This study evaluated the degree of conversion (DC), polymerization kinetics, and temperature of a new self-cure bulk-fill resin-based composite (Stela Automix, SDI). The study was divided into seven groups: (1) Stela Primer, (2) Stela Automix, (3) Stela Automix exposed to light for 20 s after 100 s, (4) Stela Primer with Stela Automix, (5) Stela Primer with Stela Automix and exposed to light for 20 s after 100 s, (6) Scotchbond Universal with Stela Automix, and (7) Scotchbond Universal with Stela Automix and exposed to light for 20 s after 100 s. The real-time reaction rates and DC at the bottom of 2 mm thick specimens at ∼32 °C were measured at 720 s after insertion using a spectrometer with an Attenuated Total Reflectance detector. The temperature of Stela, Stela exposed to light, Stela Primer with Stela, and Stela Primer with Stela exposed to light were measured by an infrared thermal camera in human molar teeth with Class I cavities. The temperature was recorded in real-time every 0.03 s for 720 s. The results were compared with ANOVA and Tukey's multiple comparison test (α = 0.05). The highest degree of conversion (DC) at the 2 mm depth was achieved when Stela Primer was combined with Stela (72.4 ± 3.5 % at 720 s). Stela could self-cure independently, but not as rapidly or effectively as when used with its Primer. The greatest temperature increase was for the light-cured Stela, followed by Stela Primer with Stela RBC exposed to light for 20 s. The Scotchbond Universal bonding system did not significantly increase the DC compared to Stela alone, except when exposed to light for 20 s, which slightly increased the final DC. Exposing Stela to light for 20 s did not improve the final DC of Stela as much as using the Stela Primer, but it did increase the temperature and prolonged the time taken to return to 37 °C. The Stela primer accelerates the degree of conversion of Stela. The reaction occurred rapidly and achieved a higher DC at the bottom of the specimens where the Stela was in contact with the Stela primer. Exposing Stela to light for 20 s is not recommended. Instead, Stela should be used with Stela Primer.
To determine if the PinkWave (PW) light-curing unit (LCU) that emits red and infrared (IR) light as well as violet and blue light improves the depth of cure and degree of conversion (DC) of resin-based composites (RBCs). The DC of RBCs at various distances was calculated from data collected at a rate of 13 Hz using attenuated total reflectance Fourier-transform infrared spectroscopy. To assess the contributions of the different wavelengths of light, optical filters were used to block the red and IR light from the PW. The depth of cure was also evaluated by photocuring RBC samples in both metal and plastic molds for 20 s at a 0 mm distance. The length of resin remaining was then measured and divided by 2. Starting from a baseline of 32 °C, the temperature rise during photocuring was measured in the plastic and metal rings reproducing the conditions used to measure the depth of cure and the DC respectively. In general, the PW produced greater depth of cure, however the use of metal molds greatly reduced this effect because the temperature increase was reduced. Increasing the distance by up to 4 mm from the light tip produced a significant increase in the DC for the RBCs photocured with the PW, but not for the G4. The wavelength of the blue peak (peaking at 473 nm) from the PW was longer compared to the control LCU (peaking at 448 nm). This 25 nm difference negatively affected the photocuring efficiency of some resins. The internal optics and the additional red and IR wavelengths from the PW significantly increased the temperature in the RBCs and increased both depth of cure and the DC.
Identifying the boundary between the tooth and the resin-based composite (RBC) is difficult when replacing restorations. Ultraviolet (UV) light has been reported to assist the viewer by causing the RBC to fluoresce. Using a laboratory-grade fiberoptic spectrometer, 46 RBCs were exposed to UV light from the Woodpecker O-Star curing light. The opalescence and fluorescence were measured relative to a human tooth that contained just dentin and a tooth that contained both enamel and dentin. After these quantitative measurements, 10 RBCs with large differences in light emittance were compared qualitatively to assess their brightness when exposed to UV light compared to the dentin specimen and the specimen containing both enamel and dentin. It was found that, when exposed to UV light, some of the RBCs were less bright compared to the two samples of teeth used for comparison, but most were brighter; some were up to six times brighter. The filler appears to affect the opalescence peaks, while the resin appears to affect the fluorescence peaks. It was concluded that because RBCs emit very different levels of opalescence and fluorescence, UV light from the Woodpecker O-Star cannot be relied upon to detect all brands of RBC on the tooth. The opalescence and fluorescence can also be used to detect changes in the formulation of the RBC.
This study measured the beam divergence angle and light output from dental light curing units (LCUs). Twenty LCUs were assessed using a laboratory-grade wide beam imager to determine the relationship between the beam divergence on the irradiance as a function of distance from the light tip. The irradiance (mW/cm2) and beam divergence angles (°) at 5, and 10 mm from the tips of 18 Light-Emitting Diode (LEDs), 1 Quartz-Tungsten-Halogen (QTH), and 1 Laser diode LCU. There were significant differences in the power, irradiance, and emission spectra from the 20 LCUs. At 10 mm from the LCU tip, the irradiance delivered by one LCU decreased by approximately 85.7 %, whereas this decrease was as low as 5.6 % for a different LCU. There was a positive correlation between the divergence angle reported by the wide beam imager and the reduction in irradiance. The laser diode LCU had the least beam divergence and the smallest decrease in irradiance as the distance increased. In contrast, the QTH LCU with the turbo light guide had the greatest beam divergence and the greatest reduction in irradiance as the distance increased. 50 % of the LCUs tested would require exposure times longer than 20 s to deliver 10 J/cm2 at the 10 mm distance. The wide beam imager is a useful tool for measuring the beam divergence from LCUs and predicting the effect of distance on their irradiance. At 10 mm, some LCUs may require a fivefold increase in the exposure time to deliver the same energy they deliver at 0 mm from the tip of the LCU.