A systematic and comprehensive analysis of the hot deformation and mechanisms of SiC particle-reinforced aluminum matrix composites is significant for optimizing the processing of the composites and obtaining the desired components. Based on this, related research on 11 vol% SiCp particle-reinforced 7050Al matrix composites was carried out. Hot compression experiments were carried out on the Gleeble-3500 thermal simulator to study the hot deformation behavior of composites at the temperature of 370–520 °C and strain rate of 0.001–10 s−1. The hyperbolic sine constitutive equation of the material was established, and the processing map was calculated. Combining the typical metallograph and misorientation angle distribution, the microstructure evolution mechanism of composites was analyzed, and the effect of particles on recrystallization behavior was investigated. Under certain process conditions, the dominant deformation mechanism of composites changed from dynamic recovery (DRV) to dynamic recrystallization (DRX), and the grain boundary sliding mechanism began to play a role. In addition, high temperature tensile and elongation at break were tested, and it was found that the dominant form of fracture failure changed from brittle fracture of the particles to ductile fracture of the matrix as the temperature increased.
Functionally graded Al-based joints are promising for electronic packaging, yet achieving reliable dissimilar layer bonding remains challenging. Here, we compare 6063Al-SiC/Al and 6063Al-Si/Al joints fabricated by hot isostatic pressing (HIP). Although both achieve defect-free bonding, but the SiC/Al joint exhibits a far higher tensile strength of 253 MPa and an interfacial shear strength of 203 MPa than the Si/Al joint, which reaches only 155 MPa and 48 MPa, respectively. This disparity stems from distinct interface evolution: the SiC/Al joint features an atomically bonded interface with high strain shielding efficiency, confining thermal mismatch strain to a narrow region of approximately 15 µm adjacent to the interface and protecting the 6063Al substrate. In contrast, Si particle fragmentation, imperfect interfaces, and low strain shielding efficiency in the Si/Al joint promote stress concentration and widespread substrate deformation, leading to premature failure with a brittle cleavage mode. These results demonstrate that reinforcement structural stability and strain shielding efficiency of the composite are crucial for the reliability of graded Al joints in electronic packaging.