Rongbin Li

Dr. Rongbin Li


Research Focus & Metrics

Academic Career Length

16Years (2011-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
19 February 2020 in Entropy
Verified
Journal Article
Open access
PDF file
CJChunxia Jiang
Chunxia Jiang
RLRongbin Li
Rongbin Li
XWXin Wang
Xin Wang
HSHailong Shang
Hailong Shang
Yong ZhangYong Zhang
Yong Zhang
Peter LiawPeter Liaw
Peter Liaw
In this study, high-entropy alloy films, namely, AlCrTaTiZr/AlCrTaTiZr-N, were deposited on the n-type (100) silicon substrate. Then, a copper film was deposited on the high-entropy alloy films. The diffusion barrier performance of AlCrTaTiZr/AlCrTaTiZr-N for Cu/Si connect system was investigated after thermal annealing for an hour at 600 °C, 700 °C, 800 °C, and 900 °C. There were no Cu-Si intermetallic compounds generated in the Cu/AlCrTaTiZr/AlCrTaTiZr-N/Si film stacks after annealing even at 900 °C through transmission electron microscopy (TEM) and atomic probe tomography (APT) analysis. The results indicated that AlCrTaTiZr/AlCrTaTiZr-N alloy films can prevent copper diffusion at 900 °C. The reason was investigated in this work. The amorphous structure of the AlCrTaTiZr layer has lower driving force to form intermetallic compounds; the lattice mismatch between the AlCrTaTiZr and AlCrTaTiZ-rN layers increased the diffusion distance of the Cu atoms and the difficulty of the Cu atom diffusion to the Si substrate.

4 December 2011 in Discover Nano
Verified
Journal Article
Open access
PDF file
XWXianghu Wang
Xianghu Wang
RLRongbin Li
Rongbin Li
DFDonghua Fan
Donghua Fan
The quartz/Al-ZnO film/nanostructured Al-ZnO/CdSe/Cu2O extremely thin absorber solar cell has been successfully realized. The Al-doped ZnO one-dimensional nanostructures on quartz templates covered by a sputtering Al-doped ZnO film was used as the n-type electrode. A 19- to 35-nm-thin layer of CdSe absorber was deposited by radio frequency magnetron sputtering, coating the ZnO nanostructures. The voids between the Al-ZnO/CdSe nanostructures were filled with p-type Cu2O, and therefore, the entire assembly formed a p-i-n junction. The cell shows the energy conversion efficiency as high as 3.16%, which is an interesting option for developing new solar cell devices.

13 July 2020 in Advanced Engineering Materials
Verified
Journal Article
Closed access
PDF file
RLRongbin Li
Rongbin Li
TCTongtong Chen
Tongtong Chen
CJChunxia Jiang
Chunxia Jiang
JZJing Zhang
Jing Zhang
YZYong Zhang
Yong Zhang
PLPeter K. Liaw
Peter K. Liaw

22 April 2021 in Materials
Verified
Journal Article
Open access
PDF file
YLYang Li
Yang Li
HSHailong Shang
Hailong Shang
Bingyang MaBingyang Ma
Bingyang Ma
XGXuqiang Guo
Xuqiang Guo
RLRongbin Li
Rongbin Li
GLGeyang Li
Geyang Li
Two kinds of Al2O3 ceramic samples with and without Al film deposited were designed respectively. The influences of temperature and high kinetic energy sputtering particles on the wettability and interface strength of Al/Al2O3 were studied by comparing the wetting behavior of molten aluminum on two samples. The results show that molten aluminum does not wet the Al2O3 sample without Al film deposited at 700 °C, the contact angle is 165°, and the interfacial shear strength is 28 MPa. With the increase of temperature, the contact angle decreases continuously, and the interface shear strength gradually increases. The fracture of the brazed joint is transferred from the interface to the brazing seam. In comparison, the sample deposited with Al film is wetted by molten aluminum at 700 °C, and the contact angle is only 12°. The interface shear strength is about 120 MPa and is less affected by temperature. The shear fracture of the joint occurs in the brazed seam of Al metal. Therefore, the high energy generated by either the temperature increase or the particle sputtering enable the Al atoms to overcome the energy barrier to form Al–O bonds with the O atoms on the Al2O3 ceramic surface, thereby improving the wettability of Al/Al2O3.

