This study investigates the effect of annealing heat treatment on polymer composites composed entirely of biodegradable components. Poly(lactic acid) (PLA) was used as the matrix material paired with three different types of commercial lignocellulose fibers of varying sizes. Composites containing 10 wt.% fibers were processed through extrusion followed by injection molding. The amorphous (unannealed) and semi‐crystalline (annealed) samples were characterized for their morphological, thermal, mechanical, and water absorption properties. Scanning electron microscopic analysis revealed a homogenous distribution of cellulose fibers within the PLA matrix, even though the composite with the smallest fiber size exhibited slight agglomeration. Differential scanning calorimetric measurements indicated that the annealing heat treatment successfully induced crystallization, with the filler particles capable of increasing the extent of crystallinity formed during the annealing heat treatment from 28% to 36%. Based on the tensile tests, as a result of annealing heat treatment, the composites' strength increased from 48–50 to 53–56 MPa, while their Young's modulus increased from 3.1 GPa to 3.3‐3.5 GPa. The Charpy impact tests also revealed an enhanced toughness for the samples exposed to the annealing heat treatment. In terms of water absorption, annealing enhanced the hydrophobic nature of PLA. In addition, the semi‐crystalline structure formed during the heat treatment also inhibited the highly hydrophilic cellulose fibers from absorbing as much moisture as they did when incorporated inside amorphous PLA; cellulose fibers embedded in the semi‐crystalline PLA matrix consequently exhibited less moisture absorption than the ones in amorphous PLA.Highlights: Through annealing, crystallinity was developed in PLA/lignocellulose composites. Lignocellulose fibers facilitated crystallization by acting as a nucleating agent. Crystallized biocomposites exhibited superior mechanical properties Crystalline segments hindered the water absorption of embedded lignocellulose.
This study investigates the effect of filament moisture content on material extrusion (MEX) 3D-printed composites using acrylonitrile butadiene styrene (ABS) as the polymer matrix and 0–10 vol% hexagonal boron nitride (BN) as reinforcement. ABS/BN composites were prepared through batchwise compounding and extruded into MEX-suitable filaments. The filaments were conditioned at 30 °C and 10% or 90% relative humidity (RH) before/during direct feeding into the 3D printer. Specimens were fabricated with raster angles parallel (0°) and perpendicular (90°) to their length. Micro- and macrostructural analyses using scanning electron microscopy and computed tomography revealed intensive void formation, especially in BN-filled composites 3D-printed from humid filaments. This was attributed to BN acting as a physical barrier, hindering the outgassing of evaporated water during 3D printing. Mechanical properties were evaluated using tensile and Charpy impact tests. Based on the tensile test results, neat ABS was the least sensitive to filament moisture, with tensile strength at 0° raster angle dropping from 40.5 MPa to 36.7 MPa as storage RH was increased from 10 to 90%. For composites with 10 vol% BN loading, tensile strength dropped from 34.1 MPa to 22.3 MPa. Charpy impact strength exhibited similar reductions, ascribed to the porous structure of the BN-filled composites caused by the evaporated moisture. Thermal conductivity was also examined, showing slightly superior performance for samples 3D-printed from filaments stored in less humid conditions. For unfilled ABS, the conductivity slightly decreased from 0.188 to 0.185 W/mK, while for 10 vol% BN-filled composite, it dropped from 0.778 to 0.617 W/mK.
Thermoplastic polyurethane (TPU) filament was used to fabricate specimens through material extrusion (MEX)-based 3D printing technique with varying printing parameters. Nozzle diameters of 0.4 mm and 0.8 mm were used, while the printing infill orientation (also denoted as raster angle) was either parallel (0°) to the length of the specimens, perpendicular to it (90°), or at a 45° angle with alternating direction in each layer (±45°). Tensile tests were conducted to determine tensile strength, Young’s modulus, and elongation at break of the samples. The highest tensile strength was achieved using a 0.8 mm nozzle diameter and 0° raster angle, reaching 32.5 MPa, with a corresponding Young’s modulus of 145.8 MPa. Meanwhile, the sample with the lowest modulus (100.4 MPa) and tensile strength (17.8 MPa) was the one 3D-printed with a 0.4 mm nozzle and 90° raster angle.
21 November 2025 in Macromolecular Materials and Engineering
This study evaluated the changes in the molecular structure, as well as the thermal and mechanical properties of poly‐lactic‐acid (PLA), during successive closed‐loop mechanical recycling through injection molding. Gel permeation chromatographic (GPC) analyses revealed a gradual decrease in molar mass (MM); after ten recycling steps, the MM of PLA was reduced to one‐third of its initial value. According to differential scanning calorimetric (DSC) measurements, both the glass transition temperature and the cold crystallization temperature of PLA decreased, while the crystallization was facilitated by the successive recycling steps. This was ascribed to the improved chain mobility resulting from the reduced MM. Quasi‐static mechanical properties were evaluated using tensile tests, while impact toughness was assessed through Charpy tests. The tensile strength of PLA was not significantly affected by recycling until the fifth recycling step, where it suffered a slight (∼5%) reduction. Meanwhile, Young's modulus, elongation at yield, and impact strength remained approximately the same as the freshly injected sample at that point. However, after ten recycling steps, all analyzed properties declined significantly: Young's modulus by 11%, tensile strength by 68%, elongation at yield by 63%, and impact strength by 30%.