enhance the electrochemical performance of LiMn2O4, we employed a liquid-phase co-precipitation and calcination method to incorporate Cr3+ into the LiMn2O4 cathode material, successfully synthesizing a series of LiCrxMn2−xO4 (x = 0~0.06). The prepared Cr-doped samples exhibited an excellent spinel structure and a unique truncated octahedral morphology. Additionally, the substitution of Mn3+ in LiMn2O4 by Cr3+, coupled with the significantly higher Cr-O bond energy compared to Mn-O bond energy, enhanced the stability of the crystal structure and inhibited the Jahn–Teller effect. Experimental results demonstrated that the optimized LiCr0.04Mn1.96O4 displayed superior electrochemical performance, with a capacity retention rate of 93.24% after 500 cycles under a 0.5C current density; even at 50 °C, the capacity retention rate remained at 86.46% after 350 cycles under a 0.5C current density. The polyhedral morphology formed by Cr doping in LiMn2O4 offers an effective approach to achieving high-performance LiMn2O4 cathode materials.
The P2-Na0.7MnO2.05 cathode material has long been constrained by phase transitions induced by the Jahn–Teller (J–T) effect during charge–discharge cycles, leading to suboptimal electrochemical performance. In this study, we employed a liquid phase co-precipitation method to incorporate Ti during the precursor Mn3O4 synthesis, followed by calcination to obtain Na0.7TixMn(1−x)O2.05 materials. We investigated the effects of Ti doping on the structure, morphology, Mn3+ concentration, and Na+ diffusion coefficients of Na0.7TixMn(1−x)O2.05. Our findings revealed that the 7% Ti-doped NTMO-007 sample exhibited reduced grain agglomeration and smaller particle sizes compared to the undoped sample, thereby enhancing the electrode–electrolyte contact area and electrochemical activity. Additionally, Ti doping increased the crystal cell volume of Na0.7MnO2.05 and broadened the Na+ transport channels, significantly enhancing the Na+ diffusion coefficient. At a 0.5 C rate, the NTMO-007 sample demonstrated a specific capacity of 143.3 mAh g−1 with an 81.8% capacity retention after 100 cycles, markedly outperforming the undoped NMO sample, which had a capacity retention of only 61.5%.