Bi0.5Na0.5TiO3 (BNT) emerges as a promising ferroelectric and piezoelectric lead-free candidate to substitute the contaminant Pb[TixZr1−x]O3 (PZT). However, to obtain optimal ferroelectric and piezoelectric properties, BNT must be sintered at high temperatures. In this work, the reduction of sintering temperature by using iron added to BNT is demonstrated, without significant detriment to the dielectric properties. BNT-xFe with iron from x = 0 to 0.1 mol (∆x = 0.025) were synthesized using high-energy ball milling followed by sintering at 900 °C. XRD analysis confirmed the presence of rhombohedral BNT together with a new phase of NaFeTiO4 (NFT), which was also corroborated using optical and electronic microscopy. The relative permittivity, in the range of 400 to 500 across all the frequencies, demonstrated the stabilization effect of the iron in BNT. Additionally, the presence of iron elevates the transition from ferroelectric to paraelectric structure, increasing it from 330 °C in the iron-free sample to 370 °C in the sample with the maximum iron concentration (0.1 mol). The dielectric losses maintain constant values lower than 0.1. In this case, low dielectric loss values are ideal for ferroelectric and piezoelectric materials, as they ensure minimal energy dissipation. Likewise, the electrical conductivity maintains a semiconductor behavior across a range of 50 Hz to 1 × 106 Hz, indicating the potential of these materials for applications at different frequencies. Additionally, the piezoelectric constant (d33) values decrease slightly when low concentrations of iron are added, maintaining values between 30 and 48 pC/N for BNT-0.025Fe and BNT-0.05Fe, respectively.
En este trabajo, se evaluaron las características de la estructura cristalina, actividad fotocatalitica y propiedades magnéticas de la sillenita (Bi25FeO40). Se obtuvieron polvos de Bi25FeO40 mediante molienda de alta energía asistida con un tratamiento térmico a 700°C. La estructura cristalina, analizada mediante difracción de rayos X (DRX), reveló la obtención de Bi25FeO40 con alta pureza (100 %) y una estructura cristalina cúbica del tipo I23. La actividad fotocatalítica de la Bi25FeO40 se evalúo midiendo la eficiencia de degradación del colorante cristal violeta (CV) en un espectro de luz visible (desde 420 hasta 780 nm), exhibiendo una degradación de CV del 34 % en un lapso de 210 minutos, lo cual abre la posibilidad de que la Bi25FeO40 pueda operar bajo luz solar. La caracterización magnética obtenida mediante magnetometría de muestra vibrante (VSM) revela un comportamiento ferrimagnético con una magnetización de 0.054 emu/g. Lo anterior confirma la síntesis de un fotocatalizador recuperable magnéticamente.