In this study, Zn-Al ferrite/polypyrrole (PPy) nanocomposites were synthesized and thoroughly characterized to explore their potential for microwave applications. X-ray diffraction analysis confirmed the presence of ZnO, AlFeO3, and Fe2O3 phases, with the crystal size decreasing from 31 nm to 19.6 nm as aluminum content increased. High-resolution transmission electron microscopy (HR-TEM) revealed a distinctive core–shell morphology, where the polypyrrole encapsulates the ZnAlxFe2−xO4 particles. Magnetic measurements showed that decreasing aluminum concentration led to a reduction in both saturation magnetization (Ms) from 75 emu/g to 36 emu/g and remanent magnetization (Mr) from 2.26 emu/g to 2.00 emu/g. Dielectric analysis indicated that both the real (ε′) and imaginary (ε″) components of dielectric permittivity decreased with increasing frequency, particularly between 10 and 14 GHz. Furthermore, electrical modulus analysis highlighted the significant impact of aluminum doping on relaxation time (τIP), indicating the presence of interface polarization. Impedance spectroscopy results underscored the dominance of interface polarization at lower frequencies and the presence of strong conduction paths at higher frequencies. These combined magnetic and dielectric loss mechanisms suggest that the Zn-Al ferrite/polypyrrole nanocomposite is a promising candidate for advanced microwave absorption applications.
Fabrication of Cd0.5Zn0.5NdxFe2–xO4 nanoparticles, with x = 0.00, 0.01, 0.02, 0.04, 0.06, and 0.08, has been carried out using a wet chemical co-precipitation method. The effect of the rare earth Nd3+ doping on the prepared ferrites was structurally investigated using x-ray diffraction (XRD) along with Rietveld refinement. The results indicate great crystallinity in the FCC Fd3m spinel structure of Cd0.5Zn0.5NdxFe2–xO4 nanoparticles. The lattice parameter increases with the increase of doping concentration from 8.5378 until 8.5432 Å and the crystallite size obtained using Debye-Sherrer, Williamson–Hall, Size-strain plot (SSP), and Halder-Wagner (H-W) methods, decreases until the solubility limit of the materials is at x = 0.04. By using transmission electron microscopy (TEM), the morphological analysis reveals the spherical shape of the samples with minor agglomeration with the aid of using a Polyvinylpyrrolidone (PVP) capping agent. The grain size ranges from 14.37 to 15.24 nm. Raman spectroscopy verifies the incorporation of Nd3+ in the octahedral sites and the decrease in particle size. The elemental composition was verified using x-ray photoelectron spectroscopy (XPS). The magnetic properties were studied using a vibrating sample magnetometer (VSM) and it shows superparamagnetic behavior with a decrease in the saturation magnetization from 2.207 to 1.918 emu g−1 and an increase in coercivity from 7.194 to 14.397 G. The prepared materials were tested as liquefied petroleum gas (LPG) sensors by studying their sensitivity, selectivity, optimum working temperature, response, and recovery times. Nd3+ doping shows a great increase in LPG sensing sensitivity 4 to 20 times than the pure samples. The doping concentration also decreases the response and recovery times.
6 December 2008 in Journal of Alloys and Compounds