We aimed to investigate whether the collaboration of shear wave elastosonography (SWE) and B-mode ultrasonography (US) could be offered as diagnostic tools to assess the presence, severity, and progress of bruxism, as well as a biomarker for the effectiveness of treatment in daily clinical practice. The study was designed as a quantitative evaluation of the masseter muscles (MMs) of the clinically diagnosed bruxism patients suffering from myofascial pain and MMs of the healthy individuals. Clinical examinations were made according to the diagnostic criteria for temporomandibular disorders (DC/TMD), and pain was assessed using a visual analog scale (VAS). Painful MMs with VAS scores ≥ 4 were assigned to Group A, and healthy MMs were assigned to Group B. Also, the MMs of the painful bruxers were analyzed based on wearing occlusal splints. Group A was divided into two subgroups as splint users (Group AI) and non-users (Group AII). All the participants were scanned with dynamic US and SWE to quantify the size and stiffness of the MMs. Measurements of each muscle pair while the jaw is in a resting position (relaxation) and clenching position (contraction) were recorded. The significant differences in stiffness and thickness became visible in the relaxation state. Bruxism patients with myofascial pain had significantly harder and thinner MMs than healthy individuals. During the relaxation, the mean thickness and elasticity values were 9.17 ± 0.40 mm and 39.13 ± 4.52 kPa for Group A and 10.38 ± 0.27 and 27.73 ± 1.92 for Group B, respectively. Also, stiffer MMs were measured in Group AII (38.16 ± 3.61 kPa) than in Group AI (26.91 ± 2.13 kPa). In conclusion, the combination of SWE and US using a dynamic examination technique has the potential to be a valuable tool for the management of bruxism patients suffering from myofascial pain.
The aim was to compare different surface pretreatments on definitive resin crown materials manufactured additively or subtractively in terms of shear bond strength (SBS) values. Seven subgroups (n=10) were formed from additively manufactured VarseoSmile Crown Plus (VS) and subtractively manufactured Cerasmart270 blocks (CS) according to different surface pretreatments applied; sandblasting (subgroup SB), hydrofluoric acid (subgroup HF), Multi Primer (subgroup MP), subgroup SB-HF, subgroup SB-MP, subgroup SB-HF-MP, and control subgroup. A 3-mm-diameter composite was cemented onto each sample by self-adhesive resin cement. SBS values were measured and failure modes were analyzed after thermocycling. Data were analyzed with two-way ANOVA and Tukey HSD tests. The mean SBS value of VS was found significantly higher than CS (p<0.001). Subgroups SB-HF-MP, HF, SB-MP, and MP of VS exhibited the highest SBS values (p<0.001). The VS exhibited mostly cohesive failure, while CS exhibited mostly adhesive failure.