This research introduces low-temperature soldering of Ga with practical metallization structures, namely, Cu/Ni/Pd and Cu/Ni/Au, applied to contemporary microelectronic packages. Through these multilayer configurations, the study investigates the stability of the Ni diffusion barrier by examining changes in the interfacial microstructure as Ni is consumed. The interfacial reactions are conducted across a temperature spectrum of 160, 200, 240, and 280 °C, with reaction durations ranging from 30 to 270 min. Valuable insights for low-temperature soldering with Ga are extracted from the data. At lower reaction temperatures, the presence of Ga-rich intermetallic compounds (IMCs), specifically GaxNi (x = 89 to 95 at%), on the Ga7Ni3 layer is notably confirmed. As the reaction temperature and duration increase, the gradual consumption of the Ni layer occurs. This gives rise to the formation of Ga-Cu IMCs, specifically CuGa2 and γ3-Cu9Ga4, beneath the Ga-Ni IMC layer. Concurrently, the gap between the Ga-Ni and Ga-Cu IMC layers widens, allowing molten Ga to infiltrate. The rate of Ga7Ni3 growth follows a time exponent ranging approximately from 1.1 to 1.7. This highlights the significant influence of interface reaction-controlled kinetics on Ga7Ni3 IMC growth. The activation energy for Ga7Ni3 growth is determined to be 61.5 kJ/mol. The growth of Ga7Ni3 is believed to be primarily driven by the diffusion of Ga atoms along grain boundaries, with the porous microstructure inherent in the Ga7Ni3 layer providing additional diffusion pathways.
In this study, a novel composite solder, Sn-3.5Ag-10.0Co, was tailored for transient liquid phase (TLP) bonding in electric vehicle power module integration. Employing a meticulous two-step joining process, the solder joint was transformed into a robust microstructure characterized by two high-melting point intermetallic compounds, Ni3Sn4 and (Co,Ni)Sn2. After 1 h of TLP bonding, the Sn-3.5Ag-10.0Co paste transformed into the IMCs, but voids persisted between them, particularly between (Co,Ni)Sn2 and Ni3Sn4. Voids significantly reduced after 2 h of bonding, with full coalescence of the joint microstructure observed. The joint continued to be densified after 3 h of TLP bonding, but voids tended to accumulate at the joint center. Failure analysis revealed crack propagation through Ni3Sn4/(Co,Ni)Sn2 interfaces and internal voids. The engineered Sn-Ag-Co TLP joint exhibited superior shear strength retention even at an elevated temperature of 200 °C, contrasting with the significant reduction observed in the Sn-3.5Ag control specimen due to remaining Sn.