E-waste is one of the fastest growing waste streams in the world, paradoxically containing both hazardous components and substances which can adversely impact on both the environment and public health, as well as valuable secondary resources and raw materials that could be recovered if e-waste is processed properly. Developing countries not only lack the infrastructure and technology required to manage e-waste appropriately, they largely rely on a fragmented informal sector for the management of a large fraction of e-waste that is either recognized by the state, or is marginalized and suppressed. This article examines the current situation with e-waste management in the developing countries, and assesses these countries’ challenges. The study highlights that there is an urgent need to design more better framework for e-waste that protect these countries from the problems caused by e-waste that are beyond repair and refurbishment, and to help these countries to advance their e-waste recycling and disposal facilities to prevent open burning on and dumping in the environment that can result in deleterious effects on communities at a local as well as at a global level.
This paper presents the design, development and realization of a fast and novel process for the synthesis of 3C silicon carbide (β-SiC) nanorods and submicron powder. Using SiO2 (or Si) and activated carbon (AC), this process allows β-SiC to be synthesized with almost 100% purity in timeframes of seconds or minutes using multimode microwave rotary tube reactors under open-air conditions. The synthesis temperature used was 1460 ± 50 °C for Si + AC and 1660 ± 50 °C for SiO2 + AC. The shortest β-SiC synthesis time achieved was about 20 s for Si + AC and 100 s for SiO2 + AC. This novel synthesis method allows for scaled-up flow processes in the rapid industrial-scale production of β-SiC, having advantages of time/energy saving and carbon dioxide emission reduction over comparable modern processes.
Dismantling the waste printed circuit boards (WPCBs) of obsolete mobile phones is essential for resource recycling and environmental protection. An automated WPCB disassembly equipment based on the hot-vibration process was designed and applied, with optimized process conditions of a heating temperature of 250 °C and an equipment amplitude of >3.66 mm. The dismantling rate for electronic components and metal shields was 98%, but disassembly of components with underfill was less effective. Both simulation and actual measurement results of the equipment’s thermal field showed that the temperature inside the disassembly bin was uniform, with a maximum temperature difference of 6–8 °C. The area of the low-temperature region accounted for approximately 5% of the total area. The acceleration ranged from 2.11 to 8.28 g when using the disassembly force model. This equipment and process can be applied to disassemble large quantities of WPCBs.
The paper describes one promising method and approach for the recycling, reuse, and co-resource treatment of waste photovoltaic silicon and lithium battery anode graphite. Specifically, this work considers the preparation of nano/micron silicon carbide (SiC) from waste resources. Using activated carbon as a microwave susceptor over a very short timeframe, this research paper shows that nano/micron β-SiC can be successfully synthesized using microwave sintering technology. The used sintering temperature is significantly faster and more energy-efficient than traditional processes. The research results show that the β-SiC particle growth morphology greatly affected by the microwave sintering time. In a short microwave sintering time, the morphology of the β-SiC product is in the form of nano/micron clusters. The clusters tended to be regenerated into β-SiC nanorods after appropriately extending the microwave sintering time. In the context of heat conversion and resource saving, the comprehensive CO2 emission reduction is significantly higher than that of the traditional SiC production method.