Anna Cremona

Dr. Anna Cremona

orcid

Research Focus & Metrics

Academic Career Length

19Years (2008-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
30 November 2012 in Applied Surface Science
Verified
Journal Article
Closed access
EVE. Vassallo
E. Vassallo
RCR. Caniello
R. Caniello
ACAnna Cremona
Anna Cremona
DDDavid Dellasega
David Dellasega
Enrico MiorinEnrico Miorin
Enrico Miorin

1 December 2018 in Nuclear Materials and Energy
Verified
Journal Article
Open access
ACAnna Cremona
Anna Cremona
EVE. Vassallo
E. Vassallo
EAE. Alves
E. Alves
FCF. Causa
F. Causa
SISilvana De Iuliis
Silvana De Iuliis
AUA. Uccello
A. Uccello

1 January 2017 in Nuclear Materials and Energy
Verified
Journal Article
Open access
RCR. Caniello
R. Caniello
AUA. Uccello
A. Uccello
FGFrancesco Ghezzi
Francesco Ghezzi
DMD. Minelli
D. Minelli
IRI. Bogdanović Radović
I. Bogdanović Radović
EVE. Vassallo
E. Vassallo
Iron-tungsten (Fe-W) mixed films were exposed to the low flux deuterium plasma of GyM in order to study the behavior of the sputtering yield with the ion fluence and temperature of the samples. From literature, it is known that an increase of the former lowers the Fe-W layers’ sputtering yield as a consequence of the preferential sputtering of Fe leading to an enrichment in W of the outermost layers. An opposite trend was instead found for the latter probably due to the inter-diffusion of Fe and W (effective from 200 °C) resulting in the suppression of the W enrichment. Moreover, from 500 °C, also W segregation to the surface occurs. What is missing from literature is a systematic investigation of the role of temperature on W enrichment. In this work, dedicated experiments in GyM were carried out to fill this gap. After exposure, W enrichment was evaluated by Rutherford Backscattering Spectrometry (RBS) and inferred from measuring the eroded thickness of the samples using RBS and profilometer. Concerning the Fe-W sputtering yield as a function of fluence, it decreases by a factor of ∼3 between the lowest (3.0×1022D+m−2) and the highest fluence (9.0×1023D+m−2) values considered. The other main result is that, at the lowest fluence, the exposure at room temperature leads to an erosion of the Fe-W samples more pronounced than that associated to the exposure at 500 °C

1 April 2025 in Nuclear Fusion
Verified
Journal Article
Open access
AUAndrea Uccello
Andrea Uccello
GAGabriele Alberti
Gabriele Alberti
MPMateto Pedroni
Mateto Pedroni
ACAnna Cremona
Anna Cremona
FGFrancesco Ghezzi
Francesco Ghezzi
TTthe GyM Team
the GyM Team
This work investigates the role of surface topography in the sputtering process of tungsten (W) exposed to helium plasma using the GyM linear device. Surfaces with varying roughness, from sub-nanometer to approximately 1 µm, and different textures, including random-like and regular configurations, were studied. The samples were exposed to helium plasma of GyM at energies ranging from 30 to 350 eV, with a fluence of ≈ 4.3 × 10 24 He+m−2 and temperatures well below the bulk W fuzz formation threshold of ≈700 ∘C. The interpretation of the experimental results was supported by simulations with the 3D Monte Carlo ERO2.0 code. Analysis with atomic force and scanning electron microscopy revealed that surface topography remained largely unchanged, while a nanoscale undulating surface structure formed on all samples at the highest incident energies. The effective sputtering yield ( Y eff ) of tungsten, derived from mass and thickness loss data, was consistently lower than predictions from simulations by up to an order of magnitude, likely due to the dynamic retention of helium on the tungsten surface. On the other hand, both experimental results and modelling agree that surface topography’s influence on sputtering can be entirely captured by the average surface inclination angle ( δ m ), which unequivocally characterises each specimen, unlike the average roughness ( R a ). Moreover, Y eff values from both mass loss data and ERO2.0 simulations as a function of δ m align well with a decreasing sigmoid fit function. A reduction of more than 50% was observed when comparing the flat surface to that with the highest R a , attributed by ERO2.0 to the increasing fraction of sputtered tungsten atoms being deposited on neighbouring surfaces. These findings underscore the importance of accurately calibrating simulation tools against linear plasma device experiments for predicting the lifetime of plasma-facing components in fusion reactors such as ITER and DEMO, emphasising the potential of structured tungsten surfaces to reduce erosion and impurity concentration in the plasma core.


1 June 2016 in Nuclear Instruments and Methods in Physics Research Section A: Accelerators, Spectrometers, Detectors and Associated Equipment
Verified
Journal Article
Closed access
CCCarlo Cazzaniga
Carlo Cazzaniga
ACAnna Cremona
Anna Cremona
Massimo NocenteMassimo Nocente
Massimo Nocente
MRM. Rebai
M. Rebai
DRD. Rigamonti
D. Rigamonti
Giuseppe GoriniGiuseppe Gorini
Giuseppe Gorini