High-performance hybrid polymer blends can be prepared by blending different types of polymers to improve their properties. However, most polymer blends exhibit phase separation after blending. In this study, polymethylmethacrylate/polyethylene glycol (PMMA/PEG) polymer blends (70/30 and 30/70 w/w) were prepared by solution casting with and without ZnO nanoparticles (NPs) loading. The effect of loading ZnO nanoparticles on blend morphology, UV blocking, glass transition, melting, and crystallization were investigated. Without loading ZnO NP, the PMMA/PEG blends showed phase separation, especially the PEG-rich blend. Loading PMMA/PEG blend with ZnO NPs increased the miscibility of the blend and most of the ZnO NPs dispersed in the PEG phase. The interaction of the ZnO NPs with the blend polymers slightly decreased the intensity of infrared absorption of the functional groups. The UV-blocking properties of the blends increased by 15% and 20%, and the band gap energy values were 4.1 eV and 3.8 eV for the blends loaded with ZnO NPs with a PMMA/PEG ratio of 70/30 and 30/70, respectively. In addition, the glass transition temperature (Tg) increased by 14 °C, the crystallinity rate increased by 15%, the melting (Tm) and crystallization(Tc) temperatures increased by 2 °C and 14 °C, respectively, and the thermal stability increased by 25 °C compared to the PMMA/PEG blends without ZnO NP loading.
The development of poly(lactic acid) (PLA) nanocomposites incorporating urchin-like WO3 particles through a cost-effective solution-casting method has led to significant enhancements in structural, thermal, optical, and rheological properties. The incorporation of these WO3 particles up to 7 wt% resulted in the formation of an irregular honeycomb-like morphology with broad pore sizes ranging from 14.1 to 24.7 µm, as confirmed by SEM and EDX analysis. The urchin-like WO3 particles acted as effective nucleating agents, increasing the crystallinity of PLA from 40% to 50% and achieving an impressive overall crystallinity rate of 97%. Differential scanning calorimetry (DSC) revealed an 11 K reduction in the crystalline phase transition temperature while maintaining stable melting (Tm) and glass transition (Tg) temperatures. Thermal analysis indicated a significant decrease in the onset of degradation and maximum thermal stability (Tmax), with a reduction of 21 K due to the incorporation of the WO3 particles. Optical measurements showed enhancement of UV-blocking properties from 9% to 55% with the WO3 particle loading. Rheological tests demonstrated substantial improvements in viscoelastic properties, including a remarkable 30-fold increase in storage modulus, suggesting enhanced gel formation. Although the nanocomposites showed minimal antibacterial activity against Escherichia coli and Staphylococcus aureus, they exhibited significant antifungal activity against Candida albicans. These results underscore the potential of the PLA/WO3 nanocomposites for advanced material applications, particularly where enhanced mechanical, thermal, optical, and antifungal performance is required.