This research focuses on deducing the kinetic mechanism for biodiesel production catalyzed by a CaO nanocatalyst derived from waste cockle shells via thermal hydration–dehydration treatment. In addition, the CaO nanocatalyst preparation method via thermal hydration–dehydration-related parameters (hydration duration, recalcination temperature, and recalcination duration) was studied and optimized. The transesterification reaction catalyzed by the CaO nanocatalyst followed the Langmuir–Hinshelwood kinetic mechanism with surface reaction as the rate-limiting step. The relatively low activation energy (3786.7 J/mol) for a transesterification reaction offered by the CaO nanocatalyst enhanced the reaction rate to 27.3% FAME yield/hr. The optimal conditions for the thermal hydration–dehydration treatment used to develop the nano CaO catalyst were 6 h of hydration duration, 650 °C of recalcination temperature, and 3 h of recalcination duration. Of biodiesel yield, 94.13% was obtained at a moderate temperature of 60 °C and 3 h reaction time during the transesterification of palm oil catalyzed by the nano-CaO. SEM, BET, and TPD results proved that the CaO nanocatalyst had a large surface area (13.9113 m2/g) and high pore volume (0.0318 cm3/g) that were rich in active sites (1046.46 μmol CO2/g), and the pore diameter (33.17 nm) was accessible to reactants and products.
1 June 2019 in IOP Conference Series: Earth and Environmental Science
Currently, carbon capture and storage (CCS) technology appeared to be the most viable method to reduce carbon dioxide (CO2) emission from its existing sources. This paper reports the improved performance of calcium oxide (CaO)-based sorbents with the addition of nickel oxide (NiO) as an additive (denoted as CaO:NiO) in CO2 sorption process (CaO carbonation reaction). Pure CaO was used as benchmarked sorbent in this study. The samples were synthesized using the sol-gel method and CaO:NiO were evaluated for their performance in CaO carbonation at different sorption temperatures, from its CO2 sorption capacity, CO2 sorption rate, and kinetic performance. CaO:NiO has demonstrated an excellent CO2 sorption capacity of 0.79 mmol CO2/mmol CaO, meanwhile pure CaO exhibited lower CO2 sorption capacity of 0.61 mmol CO2/mmol CaO at 600 °C. During the chemical reaction controlled stage, the CO2 sorption rate of CaO:NiO was 0.78 mmol CO2/mmol CaO.min at 600 °C compared to pure CaO with sorption rate of 0.18 mmol CO2/mmol CaO.min. This study indicates that the addition of nickel oxide has successfully improved the CO2 sorption rate and capacity of CaO for CaO:NiO. Based on the kinetic study, it has been observed that the diffusion controlled stage has a greater resistance towards the CO2 sorption process (carbonation reaction) compared to rapid chemical reaction controlled stage. Experimental carbonation data for CaO:NiO fitted very well to the shrinking core model (SCM) with high correlation coefficient (R2 >0.936). The specific rate constants of rapid chemical reaction and diffusion-limited stages are directly proportional to the carbonation temperature. The activation energy required for CaO:NiO sorbent during the chemical reaction control stage was 31.81 kJ/mol.
Direct ink writing (DIW) enables the additive manufacturing of silicone elastomers, offering an alternative to traditional moulding and casting methods for applications from healthcare products to machine–human interaction sensors. Polydimethylsiloxane (PDMS) foam, a porous silicone elastomer, is valued for its elasticity, chemical and thermal resistance, hydrophobicity, and biocompatibility. The emulsion templating method is a simple and cost-effective approach to create silicone foams by incorporating and later removing a sacrificial dispersed phase from the PDMS precursor. This study developed glycerol/PDMS emulsion-based inks for DIW using high-shear centrifugal mixing, with ethanol as a solvent to remove the glycerol template, creating silicone foam. An optimal glycerol dosage of 50 parts per hundred rubber (phr) produced foam with 27.63% porosity and pore diameter up to 4.66 µm. Each 10 phr increase in glycerol content raised porosity by 10% and average pore diameter by 2 µm. Both tensile and compressive behaviour inversely correlated with porosity, with a 10% porosity rise in the silicone foam reducing tensile strength by 0.07 MPa and stiffness by 0.02 MPa. Models with strong data alignment were developed to benefit researchers in 3D printing to customize silicone foams (pore properties, mechanical properties, compressive properties) based on specific application requirements.
20 May 2025 in Journal of Analytical and Applied Pyrolysis
Zeolite has been identified as a potential low-temperature CO₂ adsorbent with the highest adsorption capacity among adsorbents in its category. However, its adsorption capacity remains relatively low, limiting its industrial application for CO₂ adsorption. Additionally, there is a need to increase the optimal adsorption temperature of this porous material to effectively adsorb CO₂ emitted from flue gas, which has an average temperature of 100 - 125°C. To address these challenges, a preliminary study on Zn-doped zeolite has been conducted. This study aims to investigate the ability of Zn-doped zeolite to enhance CO₂ adsorption capacity and its effect on the optimal temperature for CO₂ adsorption. Zinc-doped zeolite was synthesized by doping zinc oxide into natural zeolite using a zinc ion exchange method at different doping concentrations (0.2 M & 1.0 M). Undoped natural zeolite was studied as a benchmark. Their CO₂ adsorption performance was tested using TGA at 30°C, 50°C, and 100°C. The effects of temperature and doping concentration on adsorption capacity were investigated. The adsorbent samples were characterized using X-ray Diffraction (XRD) and Scanning Electron Microscopy (SEM) with Energy Dispersive X-ray (EDX) analysis. It was found that increasing the temperature from 30°C to 50°C increased the CO₂ adsorption capacity, but the capacity decreased when the temperature was further increased to 100°C. Furthermore, increasing the doping concentration tended to enhance the CO₂ adsorption capacity. The highest adsorption capacity of 0.0281 g CO₂/g sorbent was observed in zinc-doped zeolite with a 1.0 M doping concentration at 50°C. The improvement was mainly attributed to the zinc oxide doped on the zeolite, which provided a functional group that formed chemical bonds with CO₂. This study also found that the adsorption rate of CO₂ was predominantly influenced by temperature, while the effect of doping concentration was less significant. All testing and characterization results suggested that the zinc-ion exchange method improved the CO₂ adsorption capacity of zeolite.
The abundant sawdust waste from the timber production industries in Malaysia can be a potential biomass feedstock for pyrolysis process. However, the understanding of product composition and bio-oil quality from sawdust pyrolysis remains limited in Malaysian’s context. In this study, pyrolysis of sawdust was conducted in a horizontal tube furnace to investigate the effects of temperatures (400-550 °C) and heating rates (10-20 °C/min) on the composition of products, quality and properties of bio-oil. According to Gas chromatography (GC) analysis, phenol group appears to be the major compound in the bio-oil. The chemical components of bio-oil were found to be richer at lower reaction temperatures (400-450 °C), where it showcased the presence of phenols, ketones, carboxylic acids, furans, aldehydes, alkenes, alcohols, ether and amine. At increased reaction temperatures (500–550 °C), the process favoured the production of catechol (17%). The yield of bio-char decreased with increasing temperatures and heating rates due to the loss of volatile matter, and 400 °C proved to be the optimum temperature for maximum biochar yield. The biochar also displays porous structure, with increased adsorption capacity. Since the pyrolysis of sawdust could produce phenolic compounds, it appears to be a potential feedstock for biomass pyrolysis.