Defects can be introduced into shotcrete materials after a few freeze–thaw cycles, which has a significant influence on the fracture performance of shotcrete. In this study, a series of shotcrete specimens with varying sizes, geometries, and initial crack lengths were prepared to investigate the fracture properties of notched shotcrete under freeze–thaw conditions. Considering the effects of specimen boundaries and material microstructure, a linear closed-form solution was proposed to determine the fracture toughness of frost-damaged shotcrete. The fracture toughness was found to be a reliable material constant, independent of specimen geometry variations. Results from three-point bending (3PB) tests show that freeze–thaw cycles severely weaken the fracture toughness of shotcrete, which is consistent with CT scan images of the damaged microstructure of the shotcrete specimens. Moreover, specimens with longer initial notches exhibited more severe freeze–thaw damage, which should be carefully considered in practical engineering assessments. These findings highlight the critical importance of considering freeze–thaw effects and notch length when evaluating the durability of shotcrete in cold region applications.
Fracture failure in quasi-brittle materials poses a persistent challenge in materials science and engineering. This study presents a thorough investigation of the Boundary Effect Model (BEM), offering a nuanced understanding of the size effect on fracture properties. The conceptual framework, evolutionary process, and applicability scope of BEM are elucidated, highlighting its accuracy and reliability in calculating fracture properties across various quasi-brittle materials. Through the integration of BEM with diverse fracture tests—such as three-point bending, four-point bending, and wedge-splitting—a linear correlation between maximum failure loads and material fracture properties is established. Notably, the study demonstrates that fracture properties, determined by BEM, can be regarded as consistent material constants across specimens of varying sizes, initial notch lengths, geometries, and microstructures. Validation of the BEM’s reliability encompasses the analysis of 140 fracture test results involving concrete, hard rocks, and bamboo scrimber. The synergy of non-linear and linear BEM analyses emerges as a robust approach for accurately predicting the fracture behavior of quasi-brittle materials. This comprehensive exploration sheds light on the potential of the Boundary Effect Model as a valuable tool for predicting and understanding fracture mechanics in diverse materials and scenarios. This research serves as an effective approach to accurately evaluating the fracture properties of quasi-brittle materials, which is of great practical significance for material design, engineering construction, and various industrial applications.
11 August 2025 in Transportation Infrastructure Geotechnology
This study investigates the effect of added sodium sulfate on the performance of high-volume slag-cement mortar (HVSCM). Herein, Na2SO4 (0, 1, 2, and 4 wt.% Na2O) was used to modify HVSCM. The compressive strength, fracture properties, microstructure, and environmental impact of the synthesized samples were analyzed. The results showed that the 1 day compressive strength of HVSCM can be improved by 345.5% with the addition of 4% Na2O (as Na2SO4), compared to samples without Na2SO4. However, the 28 day compressive strength of Na2SO4-activated HVSCM was 14.3–26.4% lower than that of the non-activated HVSCM, though still comparable to OPC. Regarding fracture properties, the initial fracture toughness of non-activated HVSCM was 45.6% higher than that of Ordinary Portland cement (OPC) mortar. Furthermore, Na2SO4 activation further increased initial fracture toughness, with the sample containing 4% Na2O showing a 101.1% improvement over OPC. In contrast, fracture energy was not significantly influenced by Na2SO4 addition. Microstructurally, the enhanced fracture properties of non-activated HVSCM were attributed to a higher degree of C-(A)-S-H polymerization and a denser binder phase. Sodium sulfate introduced sodium ions to strengthen electrostatic attraction and cohesion between C-(A)-S-H globules, offsetting reduced polymerization. Environmental assessment confirms that both activated and non-activated HVSCM substantially reduce embodied energy and CO2 relative to OPC, while the additional embodied energy associated with Na2SO4 activation remains limited (<12%). Overall, this work provides a comprehensive understanding of the fracture behavior of Na2SO4-activated HVSCM, elucidating its capacity to enhance early-age strength and fracture toughness while highlighting its limited effect on long-term strength and fracture energy. These findings support the tailored use of Na2SO4 activation for sustainable construction applications.
Shotcrete, due to its excellent performance, has become widely adopted as a lining material in tunnel construction. However, research on the fracture behavior of shotcrete, especially in terms of precise fracture toughness determination methods, remains limited. In this study, three distinct batches of shotcrete with varying porosities were fabricated, and their fracture properties were evaluated using three-point bending tests. A closed-form solution was developed to calculate the fracture toughness of shotcrete used in tunnel linings, incorporating factors such as micro-structure, specimen boundaries, and geometry. The results demonstrated that the fracture toughness obtained through this method can be treated as a material constant, independent of specimen geometry. Additionally, the study emphasized the importance of considering the pore structure in the design and fracture analysis of shotcrete materials.
The stability of ice structures in cold regions and polar environments has been increasingly challenged by global warming and climate change, making the accurate estimation of ice flexural properties essential. However, the flexural failure process of ice is highly complex, and the calculated flexural properties are influenced by multiple factors. Hence, several data-driven artificial intelligence models were developed to predict flexural strength, using classification and regression tree (CART), AdaBoost, and Random Forest methods, while the Elitist Ant System (EAS) was applied to optimize model parameters. The EAS procedure converged rapidly within ten iterations and effectively enhanced overall model performance. Compared with the single CART model, ensemble approaches exhibited higher prediction accuracy and better generalization, with AdaBoost achieving the best performance (R2 = 0.736). Feature-importance analysis indicated that the testing method and specimen geometry had the greatest influence on the results, highlighting the importance of careful control of experimental conditions. The proposed ensemble–metaheuristic framework provides an efficient tool for predicting the mechanical behavior of ice and offers useful support for stability assessments of ice structures under changing climatic conditions.