Wojciech Banaś

Mr. Wojciech Banaś

orcid

Research Focus & Metrics

Academic Career Length

4Years (2023-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
9 January 2026 in Crystals
Verified
Journal Article
Open access
PDF file
DKDawid Dariusz Kozień
Dawid Dariusz Kozień
KMKrzysztof Malata
Krzysztof Malata
ZKZuzanna Krysińska
Zuzanna Krysińska
KMKrystian Misieńko
Krystian Misieńko
JDJurij Delihowski
Jurij Delihowski
Zbigniew PędzichZbigniew Pędzich
Zbigniew Pędzich
This study investigated the fabrication and characterization of polylactic acid (PLA)-based ceramic composite filaments for fused deposition modeling (FDM) 3D printing. Boron carbide (B4C) and silicon carbide (SiC) were incorporated into PLA at various weight fractions (1–40 wt. % for B4C and 1–20 wt. % for SiC) to produce composite filaments using a commercial extruder. The rheological properties, thermal stability, and printability of the filaments were evaluated. Filaments with low ceramic content exhibited satisfactory quality, whereas those with higher loadings required reprocessing to improve their dimensional stability and surface morphology. Successful printing was achieved with SiC contents of up to 8 wt. % using single-extruded filaments and up to 20 wt. % using double-extruded filaments. Rheological tests revealed that filaments with low ceramic content exhibited shear-thinning behavior, whereas those with higher loadings displayed nearly Newtonian-like behavior. Thermal analysis using thermogravimetric analysis (TGA) and differential scanning calorimetry (DSC) determined the optimal processing temperature range for the composite filaments to be between 200 °C and 270 °C. High-temperature microscopy was used to study the temperature behavior of the B4C-containing filaments and set the optimum printing temperature. The results demonstrate the feasibility of producing PLA-based ceramic composite filaments for FDM 3D printing with the potential to tailor the thermal and functional properties of the printed parts for specific applications.

31 July 2025 in Desalination and Water Treatment
Verified
Journal Article
Open access
EWEdyta Waluś
Edyta Waluś
WBWojciech Banaś
Wojciech Banaś
MMMaciej Manecki
Maciej Manecki

1 January 2025 in Processing and Application of Ceramics
Verified
Journal Article
Open access
PDF file
DKDawid Dariusz Kozień
Dawid Dariusz Kozień
WBWojciech Banaś
Wojciech Banaś
SCStanislaw Cudzilo
Stanislaw Cudzilo
AGAdrian Graboś
Adrian Graboś
KPKatarzyna Pasiut
Katarzyna Pasiut
Zbigniew PędzichZbigniew Pędzich
Zbigniew Pędzich
With each passing year, multi-layered armours for military vehicles become more and more advanced to meet growing demands and counterpart novel offensive solutions. Layers that are responsible for track deviation and blunting of the projectile, typically made of hard ceramics, are nowadays considered to be replaced by ceramic composite. In this study, two ceramic systems composed of the TiB2 matrix and SiC or SiC/TiC reinforcement phases were fabricated from mixture of B4C powder with different amount of TiSi2 or Ti5Si3 intermetallic phases. Importantly, the desirable microstructure was obtained by reactive sintering at 1550?C and pressure of 2.5GPa. The obtained ceramic composites underwent dynamic loading tests to evaluate their applicability for ballistic shields. Two systems were then compared in terms of the potential pulverization rate which determines usability as a primary layer for a multi-layered vehicle armour.

27 December 2023 in Preprints.org
Verified
Preprint
Open access
PDF file
DKDawid Dariusz Kozień
Dawid Dariusz Kozień
KPKatarzyna Pasiut
Katarzyna Pasiut
WBWojciech Banaś
Wojciech Banaś
MZMateusz Zagórny
Mateusz Zagórny
JPJanusz Partyka
Janusz Partyka
Owing to its properties, boron carbide has been applied in scientific and industrial fields. For this reason, B4C powders should be characterized by high purity and homogeneity in grain size and shape. In this study, boron carbide was prepared using precursors obtained by a hydrothermal method, and the grain morphology of the product was investigated. Boric acid and the saccharides glucose, fructose, inulin, and sorbitol were used as the precursors. Two precursor dehydration methods, freeze-drying and recrystallization, were compared. The precursors were subjected to DLS grain size and FT-IR spectrophotometric studies, and SEM observations of the precursors and products were performed, confirming that boron carbide powders with submicron spherical grains could be successfully synthesized.

14 September 2026 in Journal of the European Ceramic Society
Verified
Journal Article
Open access
DKDawid Dariusz Kozień
Dawid Dariusz Kozień
WBWojciech Banaś
Wojciech Banaś
AWAgnieszka Wojteczko
Agnieszka Wojteczko
GGGrzegorz Grabowski
Grzegorz Grabowski
AWAlan Wilmański
Alan Wilmański
Zbigniew PędzichZbigniew Pędzich
Zbigniew Pędzich

31 January 2024 in Crystals
Verified
Journal Article
Open access
PDF file
DKDawid Dariusz Kozień
Dawid Dariusz Kozień
KPKatarzyna Pasiut
Katarzyna Pasiut
WBWojciech Banaś
Wojciech Banaś
MZMateusz Zagórny
Mateusz Zagórny
JPJanusz Partyka
Janusz Partyka
Owing to its properties, boron carbide has been applied in scientific and industrial fields. For this reason, B4C powders should be characterized by high purity and homogeneity in grain size and shape. In this study, boron carbide was prepared using precursors obtained using a hydrothermal method, and the grain morphology of the product was investigated. Boric acid and the saccharides glucose, fructose, inulin, and sorbitol were used as the precursors. Two precursor dehydration methods, freeze-drying and recrystallization, were compared. The precursors were subjected to DLS grain size and FT-IR spectrophotometric studies, and SEM observations of the precursors and products were performed, confirming that boron carbide powders could be successfully synthesized.