Redox polymerization of poly(acrylonitrile-co-acrylic acid) (poly(AN-co-AA)) is performed at 40 °C under N2 gas by varying the ratio of acrylonitrile (AN) and acrylic acid (AA) in the feed. The yield production of poly(acrylonitrile) (PAN) is 73% and poly(AN-co-AA) with a feed ratio of 93:7 is the highest yield (72%). The PAN and poly(AN-co-AA) are further chemically modify with hydroxylamine hydrochloride. The FTIR spectroscopy is used to confirm the copolymerization of poly(AN-co-AA) and chemical modification of poly(AN-co-AA). Elemental microanalysis shows that the overall trend percentage of carbon, hydrogen, and nitrogen for all feed ratios are slightly decreasing as the feed ratio of AA is increasing except for poly(AN-co-AA) 93:7. The SEM images shows that spherical diameter of poly(AN-co-AA) is smaller compared to the PAN and amidoxime (AO) modified poly(AN-co-AA). The TGA (thermogravimetric analysis) analysis reveals that the poly(AN-co-AA) degrades at lower temperatures compared to the PAN but higher than AO modified poly(AN-co-AA). The case study adsorption test showed that the AO modified poly(AN-co-AA) 93:7 had the highest percentage removal of Cd2+ and Pb2+.
This research focuses on deducing the kinetic mechanism for biodiesel production catalyzed by a CaO nanocatalyst derived from waste cockle shells via thermal hydration–dehydration treatment. In addition, the CaO nanocatalyst preparation method via thermal hydration–dehydration-related parameters (hydration duration, recalcination temperature, and recalcination duration) was studied and optimized. The transesterification reaction catalyzed by the CaO nanocatalyst followed the Langmuir–Hinshelwood kinetic mechanism with surface reaction as the rate-limiting step. The relatively low activation energy (3786.7 J/mol) for a transesterification reaction offered by the CaO nanocatalyst enhanced the reaction rate to 27.3% FAME yield/hr. The optimal conditions for the thermal hydration–dehydration treatment used to develop the nano CaO catalyst were 6 h of hydration duration, 650 °C of recalcination temperature, and 3 h of recalcination duration. Of biodiesel yield, 94.13% was obtained at a moderate temperature of 60 °C and 3 h reaction time during the transesterification of palm oil catalyzed by the nano-CaO. SEM, BET, and TPD results proved that the CaO nanocatalyst had a large surface area (13.9113 m2/g) and high pore volume (0.0318 cm3/g) that were rich in active sites (1046.46 μmol CO2/g), and the pore diameter (33.17 nm) was accessible to reactants and products.
11 October 2023 in Asia-Pacific Journal of Chemical Engineering
Direct ink writing (DIW) enables the additive manufacturing of silicone elastomers, offering an alternative to traditional moulding and casting methods for applications from healthcare products to machine–human interaction sensors. Polydimethylsiloxane (PDMS) foam, a porous silicone elastomer, is valued for its elasticity, chemical and thermal resistance, hydrophobicity, and biocompatibility. The emulsion templating method is a simple and cost-effective approach to create silicone foams by incorporating and later removing a sacrificial dispersed phase from the PDMS precursor. This study developed glycerol/PDMS emulsion-based inks for DIW using high-shear centrifugal mixing, with ethanol as a solvent to remove the glycerol template, creating silicone foam. An optimal glycerol dosage of 50 parts per hundred rubber (phr) produced foam with 27.63% porosity and pore diameter up to 4.66 µm. Each 10 phr increase in glycerol content raised porosity by 10% and average pore diameter by 2 µm. Both tensile and compressive behaviour inversely correlated with porosity, with a 10% porosity rise in the silicone foam reducing tensile strength by 0.07 MPa and stiffness by 0.02 MPa. Models with strong data alignment were developed to benefit researchers in 3D printing to customize silicone foams (pore properties, mechanical properties, compressive properties) based on specific application requirements.
Complex three-dimensional (3D) silicone structures with functional properties for medical applications can be produced using 3D printing technology. The printability of extrusion-based 3D silicone structure is dependent on precise control of silicone rheological behaviour, especially shear-thinning behaviour and static yield stress. However, the rheology behaviour of silicone elastomer limits its fabrication technique to the moulding process, which is more suited for mass production but not small batch production and prototyping. In this study, a custom condensation-cured room temperature vulcanisation (RTV-1) silicone is formulated for an extrusion-based 3D printer to tackle this problem. Pure silicone polymer lacks key rheology behaviours to ensure a successfully 3D print. The roles and impacts of crosslinkers, catalyst and filler (nano-silica) on the rheology properties of silicone were investigated. Through the rheology characterisation of the formulated silicone materials, the critical component in contributing to the success of extrusion-based silicone printing can be identified.
Direct ink writing (DIW) enables the additive manufacturing of silicone elastomers, offering an alternative to traditional moulding and casting methods for applications such as healthcare products to machine-human interaction sensors. Polydimethylsiloxane (PDMS) foam, a porous silicone elastomer, is valued for its elasticity, chemical and thermal resistance, hydrophobicity, and biocompatibility. The emulsion templating method is a simple and cost-effective approach to create silicone foams by incorporating and later removing of sacrificial dispersed phase from the PDMS precursor. This study developed glycerol/PDMS emulsion-based inks for DIW using high-shear centrifugal mixing, with ethanol as a solvent to remove the glycerol template, creating silicone foam. An optimal glycerol dosage of 50 parts per hundred rubber (phr) produced foam with 27.63% porosity and pore diameter up to 4.66 µm. Each 10 phr increase in glycerol content raised porosity by 10% and average pore diameter by 2 µm. Both tensile and compressive behaviour inversely correlated with porosity, with a 10% porosity rise in the silicone foam reducing tensile strength by 0.07 MPa and stiffness by 0.02 MPa. Models with strong data alignment were developed to benefit researchers in 3D printing to customize silicone foams (pores properties, mechanical properties, compressive properties) based on specific application requirements.