Commercially available formulations of the popular conductive polymer, poly(3,4-ethylenedioxythiophene):polystyrene sulfonate (PEDOT:PSS) are aqueous dispersions that require the addition of secondary dopants such as dimethyl sulphoxide (DMSO) or ethylene glycol (EG) for fabricated films to have the desired levels of conductivity. CleviosTM F HC Solar, a formulation of PEDOT:PSS produced by Heraeus, GmbH, achieves over 500 S/cm without these secondary dopants. This work studies whether secondary dopants such as DMSO have any additional effect on this type of PEDOT:PSS. The temperature dependencies of the conductivity of F HC Solar spin-coated thin films measured using a four-probe method seem to exhibit different charge transport properties compared with secondary doped PH1000. Observations made using atomic force microscopy (AFM) show that different concentrations of DMSO affect the orientation of the PEDOT domains in the thin film. These morphological changes cause room temperature conductivity to reduce from 640 S/cm in pristine films to as low as 555 S/cm after adding 7 wt% of DMSO along the film. Such tuning may prove useful in future applications of PEDOT:PSS, such as nanoprobes, transistors and hybrid solar cells.
Neutral-beam etching (NBE) provides a charge-free, low-damage approach for the dry processing of wide-bandgap semiconductors. By neutralizing plasma ions and precisely controlling bias power, NBE delivers reactive radicals without UV-induced damage or charging effects. We systematically compare the etching of GaN, AlGaN, and SiN under Cl2, Cl2/BCl3, and SF6 neutral beams. The gallium nitride (GaN) etch rate ranges from 25, while SF6 beams achieve SiN/GaN selectivity >675 at 10 W. Post-etch atomic force microscopy shows an rms roughness of 0.3–0.7 nm, in some cases smoother than as-grown surfaces. These results demonstrate that NBE combines high material selectivity with atomically smooth and reproducible profiles. The reduced defect density and stable etch depth directly benefit GaN high-electron-mobility transistor fabrication, enabling precise gate recesses and suppressing threshold-voltage shifts and gate leakage. Our findings establish NBE as a versatile tool for the next generation of GaN device processing.
PEDOT:PSS/Si hybrid photovoltaic cells have been attracting attention as a potential way to simplify the manufacturing process and democratize solar energy production. Control of the PEDOT/Si interface is also one of the primary ways to ensure the improved performance and lifetimes of multijunction devices, such as perovskite/Si tandem solar cells. In this work, the effects of the interfacial silicon oxide layer were investigated by creating a novel and controllable neutral beam oxide interlayer with different thicknesses. A novel self-doped PEDOT (S-PEDOT) was used to improve interfacial contact and avoid the secondary doping of PEDOT:PSS. X-ray photoelectron spectroscopy (XPS) showed that the saturation of interfacial silicon atoms in SiOx-Si bonds as well as a very thin, (~1 nm) damage-free oxide interlayer were the keys to maintaining good passivation with a high tunneling current. Lifetime measurements also showed that the interlayers with the most SiO2 content degraded the least. The degradation of the devices was due to the continued growth of the oxide layer through reactions with silicon sub-oxides and the degradation of S-PEDOT.
Pulsed-plasmas are widely used in semiconductor dry etching because of lower plasma-induced damage compared with continuous-wave (CW) operation. Notably, in electronegative gases such as Cl, significant amounts of negative ions form in the afterglow, producing an ion-ion plasma that enables the transport of low energy ions to the surface and thereby reducing defects of etch patterns. This work studies the impact of the chamber size on plasma loss characteristics and the resulting timescale for ion-ion plasma formation using time-resolved Langmuir probe measurements applied to plasma systems with two different diameters. Relative to the large diameter chamber, the small diameter chamber exhibited more than twice the radial electron diffusion loss and ion loss to the wall during the discharge. In the pulse-OFF phase, the plasma diffusion rates were ∼1.4 × 10 4 s − 1 and ∼2.9 × 10 3 s − 1 , demonstrating that chamber geometry strongly governs diffusion-driven losses and transient plasma behavior during upscaling. GaN etching revealed a chamber-size-dependent optimal OFF time: the etch rate peaked at 1.8 nm/min at 200 μs using the large diameter and 5.5 nm/min at 100 μs using the small diameter. These results provide practical guidance for pulse-OFF time optimization and establish a foundation for large diameter pulsed-plasma modeling toward mass manufacturing.