Laser cutting is a cutting technology that enables fast processing in high precision. This technology utilizes high temperatures generated by engine to perform the cutting process. Selection of cutting parameters becomes the main factor to determine the cutting surface quality. Cutting parameters in the form of cutting speed and gas pressure are varied between 60 mm/minute - 100 mm/minute and 17 bar - 21 bar to examine the effect on surface character. The character of the laser-cutting surface on 316L series stainless steel material was observed related to the roughness, hardness and microstructure. The results showed that the parameters of cutting speed and gas pressure had an effect on the cutting surface. Changes in cutting speed has more effect on surface roughness while gas pressure has more effect on cutting surface hardness. Observations on the surface also illustrated that there were differences in cutting quality along with the deeper penetration performed by the laser.
This study introduces Sn-substituted higher manganese silicides (MnSi1.75, HMS) synthesized via an arc-melting process followed by spark plasma sintering (SPS). The influences of Sn concentrations on the thermoelectric performance of Mn(Si1−xSnx)1.75 (x = 0, 0.001, 0.005, 0.01, 0.015) are systematically investigated. Our findings reveal that metallic Sn precipitates within the Mn(Si1−xSnx)1.75 matrix at x ≥ 0.005, with a determined solubility limit of approximately x = 0.001. In addition, substituting Si with Sn effectively reduces the lattice thermal conductivity of HMS by introducing point defect scattering. In contrast to the undoped HMS, the lattice thermal conductivity decreases to a minimum value of 2.0 W/mK at 750 K for the Mn(Si0.999Sn0.001)1.75 sample, marking a substantial 47.4% reduction. Consequently, a figure of merit (ZT) value of ~0.31 is attained at 750 K. This considerable enhancement in ZT is primarily attributed to the suppressed lattice thermal conductivity resulting from Sn substitution.