Jingjing Liao

Dr. Jingjing Liao


Research Focus & Metrics

Academic Career Length

6Years (2021-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
18 June 2024 in Heliyon
Verified
Journal Article
Open access
JLJingjing Liao
Jingjing Liao
ZCZhuqing Cheng
Zhuqing Cheng
WZWei Zhang
Wei Zhang
YTYan Tang
Yan Tang
ZYZhongbo Yang
Zhongbo Yang
SQShaoyu Qiu
Shaoyu Qiu
Corrosion transition during uniform corrosion of zirconium alloys receives much attention since it is the major degradation procedure. However, predicting the time and oxide thickness at transition has been hindered by the lack of knowledge about transition kinetics and how it responds to varied temperatures. Current study investigated the temperature-sensitivity of corrosion kinetics, transition behavior and microstructures of various zirconium alloys corroded in superheated steam ranging from 390 °C/10.3 MPa to 455 °C/10.3 MPa by autoclave experiment and microscopy analyses. Transition time was found to follow Arrhenius-type relationship with temperature for the first time. Both the transition oxide thickness and metastable oxide thickness increased with temperature, which was theoretically deduced and experimentally confirmed. In Zr-4 oxides, a transition thickness varying from 3.3 μm at 390 °C to 4.2 μm at 455 °C was observed. Microstructure results presented rather large HCP-ZrO particles (200∼400 nm) at O/M interface and they were even larger at the protruded positions. An intense sub-stoichiometric atmosphere was identified at O/M interface, promoting the growth of metastable oxides. The activation energy of transition kinetics was 86∼114 kJ/mol, which is close to diffusion activation energy of oxygen in tetragonal zirconia. A new model based on parabolic-law empirical relationship was thus proposed to predict transition kinetics. Predictions regarding the time to oxidation breakaway at 900-1000 °C were reported, and the results were in good agreement with the experimental data.

14 April 2022 in Ceramics International
Verified
Journal Article
Closed access
XXXiangmin Xie
Xiangmin Xie
ZSZhean Su
Zhean Su
XTXian Tang
Xian Tang
JLJingjing Liao
Jingjing Liao
KTKai Tong
Kai Tong
QHQizhong Huang
Qizhong Huang

1 September 2021 in Materials Research Express
Verified
Journal Article
Open access
JWJun Wu
Jun Wu
MZMa Zhaodandan
Ma Zhaodandan
LXLiu Xiao
Liu Xiao
WLWang Li
Wang Li
WHWang Hui
Wang Hui
JLJingjing Liao
Jingjing Liao
The microstructure and twin behavior of Ti-2Al-2.5Zr tube during cold pilgering were investigated. During the deformation, the intragranular deformation is not uniform, and the microstructure characteristics are similar to low-cycle shear fatigue. Under alternating stress, the rotation tendency of grain is mainly related to the ratio of circumferential to radial strain. As the mainly primary twin, tensile {10–12}〈10–11〉 is activated in large number, which selection of twinning variant conforms to the Schmidt factor law. However, the selection of the secondary twinning variant is related to the slip system activated by the adjacent grains to accommodate the shear strain caused by the twins. The Schmidt factor of the secondary twin is determined by the slip system opened by the adjacent grains.

1 January 2022 in SSRN Electronic Journal
Verified
Preprint
Open access
PDF file
JLJingjing Liao
Jingjing Liao
HWHui Wang
Hui Wang
JWJun Wu
Jun Wu
WZWei Zhang
Wei Zhang
FXFei Xu
Fei Xu
SQShaoyu Qiu
Shaoyu Qiu
Niobium addition in candidate accident tolerant fuel (ATF) cladding FeCrAl alloy has received much attention, but its effect on high temperature water corrosion behavior has not been revealed. Four alloys with different Nb content (0wt%, 0.5wt%, 1.0wt% and 1.5wt%) based on Fe-13Cr-4.5Al-2Mo model alloy were designed, and the corrosion behavior was investigated by in-situ electrochemistry and microscopy. The in-situ electrochemistry analyses were carried out in 360℃/19.0MPa lithiated and borated water connected with a loop system to monitor the water chemistry. Detailed studies on the oxide film formed after exposure for 85 days were conducted by focused ion bombarding and transmission electron microscopy. FeCrAl alloys have satisfactory corrosion resistance because of small corrosion currents and thin oxide films. Only monolayer multicrystal spinel oxide forms on alloy surface. Slight Nb addition (0.5% and 1.0wt%) benefits the corrosion resistance due to relatively large impedance of oxide and delayed oxidation of Fe 2 Nb particles. Porosities with Fe depletion are spotted in oxide and especially severe in 1.5wt%-Nb alloy. Cathodic Tafel kinetics and corrosion mechanisms of FeCrAl are further discussed.

9 September 2026 in SSRN Electronic Journal
Verified
Preprint
Open access
YZYuqi Zheng
Yuqi Zheng
JXJun Xiao
Jun Xiao
TXTing Xiao
Ting Xiao
YCYong Chen
Yong Chen
JLJingjing Liao
Jingjing Liao
QXQi Xu
Qi Xu
The stress corrosion cracking (SCC) behavior of a Zr–Sn–Nb alloy in simulated PWR primary water was systematically investigated as a function of dissolved oxygen (DO, ~10–500 ppb), dissolved hydrogen (DH, 0–50 cc STP H2/kg H2O), and pre-hydrogenation (~640 ppm H). Crack growth rates, crack-tip oxide thickness, hydride fraction, and local plasticity were characterized by DCPD, TEM, and TKD. The SCC propagation rate is largely insensitive to DO, whereas DH exerts a clear retarding effect, reducing the rate by a factor of 2 to 5. Pre-hydrogenation slightly accelerates cracking, an effect attributed not to altered oxidation kinetics, since oxide thickness and hydride fraction remain essentially unchanged, but to enhanced oxide film rupture promoted by solute hydrogen via the HELP mechanism. This hydrogen-induced effect primarily lowers the threshold stress intensity factor for crack propagation, while its influence on the subsequent growth rate is marginal. Crack-tip oxidation is governed predominantly by the direct Zr–H2O reaction, with DO/DH-mediated cathodic reactions playing only a subordinate role. These findings reveal that oxidation kinetics and hydrogen uptake are decoupled in governing SCC propagation: oxidation kinetics control the rate of film regrowth, whereas hydrogen uptake modulates the plasticity-dependent film rupture process through the competing effects of solute hydrogen and hydrides. A distinct slip-oxidation mechanism is thus established for zirconium alloys in high-temperature water, fundamentally different from the water-chemistry-controlled behavior of stainless steels. This mechanistic distinction provides a new basis for evaluating SCC susceptibility in zirconium-based fuel cladding under extended service conditions.