In this study, a new method was proposed to reduce the keyhole volume with friction stir spot welding process and improve the lap joint shear load-carrying capacity of the weld by analyzing the effects of tool rotation speed, plunge depth and dwell time on the weld. Single lap shear tests were carried out to determine the influences of the welding parameters on the mechanical behavior of the welds. The quality of the joint was evaluated by examining the characteristics of the joint as a result of the lap joint shear load. For friction stir spot welding of the acrylonitrile butadiene styrene samples, the experiments were designed according to Taguchi’s L9 orthogonal array in a randomized way. From the analysis of variance and the signal-to-noise ratio, the significant parameters and the optimum combination level of the parameters were obtained. It was found that using a tool rotation of 1000 rpm, plunge depth 11.5 mm and dwell time of 40 s, an improved joint strength can be obtained. The results showed that joint strength was improved by an amount of 20% as compared with the optimum welding parameters to the initial welding parameters. Macrostructure examination plays an important role to determine the joint strength and evaluate the influences of each welding parameters. So, weld morphology was investigated by morphological analysis and visual comparisons. It was also observed failure modes for fractured samples having the highest, moderate and lowest lap joint shear load.
As a light-weight solution for electromagnetic shielding, this paper aims to investigate the development of electrically conductive composites that shield from electromagnetic radiation while providing sustainability by using recycled fibers in the structure of nonwoven reinforcement materials. The main novelty of this research is the conversion of waste fabrics into functional composites via a fast and inexpensive method. For this purpose, waste fabrics were recycled into fibers, and the recycled fibers were processed into needle-punched nonwovens to be used as reinforcement materials for electromagnetic shielding composites. Electrically conductive composite structures were obtained by adding copper (II) sulfate and graphite conductive particles with different ratios to polyester resin. The hand lay-up method was used for the production of composites. Electromagnetic shielding, electrical resistivity, and some mechanical properties of the composites were investigated. The results were analyzed statistically using IBM SPSS software version 18. The results have shown that up to 31.43 dB of electromagnetic shielding effectiveness was obtained in the 1–6 GHz frequency range. This result corresponds to a very good grade for general use and a moderate grade for professional use, according to FTTS-FA-003, exceeding the acceptable range for industrial and commercial applications of 20 dB. The composites developed in this research are good candidates to be used in various general and professional applications, such as plastic parts in household applications, electronic industry, building and construction industries, and other applications where light weight shielding materials are needed.
30 June 2014 in Usak University Journal of Material Sciences
The aim of this study is to investigate the effect of important process parameters and tool parameters on joint strength in fiction stir welding process of high density polyethylene (HDPE) using the Taguchi experimental design method. The tool rotation, feed rate and tool shoulder diameter were considered as varying parameter and used to fabricate the joints. The quality of the joint was evaluated by examining the characteristics of the joint as a result of ultimate tensile strength. For friction stir welding of the plates, the experiments were arranged by using Taguchi's L9 orthogonal array in randomized way. From the analysis of variance and the signal-to-noise response graphs, the significant parameters and the optimal combination level of the parameters were obtained. It was found that using a tool rotation of 1600 rpm, a feed rate of 20 mm·mm−1 and a shoulder diameter of 20 mm, an improved joint strength can be obtained. A confirmation run is also performed to prove the effectiveness of the Taguchi method. The results show that joint strength was improved by about 25% compared with the initial welding parameters.
17 December 2020 in Materialwissenschaft und Werkstofftechnik