High boron steel is prone to brittle failure due to the boride distributed in it with net-like or fishbone morphology, which limit its applications. The Quenching and Partitioning (Q&P) heat treatment is a promising process to produce martensitic steel with excellent mechanical properties, especially high toughness by increasing the volume fraction of retained austensite (RA) in the martensitic matrix. In this work, the Q&P heat treatment is used to improve the inherent defect of insufficient toughness of high boron steel, and the effect mechanism of this process on microstructure transformation and the change of mechanical properties of the steel has also been investigated. The high boron steel as-casted is composed of martensite, retained austensite (RA) and eutectic borides. A proper quenching and partitioning heat treatment leads to a significant change of the microstructure and mechanical properties of the steel. The net-like and fishbone-like boride is partially broken and spheroidized. The volume fraction of RA increases from 10% in the as-cast condition to 19%, and its morphology also changes from blocky to film-like. Although the macro-hardness has slightly reduced, the toughness is significantly increased up to 7.5 J·cm−2, and the wear resistance is also improved.
10 June 2020 in International Journal of Minerals, Metallurgy and Materials
The oxidation kinetics and behavior of vanadium carbide particle-reinforced Fe-based composites (VCps-Fe-MC) were investigated at 600, 800, and 950 °C. The microstructure of the surface and cross-section of the oxidation layer was characterized by scanning electron microscope (SEM). The composition of the surface of the oxide scales was examined by X-ray diffraction (XRD) and energy-dispersive spectroscopy (EDS). The micro hardness of the specimens was measured by a micro-hardness tester after a high-temperature treatment and subsequent air cooling. The results showed that the growth of the oxide scales on the VCps-Fe-MC followed a parabolic curve with an increase in the oxidation time. In addition, the weight gain increased with the oxidation temperature during the same period. Different oxide scales and oxidation rates occurred in some regions due to different textures. The minimum oxidation rate was in the austenite region because of a high silicon and chromium contents. At the same time, severe cracking and large shedding of the oxide scales were discovered due to growth stress and thermal stress. These defects can provide channels for oxygen diffusion. Based on the micro-hardness values, temperatures greater than 900 °C can be regarded as austenitizing temperatures during heat treatment to improve the mechanical properties and the wear resistance.