Fiber-reinforced polymer (FRP) jacketing/wrapping has become an attractive strengthening technique for concrete columns. Wrapping an existing concrete column with continuous FRP jackets with the fiber in the jacket being oriented in the hoop direction is referred to as FRP full wrapping strengthening technique. In practice, however, strengthening concrete columns with vertically discontinuous FRP strips is also favored and this technique is referred to as FRP partial wrapping strengthening technique. Existing research has demonstrated that FRP partial wrapping strengthening technique is a promising and economical alternative to the FRP full wrapping strengthening technique. Although extensive experimental investigations have hitherto been conducted on partially FRP-confined concrete columns, the confinement mechanics of confined concrete in partially FRP-confined circular columns remains unclear. In this paper, an experimental program consisting of fifteen column specimens was conducted and the test results were presented. A reliable three-dimensional (3D) finite element (FE) approach for modeling of partially FRP-confined circular columns was established. In the proposed FE approach, an accurate plastic-damage model for concrete under multiaxial compression is employed. The accuracy of the proposed FE approach was verified by comparisons between the numerical results and the test results. Numerical results from the verified FE approach were then presented to gain an improved understanding of the behavior of confined concrete in partially FRP-confined concrete columns.
Strengthening existing reinforced concrete (RC) columns using a partial wrapping strengthening technique (PWST) by fiber-reinforced polymer (FRP) strips has been widely implemented. However, compared with the confinement mechanism of confined concrete in columns strengthened with the FRP full wrapping strengthening technique (FWST), the confinement mechanism of confined concrete in FRP partially wrapped columns is less understood. This paper presents the results of an experimental investigation into the behavior of confined concrete in FRP partially wrapped square columns under axial compression. The effects of FRP strip width and thickness on stress–strain behavior were thoroughly investigated. The novel particle image velocimetry (PIV) non-contact strain sensing technique was adopted to measure the strain in the specimens. Results show that the axial strains as well as the hoop strains are generally larger at the mid-plane of adjacent FRP strips than those at the mid-plane of each FRP strip, and considerable variation in hoop strains along the height of the specimens was observed. Comparisons between the experimental results and predictions by existing design-oriented stress–strain models were carried out to examine the accuracy of the models. A new design-oriented stress–strain model is proposed for confined concrete in FRP partially wrapped square columns and the comparisons between laboratory results and predictions from the proposed model show that the proposed model is superior to the existing models.
The influence of different replacement ratios of steel-slag powder as cement-replacement material on the fracture performance of concrete is studied in this paper. A three-point bending fracture test is carried out on slag powder-cement-based concrete (SPC)-notched beams with steel-slag powder as cementitious materials, partially replacing cement (0%, 5%, 10%, 15%, and 20%). Load-deflection curves and load-crack-opening displacement curves of SPC-notched beams with five different replacement ratios of steel-slag powder were obtained. The effects of different steel-slag-powder replacement ratios on the fracture properties (fracture energy, fracture toughness, and double-K fracture parameters) of the SPC were analyzed and discussed. The results showed that the incorporation of appropriate steel-slag powder can affect the fracture performance of SPC. Compared with concrete without steel-slag powder, adding appropriate steel-slag powder can effectively improve the bond performance between aggregate and matrix because the steel-slag powder contains hydration activity substances such as calcium oxide and aluminium trioxide. The fracture energy and fracture toughness of SPC increased and then decreased with the increase in steel-slag-powder replacement ratios, and the SPC concrete showed best fracture performance with a 5% steel slag powder replacement ratio. Its fracture energy increases by 13.63% and fracture toughness increases by 53.22% compared with NC.
Geopolymer concrete (GC) has been gaining attention in research and engineering circles; however, it is a brittle material with poor tensile performance and crack resistance. To address these problems, we introduced fibers into GC. In this study, axial compression and scanning electron microscope (SEM) tests were carried out on polyvinyl alcohol (PVA) short fiber reinforced low-calcium fly ash-slag-based geopolymer concrete (PFRGC). The ratio of PVA short fibers and low-calcium fly ash on the compression behavior of fiber reinforced geopolymer concrete (FRGC) were investigated and discussed. The test results show that PVA fibers play a bridging role in the cracks of the specimen and bear the load together with the matrix, so the addition of PVA fibers delayed the crack propagation of GC under axial compression. However, with the increase of low-calcium fly ash/PVA fibers, the number of unreacted fly ash particles in PFRGCs increases. Too many unreacted fly ash particles make GC more prone to micro-cracks during loading, adversely affecting compressive properties. Therefore, the axial compressive strength, elastic modulus, and Poisson’s ratio of GC decrease with the increasing low-calcium fly ash/PVA fibers.
Fiber-reinforced polymer (FRP) has become increasingly popular in repairing existing steel-reinforced concrete (RC) members or constructing new structures. Although the quasi-static axial compression performance of FRP-confined concrete (FCC) has been comprehensively studied, its dynamic compression performance is not well understood, especially the dynamic compressive behavior of FRP-confined high-strength concrete (FCHC). This paper presents an experimental program that consists of quasi-static compression tests and Split-Hopkinson Pressure Bar (SHPB) impact tests on FRP-confined high-strength concrete. The effects of the FRP types, FRP confinement stiffness, and strain rate on the impact resistance of FCHC are carefully studied. The experimental results show that the strain rate effect is evident for FRP-confined high-strength concrete and the existence of the FRP greatly improves the dynamic compressive strength of high-strength concrete. An existing strength model is modified for impact strength of FCHC and the predicted results are compared with the test results. The results and discussions show that the proposed model is accurate and superior to the existing models.
Low carbon and high performance have become key trends in the development of construction materials. Understanding the mechanism by which curing conditions affect the mechanical properties of high-ductility geopolymer concrete (HDGC) is of significant importance. This study investigated three sealing curing temperatures (room temperature, 45 °C, and 60 °C) and four curing durations (1 day, 3 days, 5 days, and 7 days), while considering two final curing ages (7 days and 28 days) to explore their effects on the axial tensile and compressive properties of HDGC. The results showed that both 45 °C and 60 °C could improve the brittle failure of HDGC under axial compressive loading. However, curing at 60 °C and for durations longer than 1 day in an oven would catalyze the formation of eight-faced zeolite crystals within the slag–fly ash geopolymer matrix, and it could weaken the matrix’s pore structure and subsequently affect the material’s later strength development. Nevertheless, oven heat curing enhanced the bridging effect between the fibers and the matrix, partially compensating for the reduction in the initial tensile strength of HDGC. This follows the pseudo-strain-hardening material’s saturation cracking criterion to enhance the strain-hardening behavior of HDGC and improve its tensile energy absorption capacity. A curing condition of 45 °C for 5 days is recommended to maximize the ductility of HDGC. This study provides important theoretical support for the design and promotion of green, low-carbon, high-ductility composite materials.