Piston-based material extrusion enables cost savings for metal injection molding users when it is utilized as a complementary shaping process for green parts in small batch sizes. This, however, requires the use of series feedstock and the production of sufficiently dense green parts in order to ensure metal injection molding-like material properties. In this paper, a methodological approach is presented to identify material-specific process parameters for an industrially used Ti-6Al-4V metal injection molding feedstock based on the extrusion force. It was found that for an optimum extrusion temperature of 95 °C and printing speed of 8 mm/s an extrusion force of 1300 N ensures high-density green parts without under-extrusion. The resulting sintered part properties exhibit values comparable to metal injection molding in terms of part density (max. 99.1%) and tensile properties (max. yield strength: 933 MPa, max. ultimate tensile strength: 1000 MPa, max. elongation at break: 18.5%) depending on the selected build orientation. Thus, a complementary use could be demonstrated in principle for the Ti-6Al-4V feedstock.
Metal binder jetting shows great potential for medical technology. This potential can be exploited by integrating binder jetting into existing process routes known from metal injection molding. The biggest challenge here is the flowability and packing behavior of the powders used, due to their low size distributions. This paper investigates different powder-drying strategies to improve flowability using a statistical experimental design. Because of its relevance for medical applications, spherical Ti-6Al-4V powder with a size distribution under 25 µm is dried under various parameters using vacuum and gas purging. The investigated parameters, time and temperature, are selected in a central-composite-circumscribed test plan with eleven tests and three center points. The target parameters—water content, flowability and impurity levels (oxygen, nitrogen)—of the powder are analyzed. For validation, practical test trials are carried out on an industrial binder jetting system with unconditioned powder and conditioning with optimized parameters, comparing the manufactured parts and the powder bed. An optimized drying cycle with a duration of 6 h at 200 °C was determined for the investigated powder. Significant improvements in the dimensional accuracy (from ±1.5 to 0.3%) of the components and the visual impression of the powder bed are demonstrated.
14 April 2022 in Macromolecular Materials and Engineering
Commercial UHMWPE powder of 60 µm size (d50) embossed with 2–5 wt% of nanosilica is used as a support for the preparation of core–shell HDPE@silica@UHMWPE particles. The HDPE shell is generated by polymerization of ethylene in toluene slurry after treatment of the silica@UHMWPE with a methyl aluminoxane activated bisimine pyridine iron complex. Heat pressing the powder gives a solid material with identifiable original UHMWPE particles and a layer from fusion of UHMWPE and the surrounding HDPE shell; the properties match those of the UHMWPE base material. The powder flow properties of the HDPE@silica@UHMWPE are insufficient for a powder bed fusion process, a value for the flow function between 2 and 3 is measured in a ring shear tester. Additivation with nanosilica helps to overcome the insufficient flowability and allows the material to be recoated in a power bed fusion system. Laser sintering gives evidence for a substantial mixing and welding of the HDPE shells and UHMWPE. Caking at the surface of the built parts hinders the manufacturing of isolated parts. Further additivation with carbon black reduces the caking; however, the welding within the HDPE@silica@UHMWPE material is much less strong.
Laser-based powder bed fusion of metals (PBF-LB/M) is the most used additive manufacturing (AM) technology for metal parts. Nevertheless, challenges persist in effectively managing metal powder, particularly in blending methodologies in the choice of blenders as well as in the verification of blend results. In this study, a bespoke laboratory-scale AM blender is developed, tailored to address these challenges, prioritizing low-impact blending to mitigate powder degradation. As a blending type, a V-shape tumbling geometry meeting the requirements for laboratory AM usage is chosen based on a literature assessment. The implementation of thermal oxidation as a powder marking technique enables particle tracing. Blending validation is achieved using light microscopy for area measurement based on binary image processing. The powder size and shape remain unaffected after marking and blending. Only a small narrowing of the particle size distribution is detected after 180 min of blending. The V-shape tumbling blender efficiently yields a completely random state in under 10 min for rotational speeds of 20, 40, and 60 rounds per minute. In conclusion, this research underscores the critical role of blender selection in AM and advocates for continued exploration to refine powder blending practices, with the aim of advancing the capabilities and competitiveness of AM technologies.