Methods of optical metallography, X-ray diffraction, and transmission and scanning electron microscopy were used to study changes in the structure of the aluminum alloy D16 (2024) caused by isothermal rolling at a temperature of liquid nitrogen. It has been established that the basic structural changes that take place in the material upon deformations to e ∼ 2.0 are due to the formation and evolution of the dislocation structure, which contains cells of nanometer size. With further straining to e ∼ 3.5, the processes of recovery and recrystallization become activated, which lead to the formation of a mixed grain-subgrain nanosized structure.
1 November 2017 in Protection of Metals and Physical Chemistry of Surfaces
Structural and phase factors influencing the intergranular corrosion (IGC) of D16 aluminum alloy after quenching, isothermal rolling at liquid-nitrogen temperature, and subsequent natural and...
Influence of precipitates, formed upon preliminary heat treatment, on development under severe straining of nanocrystalline (NC) structure and hardness of 7xxx - type aluminum alloy with Zr and Sc additions was investigated. The samples cut from homogenized ingot were processed by high-pressure torsion (HPT) via 10 revolutions under 6 GPa at room temperature. Prior HPT, the alloy was solution treated, water quenched and annealed for 5 hours in the temperature range of 170-250 0C to change its structural heterogeneity - size and density of precipitates of different origin. In addition to coherent disk-type aluminides of transition metals ~25 nm in diameter (so-called dispersoids), that were in pre-quenched alloy, annealing led to precipitation of the main strengthening (MgZn) - type phases with equivalent diameter from ~10 to 200 nm. Most highly developed NC structure with a (sub)grain size of ~80 nm was processed in the pre-quenched alloy and resulted in its abnormally high hardness. HPT of the pre-annealed at 170 0C alloy with -phase precipitates of less size and one order higher densities than that of dispersoids, on the opposite, produced completely non-recrystallized structure with near 15% reduced hardness owing to the grain refinement suppression. Increasing the temperature of annealing led to coarsening and less densities of - phases, intensifying nanostructuring. However, all pre-annealed NC states demonstrated minimum hardness as their work hardening did not compensate the softening due to -phase coagulation.
The effect of a treatment combining isothermal cryogenic rolling and single electro-pulsing on the structure and hardness of M1 grade copper with an initial grain size of 10 –15 μm was investigated.