12 January 2024 in Coatings
Verified
Journal Article
Open access
PDF file
RLRongbin Li
Rongbin Li
YXYue Xing
Yue Xing
QLQianqian Li
Qianqian Li
ZCZhijun Cheng
Zhijun Cheng
LGLinlin Guo
Linlin Guo
Five thermal barrier coatings (TBCs), namely TBC-1 (YSZ), TBC-2 (CeYSZ), TBC-3 (YSZ:CeYSZ = 1:2), TBC-4 (YSZ:CeYSZ = 1:1), and TBC-5 (YSZ:CeYSZ = 2:1), were fabricated using the atmospheric plasma spraying (APS) method. Their oxidation behaviors at 1100 °C and corrosion resistance to molten salts (V2O5 + Na2SO4) at 900 °C were examined. After 100 h of oxidation, the thermally grown oxide layer (TGO) for YSZ primarily contained Cr and Ni oxides with significant internal fractures, presenting a continuous band-like Al2O3. In dual-ceramic configurations, an increase in CeYSZ thickness led to a rise in Al content and reduced Cr and Ni in TGO, with the surface fracture morphing into an internal porosity. Following salt corrosion, YSZ revealed rod-like YVO4 and m-ZrO2 as corrosion products, whereas CeYSZ displayed chain-structured CeO2, CeYO4, and YVO4 combined with m-ZrO2. YSZ coatings underwent notable phase transitions with evident densification, forming a corrosion layer of approximately 10 μm. Conversely, CeYSZ showed a limited phase change, retaining porosity without a distinguishable corrosion layer. As CeYSZ thickness increased from 100 μm to 200 μm in the dual-ceramic structure, salt penetration reduced. Evidently, the dense structure of CeYSZ heightened diffusion resistance against oxygen and corrosive salts, rendering superior oxidation and corrosion resistance over YSZ. By optimizing the thickness ratio between CeYSZ and YSZ, whilst retaining total ceramic layer thickness, the dual-ceramic TBC’s resistance to high-temperature oxidation and corrosion can be enhanced.

7 November 2024 in Nanomaterials
Verified
Journal Article
Open access
PDF file
CJChunxia Jiang
Chunxia Jiang
RLRongbin Li
Rongbin Li
FHFeng He
Feng He
ZCZhijun Cheng
Zhijun Cheng
WLWenge Li
Wenge Li
YZYUANTAO ZHAO
YUANTAO ZHAO
In this study, Gd2O3 and Yb2O3 co-doped YSZ (GYYSZ) ceramic coatings were prepared via atmospheric plasma spraying (APS). The GYYSZ ceramic coatings were subjected to heat treatment at different temperatures for 5 h to analyze their high-temperature phase stability and sintering resistance. The thermophysical properties of GYYSZ, YSZ, and composite coatings were compared. Three types of thermal barrier coatings (TBCs) were designed: GYYSZ (TBC-1), YSZ/GYYSZ (TBC-2), and YSZ/Composite/GYYSZ (TBC-3). The failure mechanisms of these three TBCs were investigated. The results indicate that both the powder and the sprayed GYYSZ primarily maintain a homogeneous cubic phase c-ZrO2, remaining stable at 1500 °C after annealing. The sintering and densification of the coatings are influenced by the annealing temperature; higher temperatures lead to faster sintering rates. At 1500 °C, the grain size and porosity of GYYSZ are 4.66 μm and 9.9%, respectively. At 1000 °C, the thermal conductivity of GYYSZ is 1.35 W·m−1 K−1, which is 44% lower than that of YSZ. The thermal conductivity of the composite material remains between 1.79 W·m−1 K−1 and 1.99 W·m−1 K−1 from room temperature to 1000 °C, positioned between GYYSZ and YSZ. In the TBC thermal shock water quenching experiment, TBC-3 demonstrated an exceptionally long thermal shock lifetime of 246.3 cycles, which is 5.8 times that of TBC-1 and 1.8 times that of TBC-2. The gradient coating structure effectively reduces the thermal mismatch stress between layers, while the dense surface microcracks provide a certain toughening effect. Failure analysis of the TBC reveals that TBC-3 exhibits a mixed failure mode characterized by both spallation and localized peeling. The ultimate failure was attributed to the propagation of transverse cracks during the final stage of water quenching, which led to the eventual spallation of the ceramic blocks.