Numerous phenomena that occur during the process of machine parts’ regeneration have a significant impact on the loss of their working ability. Therefore, the properties of the working surfaces of the teeth flanks of repaired gears were analyzed in this research. The hereditary properties of the gear teeth are expressed by the interdependence of their geometric and physical-mechanical-metallurgical parameters created during the technological operations of regeneration of worn teeth by welding/hard-facing. The hard-facing was executed with three filler metal types, namely: combination Inox 18/8/6 + EDur 600, Castolin 2 and UTP 670. The tested properties included geometrical accuracy, microstructure and microhardness. Evaluation of the executed regeneration procedures was done by comparing the mentioned parameters of the regenerated gears and the new ones. The tested gears were not withdrawn from production due to damage, but they were newly manufactured and intentionally damaged gears, made of the same materials, subjected to the same manufacturing process. In this way, all influences except for the considered filler metal type were eliminated. Based on results of the conducted experiments, it was possible to establish the influence of the filler metal type on the surface characteristics of the regenerated gears’ teeth flanks.
The problems of a material selection for making the boiler pipes in a responsible steam plant and the technology for their welding are considered in this paper. The boiler is screened, complex, radiating energetic plant, with the natural water circulation in the hanging steel structure. Based on the legal regulations, the mandatory periodic reparation of the most important components is performed. This is why the check of mechanical properties, for the used and new materials for eventual replacement and building-in was done, as well as the check of the prescribed reparation procedures. The components that were in exploitation were checked, since their properties change with time. Checking consisted of testing the tensile material properties at room and elevated temperatures, measurements of hardness and analysis of materials’ microstructures. Besides the experimental tests, the numerical modeling and analysis of the workload of the fluid transporting pipes was conducted. In that way it was established which material is optimal for manufacturing the boiler pipes
Steel of the mild-strength S355J2+N steel grade is the most often used steel for manufacturing carrying sections of constructions exposed to fatigue loads. The use of high-strength steels, such as S690QL, allows for the creation of structures that are light and simple to construct. However, increasing the yield strength of high-strength steels does not result in a corresponding increase in fatigue resistance. As a result, using high-strength steels for constructions subjected to fatigue loading can be a major design concern, raising the question of whether high-strength steels should be used at all. Most of the experimental investigations regarding the hot work tool steel X37CrMoV5-1 found in the literature are focused on its machining and wear resistance, with insufficient attention paid to the cyclic loads. This article evaluates the fatigue properties of mild-strength S355J2+N, high-strength S690QL, and X37CrMoV5-1 steel grades. A SHIMADZU servo-hydraulic testing machine is used to perform uniaxial tensile tests under uniaxial fatigue stress-controlled, fully reversed conditions (tensile–compression testing with R = −1 stress ratio) in accordance with EN ISO and ASTM standards. The aim of this paper is to highlight the fatigue characteristics of these three steels that are among the most used in their respective groups. Steel S355J2+N belongs to the group of hot-rolled normalized steels, S690QL belongs to the group of improved (quenched + tempered) steels with increased strength, and X37CrMoV5-1 belongs to the group of high-alloyed tool steels for hot work. This choice was made as the tested steels can be considered typical representatives of their groups. Based on the test results of these three steels, which are organized in S–N curves, the fatigue behavior of the entire mentioned groups of steels can be foreseen.
12 September 2016 in Industrial Lubrication and Tribology
Purpose: The purpose of this study is to show which filler metal is the best for hard facing. Because the quality of the surface layer has a great influence on the working life of parts, the purpose was to extend the working life of parts exposed to intensive wear. The tested hard-faced models were made of low carbon steel to save the expensive base metal and to analyze the possibilities of extending the service life of existing structural parts. Design/methodology/approach: Samples were prepared from plates hard faced with various filler metals. Samples were then subjected to experimental testing – testing of tribological properties and hardness and microstructure. Testing was done in conditions similar to real ones – with a sliding speed of 0.25, 0.5 and 1 m/s and with a load of 50, 75 and 100 N and in most rigorous dry conditions. Research was done by using a combination of experimental and theoretical approaches. Findings: The paper shows the results of the experimental testing of four different filler metals aimed for hard facing of parts exposed to highly intensive wear. Results shown that CrWC 600 alloy is the most favorable filler metal for hard facing of parts such as those of construction mechanization and those subjected to intensive abrasive wear at stone mines. Practical implications: All obtained results are real and fully applicable, as there is a huge industrial need for these types of technologies. With the application of these technologies, beside money savings, the working life of parts can be significantly extended. Originality/value: The research presented in this paper was conducted because of the lack of results from this area in Serbia and because of the necessity for application of obtained results in companies for road maintenance and stone excavation in the region of Šumadija, Serbia.
Two aspects of various steels’ weldability are considered in this article. The theoretical part presents general concepts related to steel’s weldability and the application of the most important methods for its determination. In the experimental section, results of the hard-facing application to several samples are presented, and consist of hardness measurements in the different zones of the welded samples, with the evaluation of those zones’ microstructures. The tested materials included two carbon steels and two alloyed steels, with hard-facing layers deposited by various filler metals. Experimental results were compared to results obtained by calculations; using both, authors were able to conclude which combination of filler metal, welding procedure and, if necessary, heat treatment, would achieve the optimal improvement of weldability in welding/hard-facing of each of the tested base metals.