Purpose: This paper aims to examine the impact of three-dimensional (3D) printing technological modes (using fused deposition modelling [FDM]) on physical and mechanical properties of samples from polyphenylenesulfone. Design/methodology/approach: For this study, the standard test samples were printed using the FDM method at different filament orientation angles, the gaps between them and a different width. The basic physical and mechanical properties, such as the strength, the elastic modulus and the impact strength, were studied. Findings: The authors found that the basic mechanical properties strongly depend on the printing settings. In particular, the elastic modulus generally depends on the air gap between rasters, and it is practically independent of the filament orientation angle. In contrast, the impact strength depends on the orientation and the degree of adhesion between filaments: the highest values are reached at the longitudinal orientation of rasters in the sample (0°) and the minimum value of the air gap (−0.025 mm). However, in selecting the optimal mode of 3D printing, it is necessary to take into account the specific geometry of the printing products and the direction of the stress that it will experience. Originality/value: The paper presents the results of the investigation of the influence of FDM printing modes on the mechanical properties of samples from polyphenylenesulfone, including impact strength. The authors studied the mechanisms of the destruction under impact loading and revealed the optimal printing settings for making samples with properties which are not inferior to the injection molded samples.
In this work, PPSUs with different molecular weights were synthesized for the development of highly permeable ultrafiltration hollow fiber membranes for the first time. The MW of the synthesized polymers was controlled by varying the monomers molar ratio within 1:1–1.15 under the same synthesis conditions. Based on the study of the rheological properties of polymer solutions, a high molecular weight PPSU (MW = 102,000 g/mol) was chosen for the formation of hollow fiber membranes. The addition of PEG400 to the spinning solution led to an increase in viscosity, which makes it possible to work in the region of lower PPSU concentrations (18–20 wt. %) and to form membranes with a less dense porous structure. With the addition of PEG400 to the spinning solution, the membrane permeance increased sharply by more than two orders of magnitude (from 0.2 to 96 L/m2·h bar). At the same time, the membranes had high rejection coefficients (99.9%) of Blue Dextran model filtered substance (MW = 69,000 g/mol).
For the first time, polysulfones (PSFs) were synthesized with chlorine and hydroxyl terminal groups and studied for the task of producing porous hollow fiber membranes. The synthesis was carried out in dimethylacetamide (DMAc) at various excesses of 2,2-bis(4-hydroxyphenyl)propane (Bisphenol A) and 4,4′-dichlorodiphenylsulfone, as well as at an equimolar ratio of monomers in various aprotic solvents. The synthesized polymers were studied by nuclear magnetic resonance (NMR), differential scanning calorimetry, gel permeation chromatography (GPC), and the coagulation values of 2 wt.% PSF polymer solutions in N-methyl-2-pyrollidone were determined. According to GPC data, PSFs were obtained in a wide range of molecular weights Mw from 22 to 128 kg/mol. NMR analysis confirmed the presence of terminal groups of a certain type in accordance with the use of the corresponding monomer excess in the synthesis process. Based on the obtained results on the dynamic viscosity of dope solutions, promising samples of the synthesized PSF were selected to produce porous hollow fiber membranes. The selected polymers had predominantly –OH terminal groups and their molecular weight was in the range of 55–79 kg/mol. It was found that porous hollow fiber membrane from PSF with Mw 65 kg/mol (synthesized in DMAc with an excess of Bisphenol A 1%) has a high helium permeability of 45 m3/m2∙h∙bar and selectivity α (He/N2) = 2.3. This membrane is a good candidate to be used as a porous support for thin-film composite hollow fiber membrane fabrication.
For the first time, membranes based on poly(1-trimethylsilyl-1-propyne) (PTMSP) with 5–50 wt% loading of hyper-crosslinked polystyrene sorbent particles (HCPS) were obtained; the membranes were investigated for the problem of effective removal of volatile organic compounds from aqueous solutions using vacuum pervaporation. The industrial HCPS sorbent Purolite Macronet™ MN200 was chosen due to its high sorption capacity for organic solvents. It has been found that the membranes are asymmetric when HCPS content is higher than 30 wt%; scanning electron microscopy of the cross-sections the membranes demonstrate that they have a clearly defined thin layer, consisting mainly of PTMSP, and a thick porous layer, consisting mainly of HCPS. The transport and separation characteristics of PTMSP membranes with different HCPS loading were studied during the pervaporation separation of binary and multicomponent mixtures of water with benzene, toluene and xylene. It was shown that the addition of HCPS up to 30 wt% not only increases the permeate fluxes by 4–7 times, but at the same time leads to 1.5–2 fold increase in the separation factor. It was possible to obtain separation factors exceeding 1000 for all studied mixtures at high permeate fluxes (0.5–1 kg/m2∙h) in pervaporation separation of binary solutions.
Polyetheretherketone (PEEK) is a promising polymer material for tribological applications. Friction and wear tests of PEEK samples versus steel with different melt flow indices (MFI) were studied. The results showed dependencies of the friction force on the sliding velocity, either decreasing or increasing depending on whether the normal load exceeds the yield strength of the polymer. The data can be well fitted with the assumption of the two-component friction law involving the Amontons component and an adhesional component. With a decrease in MFI, i.e., with an increase in viscosity of polymer, the adhesive component of friction increases with increasing viscosity while the abrasive wear decreases. At high loads, the plastic displacement increases with an increase in the viscosity and plasticity of the polymer. The wear does not show a clear correlation with the viscosity.