Bone tissue engineering has seen significant advancements with innovative scaffold fabrication techniques such as 3D printing. This review focuses on enhancing polycaprolactone (PCL) scaffold properties through structural modifications, including surface treatments, pore architecture adjustments, and the incorporation of biomaterials like hydroxyapatite (HA). These modifications aim to improve scaffold conformation, cellular behavior, and mechanical performance, with particular emphasis on the role of mesenchymal stem cells (MSCs) in bone regeneration. The review also explores the potential of integrating nanomaterials and graphene oxide (GO) to further enhance the mechanical and biological properties of PCL scaffolds. Future directions involve optimizing scaffold structures and compositions for improved bone tissue regeneration outcomes.
Although poly(2-hydroxyethyl methacrylate) (pHEMA) and polyethylene glycol methacrylate (PEGMA) have been demonstrated to inhibit bacterial adhesion, no study has compared antibacterial adhesion when salivary pellicle is coated on polymethyl methacrylate (PMMA) grafted with pHEMA and on PMMA grafted with PEGMA. In this study, PMMA discs were fabricated from a commercial orthodontic acrylic resin system (Ortho-Jet). Attenuated total reflection-Fourier transform infrared spectra taken before and after grafting confirmed that pHEMA and PEGMA were successfully grafted on PMMA. Contact angle measurements revealed PMMA-pHEMA to be the most hydrophilic, followed by PMMA-PEGMA, and then by PMMA. Zeta potential analysis revealed the most negative surface charges on PMMA-PEGMA, followed by PMMA-pHEMA, and then by PMMA. Confocal laser scanning microscopy showed green fluorescence in the background, indicating images that influenced the accuracy of the quantification of live bacteria. Both the optical density value measured at 600 nm and single plate-serial dilution spotting showed that pHEMA was more effective than PEGMA against Escherichia coli and Streptococcus mutans, although the difference was not significant. Therefore, the grafting of pHEMA and PEGMA separately on PMMA is effective against bacterial adhesion, even after the grafted PMMA were coated with salivary pellicle. Surface hydrophilicity, bactericidality, and Coulomb repulsion between the negatively charged bacteria and the grafted surface contributed to the effectiveness.
The effects of alumina particle size and jet pressure on the bond strength of polyetheretherketone (PEEK) were examined to determine the airborne particle abrasion parameters with minimal effects on PEEK and to achieve optimal bond strength, as a reference for future clinical use. An alumina particle with four particle sizes and three jet pressures was used to air-abrade PEEK. Surface roughness (Ra), morphology, chemical structure, and wettability were analyzed using a stylus profilometer, scanning electron microscope, X-ray diffractometer, and contact angle analyzer, respectively. The shear bond strength (SBS) of PEEK and dental resin cement was analyzed using a universal testing machine (n = 10). The failure modes and debonded fracture surfaces were observed using optical microscopy. Airborne particle abrasion increased the Ra and hydrophobicity of PEEK and deposited alumina residues. The SBS generally decreased after thermal cycling. A large particle size damaged the PEEK surface. The effects of different particle sizes and jet pressures on the SBS were only significant in certain groups. Adhesive failure was the main mode for all groups. Within the limitations of this study, 110 μm grain-sized alumina particles combined with a jet pressure of 2 bar prevented damage to PEEK, providing sufficient SBS and bonding durability between PEEK and dental resin cement.
11 August 2022 in Journal of Materials Chemistry B
Poly(γ-benzyl-L-glutamate) (PBG) made biomimetic scaffolds are explored as candidate materials for corneal nerve regeneration and neurotrophic keratopathy treatment. The PBG with built-in neurotransmitter glutamate was synthesized and fabricated into 3D fibrous scaffolds containing aligned fibers using electrospinning. In in vitro experiments, primary mouse trigeminal ganglia (TG) cells were used. Immunohistochemistry (IHC) analysis shows that TG cells cultured on PBG have no cytotoxic response for 21 days. Without any nerve growth factor, TG cells have the longest neurite length of 225.3 μm in the PBG group and 1.3 times the average length as compared with the polycaprolactone and no scaffold groups. Also, aligned fibers guide the neurite growth and extension unidirectionally. In vivo assays were carried out by intracorneal implantation of PBG on clinical New Zealand rabbits. The external eye photos and in vivo confocal microscopy (IVCM) show a low immune response. The corneal neural markers (βIII tubulin and SMI312) in the IHC analysis are consistent with the position stained by glutamate of implanted scaffolds, indicating that PBG induces neurogenesis. PBG exhibits mechanical stiffness to resist material deformation possibly caused by surgical operations. The results of this study demonstrate that PBG is suitable for corneal nerve regeneration and the treatment of neurotrophic keratopathy.
Mesoporous bioactive glass (MBG) is an advanced biomaterial widely recognized for its application in bone regenerative engineering. This study synthesized an MBG powder (80 mol% SiO2, 5 mol% P2O5, and 15 mol% CaO) using a facile sol-gel method with the non-ionic surfactant Pluronic® P123, which acted as a pore-forming agent. MBGs form bioactive surfaces that facilitate HA formation, and the presence of Pluronic® P123 increases the surface area and promotes HA nucleation. Various percentages of strontium (Sr) doping were examined to improve bioreactivity, biological response, and bone formation, with 3SMBG (3 mol% Sr) showing the highest specific surface area. In vitro biocompatibility tests revealed HA formation on all glass surfaces after immersion in simulated body fluid (SBF), indicated by sheet-like HA morphologies, the presence of PO43− and CO32− functional groups, and the amorphous structure along with SrCO3 crystalline phases corresponding to HA and Sr-HA structures. Sr doping resulted in delayed initial degradation and sustained release of Sr2+, achieving over 95% cell viability. Surfactant-induced mesoporous structure and Sr incorporation synergistically enhance osteocyte induction and formation in vitro. These findings suggest that Sr-doped MBG, particularly with P123-assisted Sr/Ca substitution, optimizes the material’s properties for advanced bone regenerative applications.