The production of green hydrogen via water electrolysis faces challenges due to the sluggish oxygen evolution reaction at the anode. In this study, we developed a self-supported bifunctional Pt/SnO2/Nb2O5/Nb electrocatalyst capable of coupling the hydrogen evolution reaction to the selective ethanol oxidation reaction (EOR) in an acidic medium. The catalyst demonstrated efficacy for the EOR, with an E onset of +130 mV versus SHE results in a peak current density of 8.97 mA cm–2. The bifunctional electrocatalyst exhibited a spontaneous and rapid increase in current for the HER, achieving an overpotential of −48 mV for a current density of 5 mA cm–2 and a Faradaic efficiency of 99.7%. This efficient coupling of the EOR with the HER reduces energy consumption for green hydrogen generation compared to traditional water splitting. With hydrogen being the sole gaseous product, the HER–EOR electrolysis system can operate effectively without a membrane, promising a more cost-effective, sustainable, and efficient green hydrogen production.
This research aims to investigate and quantify potential damage resulting from induced superficial defects on the surface of wires use on tensile armor of flexible pipes. Different values of kt factors and H2S concentration in aggressive gas mixtures with CO2, were analysed to determine the operational conditions that do not result in rupture of the tensile reinforcement during service, under the conditions studied. The tests were based on NACE TM0316 standard, using a 4-point bend test. Two superficial notches were created, which generated known stress concentration factor Kt values of 1.5 and 2.0, and three gaseous concentrations (220, 700, and 1100 ppm of H2S in CO2) were used. After bending tests, the samples were evaluated by metallographic and fractographic analysis, weight loss and liquid penetrant inspection. The results were then analysed using analysis of variance (ANOVA). Only the samples exposed to 220 ppm of H2S in CO2 did not rupture at both Kt values. However, for the Kt value of 2.0, cracks were observed in the longitudinal direction of the wires, originating from the machined notch. Additionally, the samples exposed to 700 ppm and 1100 ppm of H2S had a significantly higher damage score (approximately 15x) than the samples exposed to 220 ppm, regardless of the Kt value.