Titanium aluminides find application in modern light-weight, high-temperature turbines, such as aircraft engines, but suffer from poor plasticity during manufacturing and processing. Huge forging presses enable materials processing in the 10-GPa range, and hence, it is necessary to investigate the phase diagrams of candidate materials under these extreme conditions. Here, we report on an in situ synchrotron X-ray diffraction study in a large-volume press of a modern (α2 + γ) two-phase material, Ti-45Al-7.5Nb-0.25C, under pressures up to 9.6 GPa and temperatures up to 1686 K. At room temperature, the volume response to pressure is accommodated by the transformation γ → α2, rather than volumetric strain, expressed by the apparently high bulk moduli of both constituent phases. Crystallographic aspects, specifically lattice strain and atomic order, are discussed in detail. It is interesting to note that this transformation takes place despite an increase in atomic volume, which is due to the high ordering energy of γ. Upon heating under high pressure, both the eutectoid and γ-solvus transition temperatures are elevated, and a third, cubic β-phase is stabilized above 1350 K. Earlier research has shown that this β-phase is very ductile during plastic deformation, essential in near-conventional forging processes. Here, we were able to identify an ideal processing window for near-conventional forging, while the presence of the detrimental β-phase is not present under operating conditions. Novel processing routes can be defined from these findings.
In order to examine the feasibility of applying synchrotron radiation μCT imaging to alloy steels for non-destructive inspection of inclusions for potential origins of internal fatigue damage in the very high cycle region, synchrotron radiation μCT imaging was utilized for repeated non-destructive observation of Cr-Mo steel. An ultrasonic fatigue testing machine was used in aid of the repeated observation. As a result, it was found that the synchrotron radiation μCT imaging with 70 keV was useful for non-destructive observation of inclusions of more than 10 μm, one of which may be an internal fatigue origin. No identifiable damage was observed around every inclusion, and in the base metal, at least up to 70% of fatigue life was observed in the imaging volume.
The authors would like to apologize for any inconvenience regarding misleading errors and inconsistencies in some of the units and one number, and wish to make the following corrections to this paper [1]: