Silicon carbide (SiC), a wide-band gap semiconductor, is essential for applications in electric vehicles, 5G communications, and aerospace due to its outstanding physical properties. However, their high production costs limit their widespread industrial applications. The growth of larger diameter and thicker crystals, particularly 8 in. crystals, offers the potential to reduce these costs. Therefore, large-diameter PVT crystal growth equipment with resistance heating has become a focal point of research in this field. In this paper, a novel double-flap resistance furnace design is proposed for the first time, and the thermal field is systematically studied by three-dimensional COMSOL Multiphysics modeling to optimize the growth of 8 in. 4H-SiC single crystals. It is found that the resistance heating system significantly outperforms the induction heating system by providing a lower radial temperature gradient necessary for large-diameter SiC crystals. Additionally, the influence of key parameters such as the crucible, the distance between the heater and the crucible, and the growth power on the thermal field distribution in the crucible was also systematically studied. The influence of the distance from the surface of the source material to the crystal surface and the distance from the center of the crystal to the edge on both the axial and radial temperature differences is also analyzed. Based on the simulation results, the crystal growth scheme was further optimized and an 8 in. SiC crystal with a thickness above 20 mm and resistivity uniformity was successfully obtained using the novel resistance furnace. This is of great significance for the growth of large-diameter SiC crystals.
High-entropy alloys (HEAs) have been attracting growing interest for decades due to their unique properties. Electrodeposition provides a low-cost and convenient route for producing classified types of HEAs, compared to other synthesis techniques, making it an attention-grabbing method. However, fabricating high-quality HEAs through electrodeposition in aqueous electrolytes remains a great challenge. In this study, the effects of additives and current densities on the compositions, surface morphologies, microstructures, and corrosion behavior of the electrodeposited NiFeCoCu alloy are studied. The results indicate that saccharin plays a key role in achieving a flat and bright surface for NiFeCoCu coatings, while also relieving the internal stress and improving anti-corrosion properties. Electrodeposition under a current density of 20–40 mA/cm2 results in a uniform and dense deposit with favorable properties. The present work provides a low-cost and feasible industrial solution for the preparation of HEA coatings, which holds great potential for innovation in the field of HEA coatings through electrodeposition.
5 March 2019 in Heat Treatment and Surface Engineering
When a Si-containing steel is subjected to quenching-partitioning-tempering (Q–P–T) process, it will become a martensitic steel with considerable volume of retained austenite, which is attributed to the partitioning of carbon from martensite to retained austenite leading to carbon-depletion in martensitic matrix and carbon-enrichment in the retained austenite. The softening of the martensitic matrix caused by carbon-depletion markedly enhances its deformation ability and raises the ductility of Q–P–T steels. During deformation dislocation absorption by retained austenite (DARA) effect will occur, that is, the dislocations in martensitic matrix will move into nearby retained austenite through the martensite-austenite interface and be absorbed by the retained austenite. This second softening of the martensitic matrix also enhances its deformation ability and effectively raises the ductility. The effect of DARA on ductility during deformation is more effective than the transformation-induced plasticity (TRIP) effect caused by martensitic transformation of retained austenite, because during the TRIP effect the twin-type martensite produced by strain-induced martensitic transformation of retained austenite is very detrimental to ductility.