Operating temperature beyond 600 °C reduces fatigue strength, fracture toughness, wear resistance, corrosion resistance, oxidation resistance, surface hardness, modulus of elasticity, and strength of Ti alloys. These limitations restrict their high-strength, high-temperature applications in different industries, thus enhancing their properties. This paper critically reviews past research on different aspects of the properties enhancement of Ti alloys, describing transformations of their phases and their morphologies, as well as different phase stabilizing elements for Ti alloys. Various chemical, mechanical, and physical surface modification techniques used to enhance the properties of these alloys are discussed, highlighting their major limitations. Adding different elements to Ti alloys is highlighted as a simple and efficient technique to enhance their properties significantly. The contributions of different elements added to Ti alloys to enhance their properties and high-temperature performance are examined. This paper explains different methods used to add different elements to Ti alloys and elaborates on the mechanisms by which addition of these elements refines the grains and improves mechanical properties and high-temperature performance of Ti alloys. Design methodologies for Ti alloys are also presented. The capabilities of additive manufacturing processes used to fabricate Ti alloy components and tailored properties are also highlighted. Some typical applications of properties enhanced Ti alloys in aerospace, space, biomedical, marine and ship building, chemical, and automotive industries are also mentioned. Finally, directions for future research are suggested. This review paper will be very useful in designing and developing Ti alloys with enhanced properties through the selection of appropriate elements.
The aerospace and automotive industries find that relying solely on the intrinsic resistance of alloys is inadequate to safeguard aircraft and automotive structural components from harsh environmental conditions. While it is difficult to attribute accidents exclusively to coating failure due to the involvement of multiple factors, there are instances where defects in the coating initiate a wear or degradation process, leading to premature and unplanned structural failures. Metallic coatings have been introduced to protect the aircraft mainly from wear due to the extreme temperatures and moisture exposure during their service life. Bare metallic coatings have a limited lifespan and need to be replaced frequently. Herein, the strength and wear resistance of zinc (Zn) coating is enhanced using varying concentrations of diamond particles as an additive in the Zn matrix (Zn-D). The dispersion strengthening mechanism is attributed to the high hardness (70 HRC), and reduced friction-of-coefficient (0.21) and dissipation energy (4.6 × 10−4 J) of electrodeposited Zn-D7.5 (7.5 g l−1 of diamond concentration) composite coating. Moreover, enhanced wear resistance with minimum wear volume (1.12 × 10−3 mm3) and wear rate (1.25 × 10−3 mm3 N−1 m−1) of the Zn-D7.5 composite coating resulted in perfect blending of diamond with Zn. The improved hardness and wear resistance for Zn-D7.5 (optimum 7.5 g l−1 diamond concentration) is due to the steadiness between well-dispersed diamonds in Zn and enrichment in load-bearing ability due to the incorporation of diamond particles. Electronic structure calculations on the zinc-diamond composite models (two configurations adopted) have been performed using the density functional theory (DFT) approach, and the in silico studies appeared to facilitate meaningful and evocative outcomes. Zn-doped diamond (C10@Zn) without hydrogen (H) atoms (binding energy: 418 kcal mol−1, i.e. showing an endothermic reaction and thermodynamically not favourable) was detected to be more stable than the Zn-doped diamond (C10H16@Zn) consisting of hydrogen (H) atoms (binding energy: −33.3 kcal mol−1, i.e. showing an exothermic reaction and thermodynamically preferable). Thus, a composite coating of zinc and diamond can be a suitable candidate for the aerospace and automotive industries.
16 December 2024 in Advanced Engineering Materials
This study presents the geometrical optimization of a solar air heater. A reasonable working range of geometrical parameters: length 1–3 m, width 0.1–0.5 m, and height 0.005–0.05 m (or aspect ratio 1–20), is investigated as per general applications and installation constraints. The effect of these geometrical parameters on thermal (heat flux and outlet air temperature) and hydraulic (air velocity, mass flowrate, pressure loss and pumping power, and Bejan number) parameters are theoretically studied. Later, a numerical investigation is carried out with an optimum geometry of SAH-duct (length 2.44 mm and width 0.3 m), for aspect ratio 4–18 and Re 3000–15,000. An experimental study is also done to validate numerical results. The heat transfer and frictional loss do not show a significant change in the values for the aspect ratio 8–12.
This paper presents effects of addition of 4wt.% of Ti to Co-Cr-Mo alloy by µ-plasma arc metal powder additive manufacturing (µ-PAMPAM) process on microstructure, phase evolution, bending strength, tensile and compressive yield and ultimate strength, % elongation, microhardness, porosity, and density of the resultant alloy and their comparison with Co-Cr-Mo alloy. Microstructure and phase evolution study of Co-Cr-Mo alloy showed Co-rich matrix comprising of γ-Co and ε-Co phases, formation of Cr7C3 and Cr23C6 carbides due to presence of carbon and affinity of Cr towards it, and micro-cracks. Addition of 4 wt% Ti to Co-Cr-Mo alloy refined its grains, minimized formation of micro-cracks, led to formation of β-Ti phase and Co-Ti intermetallic compound along with the chromium carbides. It also reduced porosity and density of the resultant Co-Cr-Mo-4Ti alloy. Grain refinement increased flexural strength of Co-Cr-Mo-4Ti alloy. Solid solution effect of Ti increased tensile and compressive yield strength, ultimate compressive and tensile strength, and percentage elongation of Co-Cr-Mo-4Ti alloy as compared to Co-Cr-Mo alloy. Microhardness of Co-Cr-Mo-4Ti alloy increased to 473 MPa from 382 MPa of Co-Cr-Mo alloy due to formation of Co-Ti intermetallic compound and β-Ti phase. All these improvements enhance durability and strength of Co-Cr-Mo-4Ti alloy along with a reduction in stress shielding effect as compared to the Co-Cr-Mo, making it more suitable for knee prothesis applications.
In this study, a numerical investigation is conducted to compare the impact of various ribs such as transverse, inclined, V-shaped and arc-shaped fixed on the absorber plate of a solar air heater under consistent boundary conditions. The analysis considers Reynolds numbers ranging from 3000 to 15000 and a heat flux corresponding to 1000 W m−2. Various geometric characteristics of the ribs, including relative roughness height, relative pitch, number of gaps, rib-arm angle (attack angle), and relative gap width, are kept constant throughout the investigation in this comparative analysis. The simulations are carried out using ANSYS-Fluent software, and the theoretical results are employed for validation. Results indicate that at Reynolds number 15,000, the maximum Thermal-Hydraulic Performance Parameter (THPP) for V-shaped ribs is 2.15 followed by arc-shaped ribs as 1.6.