This study investigates the behaviour of metallic beryllium under high-temperature corrosion in a water-steam-argon atmosphere under thermal cycling conditions using thermogravimetric and differential scanning calorimetric analysis (TGA/DSC). The experiments were conducted at three heating rates (10, 20, and 30 K/min), each including two thermal cycles (C1 and C2). Oxidation was evaluated by mass gain and thermal effects, and kinetic parameters ( Ea , K 0) were determined from logarithmic Arrhenius dependencies with normalisation to surface area and partial water vapour pressure. Two characteristic temperature ranges were established: initial thermal activation (775–1050 K) and high temperature (975–1170 K), as well as a transition zone between them. For the high-temperature region, the activation energy Ea = 146 kJ/mol and the pre-exponential factor K 0 = 2.41·10 −1 mg/(s·cm 2 ·Pa) were obtained. The results obtained deepen the understanding of the mechanisms of beryllium oxidation during thermal cycling and can be used to assess safety in nuclear fusion installations.
Beryllium-based intermetallic compounds, such as Be12Nb, are attracting growing interest for their high thermal stability and potential to replace pure beryllium as neutron reflectors and multipliers in both fission and future fusion reactors, with additional applications in metallurgy, aerospace, and hydrogen technology. The paper presents the results of an investigation of the thermal treatment and phase formation of the intermetallic compound Be12Nb from a mixture of niobium and beryllium powders in the temperature range of 800–1300 °C. The phase evolution was assessed as a function of sintering temperature and time. A nearly single-phase Be12Nb composition was achieved at 1100 °C, while decomposition into lower-order beryllides such as Be17Nb2 occurred at temperatures ≥1200 °C, indicating thermal instability of Be12Nb under vacuum. Careful handling of sintering in low vacuum minimized oxidation, though signs of possible BeO formation were noted. The findings complement and extend earlier reports on Be12Nb synthesis via plasma sintering, mechanical alloying, and other powder metallurgy routes, providing broader insight into phase formation and synthesis. These results provide a foundation for optimizing the manufacturing parameters required to produce homogeneous Be12Nb-based components and billets at an industrial scale. Additionally, they help define the operational temperature limits necessary to preserve the material’s phase integrity during application.
The article presents analytical results on the estimation of the steady-state flux of tritium ions released from lithium-based ceramics Li 2 TiO 3 under reactor irradiation conditions at the WWR-K reactor. Neutron transport calculations were performed in MCNP6 using the ENDF/B-VII.1 library and compared with in-situ gas release recorded at a ceramic temperature of 650 ℃ and a thermal neutron flux of 5·10 13 n/(cm 2 ·s). The developed calculation model does not contain fitting coefficients and takes into account the ion mean free path, the self-shielding effect in ceramics (δ = 0.32) and recombination losses. The obtained values of T⁺ flux from ceramics of different isotopic composition are 3.07·10 −13 to 1.96·10 −12 mol/s. The maximum decrease in the flux due to self-shielding in ceramics does not exceed 32%. The discrepancy between the calculation and the experiment for the HT component does not exceed 15%, which confirms the adequacy of the approach. The results are of practical importance in assessing the tritium balance in fusion reactor blankets and allow optimizing the composition and size of ceramic pebbles taking into account the activation-free gas evolution of tritium.
This paper presents the results of determining the parameters of tritium transfer processes in lithium ceramics Li2TiO3 under reactor irradiation conditions. Analysis of sections with a short-term decrease in reactor power allowed numerical determination of the Arrhenius parameters of tritium diffusion (pre-exponential factor and activation energy) based on comparison with in situ experimental data. The obtained values of activation energy (70.2–74.7 kJ/mol) and pre-exponential factor (0.9–2.1 × 10−8m2/s) demonstrate growth with increasing fluence, which is explained by the accumulation of radiation defects in ceramics. A linear dependence was established between D0 and Ea, corresponding to the Mayer–Noldel rule. Unlike previously conducted studies based on a phenomenological approach to assessing only the activation energy of diffusion, in this study, a complex model that takes into account temperature gradients, tritium generation, its diffusion, and release from the surface was used. The applicability of such an integrated approach to the analysis of in situ reactor experiments with lithium ceramics was confirmed, and allowed us to estimate changes in the tritium transfer parameters in lithium ceramics Li2TiO3 depending on the irradiation time.