One of the primary challenges in the automotive industry is the wear of engine components, such as the crankshaft and camshaft, which is the most pronounced during the engine’s startup phase, when the amount of lubricant fluid is at its lowest. This study aims to enhance the surface wear resistance of automotive crankshaft steel by applying a boriding thermochemical process. This process forms a hard surface layer on the steel, improving its mechanical properties and bolstering its wear resistance, especially under dry conditions. Boride layers were achieved using the powder-pack boriding process in a conventional furnace, with meticulous treatment times of 2, 4, and 6 h at a constant temperature of 950 °C. The nature of the layers was analyzed using X-ray diffraction, and their tribological behavior was evaluated using the pin-on-disk test. The growth of the layers was directly proportional to the treatment time and was estimated at 145 µm and 48 µm for the 6 and 2 h of treatment, respectively. The surface hardness increased from 320 HV for the non-treated steel to 2034 HV for the sample exposed to 950 °C for 6 h. The results indicate a significant reduction in the coefficient of friction from 0.43 for the non-treated steel to 0.12 for the samples exposed to 950 °C for 6 h, suggesting potential wear protection during the engine starting period.
Boriding is a thermochemical process by which the surface of metallic materials is strongly improved for many applications. When boriding is applied to ferrous alloys, a boride layer containing mainly a single-phase Fe\(_{2}\)B or a double-phase Fe\(_{2}\)B/FeB grows on the metallic substrate. The thickness of the boride layers depends primarily on the temperature and the treatment time. On the other hand, the thermal diffusivity is related to the materials’ density and thermal conductivity. Therefore, as the thickness of the boride layers increases, their density decreases, and so does their thermal diffusivity. In this work, the change in thermal diffusivity of the layered material, as a function of thermochemical treatment, is assessed. Samples of AISI 1018 steel were exposed to boriding treatment during 2, 4, 6, and 8 h at a constant temperature of 950 \(^\circ\)C. The crystalline structure of the layers was analyzed by X-ray diffraction and optical microscopy. The mechanical properties and the thermal diffusivity of the steel-boride layered materials were evaluated by Vickers micro indentation and Photothermal Spectroscopy, respectively.
30 September 2025 in Measurement Science and Technology
This study introduces photopyroelectric techniques for the thermal and optical characterizations of carbon nanotubes (CNTs) while focusing on the measurement of optical absorption coefficients and thermal diffusivity of suspensions of CNTs in glycerol at different concentrations. Optical absorption coefficients were measured at selected wavelengths in the visible and infrared ranges, whereas thermal characterization was conducted by measuring the thermal diffusivity (for multiwalled CNT suspensions) with an average diameter of 140 nm and a length of 7 µm, within a concentration range of 0.001–0.01 g ml−1. A linear increase in the optical absorption coefficients with CNT concentration was obtained – a finding not achievable with absorbances measured by means of conventional UV–Vis spectroscopy. In contrast, thermal diffusivities, in the range of 0.005–0.06 g ml−1, exhibited a notable increase with concentration. The fitting of this behavior to a logistic model allowed the prediction of thermal diffusivity at “infinite” CNT concentration. This prediction is confirmed by direct measurements of the thermal properties of a CNT suspension at high concentration using a self-normalized photoacoustic methodology. The direct measurement of optical absorption coefficients provides valuable insights into the absorptivity of CNT suspensions at selected wavelengths. This methodology could be very useful for determining the optical properties of CNT suspensions in other fluids and wavelengths and their relationship with other variables of interest, such as CNT dimensions.
Currently, multiwalled carbon nanotubes (MWCNTs) are finding applications in many scientific fields, such as materials science, physics, biology, and chemistry, some of which require these materials to be functionalized. Functionalization of MWCNT enables enhancement of their properties to achieve advantages for the development of innovative nanodevices. In the present work, a self-normalized photoacoustic technique was applied for measurement of the thermal diffusivity (TD) of nanocomposites formed from MWCNTs immersed in two different polymeric matrices: polyvinylidene fluoride (PVDF) and polyvinylpyrrolidone (PVP). Pristine carbon nanotubes (p-MWCNTs) were functionalized with two different solutions: HNO 3 , and a mixture of HNO 3 and H 2 SO 4 . The nanocomposites were analyzed under different functionalization conditions. It was shown that the photoacoustic technique can detect differences in TD between these different nanocomposites. Graphical abstract
Boriding is a thermochemical process that improves the surface properties of metallic materials, such as wear resistance, hardness, and Young’s modulus. The current work evaluated the kinetics of boride layers formed by boriding on AISI H13 steel. The AISI H13 steel samples were covered with a non-commercial powder mixture of 70% wt. SiC, 20% B4C wt. and 10% wt. KBF4. The samples were treated for 2, 4, and 6 h at 850, 875, and 900 °C, respectively. The growth kinetics of boride layers were estimated as a function of the treatment parameters, using a solution of the second Fick’s Law, as in a parabolic model. Also, the hardness of layers was assessed by Vickers microindentation. Optical examination of the samples showed a biphasic FeB/Fe2B layer at all temperatures after 6 h of treatment. In contrast, those exposed for 2 h exhibited a monophasic Fe2B layer with isolated zones of the FeB phase in all temperatures. The results suggested that the obtained layer thicknesses are highly dependent on the treatment parameters. After 2 h at 850 °C, the samples exhibited a well-defined layer with a thickness of 8.51 ± 1.01 μm, whereas after 6 h it was 24.39 ± 1.01 μm. The activation energy was estimated at 230.63 kJ/mol, with a correlation coefficient (R2) of 0.97, consistent with values reported in the literature. Additionally, the hardness values were estimated to range from 1880 to 2192 HV for the FeB phase and from 1294 to 1715 HV for the Fe2B phase, indicating that the hardness of the boride layers is highly dependent on the treatment conditions.