The paper focuses on material characterization and technology properties of a new Ti-12Al-42Nb spherical powder alloy for additive manufacturing of personal medical implants. The electrode induction melting inert gas atomization (EIGA) method was used to produce the powder alloy. The powder sphericity coefficient (PSC) was 1.02. Image J software was used to calculate the spherical degree by processing images sets from scanning electron microscopy (SEM) and optical microscopy (OM). SEM of particles cross-sections indicated internal thermal-induced porosity (TIP) with a 2.3 μm pore diameter. Particle size distribution was in the range from 15.72 μm (d10) to 64.48 μm (d100) as measured by laser particle analyzer. It was indicated that flowability and powder bulk density were 196 sec and 2.79 g/cm3, respectively. XRD analysis confirmed the beta phase of the powder alloy with no additional phases. X-ray fluorescence spectrometry confirmed the alloyed composition. Reducing and oxidative melting methods of analysis showed a slight amount of impurities: oxygen (0.0087 wt.%), nitrogen (0.03 wt.%), hydrogen (0.0012 wt.%), sulfur (0.0016 wt.%), and carbon (0.022 wt.%). Simultaneous thermal analysis (STA) was performed to indicate weight growth and losses and thermal effects in argon, nitrogen, and air as well as the oxidation of Al2O3, TiO2, and Nb2O5 on the surface layer of Ti-12Al-42Nb powder alloy particles. Different phase transformations of γAl2O3 θAl2O3 αAl2O3 and TiO2 rutile TiO2 anatase phase transformation were detected by STA in the oxidative layer.
Hydrogels have a wide range of medical applications, including use within implantable systems. However, when used in implants, their visibility under conventional medical imaging techniques is limited, creating safety risks for patients. In the current work, we assessed the possibility of enhancing hydrogels using Ln-based contrasting agents to facilitate their visualization in photon-counting computed tomography (PCCT). The contrast enhancement of gelatin, polyacrylamide (PAM), and silicone shells of implants was assessed. A novel synthetic route for producing cross-linked nanosized Ln2O3 with polyacrylamide was proposed and discussed in detail. Several prototypes of silicone implants, including silicone shell and gelatin or PAM filling with different combinations of contrasting agents, were produced and assessed in phantom PCCT studies.
Objectives. To obtain porous corundum ceramics using an innovative cold sintering process starting from different phase modifications of aluminum oxohydroxide — boehmite γ-AlOOH and diaspore α-AlOOH; to study the phase and structural properties of the resulting materials; and to assess their permeability to water.Results. Cold sintering enables the formation of single-phase corundum ceramics with an open porosity of 47.9% directly from the initial boehmite powder with the addition of 5 wt % corundum in the presence of 20 wt % water at a temperature of 450°C, mechanical pressure of 220 MPa, and isothermal exposure for 30 min. Under the same conditions of cold sintering, a mixture of diaspore and boehmite was transformed into α-AlOOH ceramics. This then turned into corundum with an open porosity of 39% when calcined in air at 600°C for 1 h. The resulting materials had permeability for pure water above 5000 L/(m2∙h∙bar).Conclusions. Cold sintering is a promising approach to producing porous corundum ceramics which can be used in filtration systems. Compared to traditional ceramic technology, the new approach reduces energy, time, and labor costs in the material manufacturing. It also eliminates the need to use auxiliary substances (binders, pore-forming agents, etc.).