Measuring the low carbon performance of buildings is a crucial method for achieving the construction industry's strategic goal of “double carbon.” The carbon emission factor calculation approach proposed by the IPCC is utilized to create a carbon emission calculation model for a steel-concrete composite structure bridge across its whole life cycle. The discount rate is used to determine the dynamic carbon emissions of the steel-concrete composite structural bridge, which are then compared to the static carbon emissions. The carbon strength of the bridge is evaluated using a fuzzy comprehensive technique. The application analysis is conducted on the basis of a steel-concrete composite construction bridge in Beijing. According to the findings, carbon emissions are primarily concentrated during the preparation, production, and operation of building materials. The bridge's static and dynamic carbon emissions are 103.966 and 1378.674 ktCO 2 e, respectively. After material recovery, the values are 95.141 ktCO 2 e and 1107.751 ktCO 2 e, respectively. The ratio of dynamic and static carbon emissions ranges from 7 to 34, highlighting the significance of temporal value. After recycling the components, the bridge's static carbon strength dropped from 2.565 to 2.353, while its dynamic carbon strength fell from 2.422 to 2.210, both of which were medium carbon strengths. The model proposed in this study can successfully examine the carbon emissions and strength of bridges from both environmental and economic perspectives, and it can be used to select more environmentally friendly building materials and construction methods to increase bridge efficiency. It also provides valuable data assistance for the establishment and execution of environmental protection measures, thereby promoting the industry's long-term sustainable development.
The corrosive environment in the western region will adversely affect the fatigue performance of bridges. In order to determine the influence of the corrosion environment in western China on the fatigue failure of bridges, this paper simulated corrosion environment characteristics in northwest China, conducted alternating corrosion and high-cycle fatigue experiments on Q420 bridge steel, and used Origin (2019b 64Bit) to fit S-N curves of specimens with different corrosion periods to study the influence of corrosion damage in western China on their fatigue properties. Based on the damage theory, the corrosion fatigue failure degree of Q420 bridge steel was analyzed, and the crack propagation law was revealed by microscopic scanning of the fracture. The findings indicate that the damage to Q420 bridge steel progressively worsens with more prolonged corrosion exposure in the deicing salt conditions of western China. The 60-day corrosion resulted in a rust rate ηs of 2.17% and a corrosion rate K of 1.413 mm/a. The fatigue life of Q420 bridge steel is significantly affected by the coupling of stress level and corrosion damage. After 60 days of corrosion, the specimen’s fatigue limit decreases by 12.28%, which accelerates the fatigue property degradation rate of the specimen. The damage index effectively represents the internal damage behavior of materials under corrosion fatigue conditions. Fatigue damage escalates as the corrosion period extends, and the number of fatigue bands decreases, with the stress corrosion threshold σth diminishing by 1.77%, 3.55%, 4.61%, and 6.38% across various corrosion durations. The research results are significant for the fatigue failure prediction and reliability analysis of Q420 bridge steel in a deicing salt corrosion environment in western China.