Gold recovery from refractory pyrite-arsenopyrite concentrates using stirred tank reactor biooxidation is widely applied worldwide. Therefore, studies to address the characteristic problem of this technology are urgent. The goal of the present work was to research the possibility of counteracting the negative effects of unfavorable conditions (increasing pulp density and temperature) on the biooxidation of pyrite-arsenopyrite concentrate in laboratory-scale stirred tank reactors using additional carbon supply in the form of CO2. A refractory concentrate containing pyrite (48%) and arsenopyrite (13%) was used in biooxidation experiments. In the control experiment, biooxidation was performed under “normal conditions”: temperature 40 °C, pulp density (solid to liquid ratio, S:L) 1:10, residence time 5 days. It was shown that under “normal conditions”, additional carbon dioxide supply insignificantly affected the biooxidation rate and composition of the microbial population of biooxidation reactors. In addition, the effect of “stressful conditions” was studied. In this case, either temperature or pulp density were increased (up to 50 °C and S:L 1:5, respectively), which provided unfavorable conditions for biooxidation and led to the decrease in biooxidation rate. Under “stressful conditions”, additional carbon dioxide supply affected biooxidation to a greater extent and made it possible to increase both pyrite and arsenopyrite biooxidation rates. The analysis of microbial populations showed that additional carbon dioxide supply also changed their composition.
The goal of the present work was to perform biooxidation of a gold-bearing pyrite-arsenopyrite flotation concentrate under unfavorable conditions (decreased retention time). For this purpose, biooxidation of the concentrate containing 51% pyrite and 13% arsenopyrite was carried out in a continuous mode with a retention time of 5 days (i.e., under conditions corresponding to those used in industrial biooxidation facilities) and 3 days (i.e., under conditions unfavorable for the biooxidation). Reducing the retention time led to a decrease in the oxidation degree of sulfide minerals in the concentrate. Application of an additional carbon source (carbon dioxide) made it possible to neutralize the negative effect of reducing the retention time. Thus, it was shown that it is possible to significantly increase the rate of the biooxidation process by using carbon dioxide as an additional carbon source for the microbial population of the biooxidation reactor.