This study aims to assess the effectiveness of water-based formulations featuring m-2HEAOL and talc particles in deep drawing applications. The coefficient of friction (COF) was measured through bending under tension (BUT) tests, while the interaction mechanism between protic ionic liquid (PIL) and talc particles was analysed using FTIR, XPS, and TGA analyses. The results indicate that the formulation containing 8 wt% PIL and 0.5 wt% talc exhibited the best lubricating performance. This was due to the interaction of the PIL oleate molecules with the Mg found in the talc basal layer, which enhanced the cleavage capacity of this mineral, ultimately improving the lubricity of the formulation.
28 June 2024 in Journal of the Brazilian Society of Mechanical Sciences and Engineering
This research aims to investigate and quantify potential damage resulting from induced superficial defects on the surface of wires use on tensile armor of flexible pipes. Different values of kt factors and H2S concentration in aggressive gas mixtures with CO2, were analysed to determine the operational conditions that do not result in rupture of the tensile reinforcement during service, under the conditions studied. The tests were based on NACE TM0316 standard, using a 4-point bend test. Two superficial notches were created, which generated known stress concentration factor Kt values of 1.5 and 2.0, and three gaseous concentrations (220, 700, and 1100 ppm of H2S in CO2) were used. After bending tests, the samples were evaluated by metallographic and fractographic analysis, weight loss and liquid penetrant inspection. The results were then analysed using analysis of variance (ANOVA). Only the samples exposed to 220 ppm of H2S in CO2 did not rupture at both Kt values. However, for the Kt value of 2.0, cracks were observed in the longitudinal direction of the wires, originating from the machined notch. Additionally, the samples exposed to 700 ppm and 1100 ppm of H2S had a significantly higher damage score (approximately 15x) than the samples exposed to 220 ppm, regardless of the Kt value.