Herein, we demonstrate the successful synthesis of novel Fe80Si9B(11−x)Px (x = 0, 1, 3, 5, 7) ultra-thick amorphous ribbons by planar flow casting. The influence of P alloying on glass forming ability (GFA), microstructure, thermal stability, soft magnetic properties, and ductility has been systematically investigated. The results reveal that introduction of P into Fe80Si9B11 alloy can remarkably enhance the GFA and increase critical thickness (tc) of the alloy from 45 to 89 um. Furthermore, the annealed FeSiBP amorphous alloys exhibited excellent soft magnetic properties, including high saturation magnetic flux density of 1.54 T, the low coercivity of 1.5 A/m, and low core losses of 0.15 W/kg. In addition, the representative Fe80Si9B8P3 ultra-thick amorphous alloy demonstrate excellent ductility even after annealing at 400 °C for 10 min, which indicates the superior performance of P-doped FeSiB alloys as compared to the commercial Fe78Si9B13 (Metglas 2605 S2) alloy. The combination of high GFA, excellent ductility, and low core losses of newly developed FeSiBP amorphous soft magnetic alloys makes them attractive candidates for magnetic applications in the high-frequency and high-speed electric devices.
FeSiBCuNb powders prepared by the gas atomization method generally exhibit a wide particle size distribution and a high degree of sphericity. In addition, the correspondingly prepared nanocrystalline soft magnetic composites (NSMCs) perform good service stability. In this paper, effects of the gas-atomization pressure and annealing temperature on the microstructure and soft magnetic properties of FeSiBCuNb powders and NSMCs are investigated. The results show that the powders obtained by a higher gas-atomization pressure possess a larger amorphous ratio and a smaller average crystallite size, which contribute to the better soft magnetic performance of the NSMCs. After being annealed at 550 °C for 60 min, the NSMCs show a much better performance than those treated by the stress-relief annealing process under 300 °C, which indicates that the optimization of the soft magnetic properties resulting from the precipitation of the α-Fe(Si) nanocrystalline largely overwhelms the deterioration caused by the grain growth of the pre-existing crystals. In addition, the annealed NSMCs prepared by the powders with the gas-atomization pressure of 4 MPa show the best performance in this work, μe = 33.32 (f = 100 kHz), Hc = 73.08 A/m and Pcv = 33.242 mW/cm3 (f = 100 kHz, Bm = 20 mT, sine wave).
This research paper investigated the impact of normal annealing (NA) and magnetic field annealing (FA) on the soft magnetic properties and microstructure of Fe82Si2B13P1C3 amorphous alloy iron cores. The annealing process involved various methods of magnetic field application: transverse magnetic field annealing (TFA), longitudinal magnetic field annealing (LFA), transverse magnetic field annealing followed by longitudinal magnetic field annealing (TLFA) and longitudinal magnetic field annealing followed by transverse magnetic field annealing (LTFA). The annealed samples were subjected to testing and analysis using techniques such as differential scanning calorimetry (DSC), transmission electron microscopy (TEM), X-ray diffraction (XRD), magnetic performance testing equipment and magneto-optical Kerr microscopy. The obtained results were then compared with those of commercially produced Fe80Si9B11. Fe82Si2B13P1C3 demonstrated the lowest loss of P1.4T,2kHz = 8.1 W/kg when annealed in a transverse magnetic field at 370 °C, which was 17% lower than that of Fe80Si9B11. When influenced by the longitudinal magnetic field, the magnetization curve tended to become more rectangular, and the coercivity (B3500A/m) of Fe82Si2B13P1C3 reached 1.6 T, which was 0.05 T higher than that of Fe80Si9B11. During the 370 °C annealing process of the Fe82Si2B13P1C3 amorphous iron core, the internal stress in the strip gradually dissipated, and impurity domains such as fingerprint domains disappeared and aligned with the length direction of the strip. Consequently, wide strip domains with low resistance and easy magnetization were formed, thereby reducing the overall loss of the amorphous iron core.
In this paper, the corrosion resistance of FeCoSiBPC amorphous alloy after pre-oxidation and non-oxidation heat treatment is investigated. The corrosion behaviors of Fe80Co3Si3B10P1C3 amorphous alloys in 1 mol/L NaCl solution were investigated by the electrochemical workstation. The pre-oxidation heat treatment can improve the corrosion resistance of FeCoSiBPC amorphous alloy through an increase in the Ecorr value from −0.736 to −0.668 V, which makes it easy to reach a passive state. The corroded morphology and products of amorphous alloys were tested by scanning electron microscopy (SEM) and transmission electron microscopy (TEM). The SEM/TEM analysis showed that, after pre-oxidation treatment, the oxide layer was divided into two layers: the inner layer was amorphous, the outer layer appeared crystalline, and the main oxide was Fe2O3. During the oxidation process, Co and P elements diffused from the inner layer to the outer layer, forming phosphorus and cobalt oxides with high corrosion resistance on the surface of the ribbon, thereby improving the corrosion resistance of the ribbon.
31 August 2016 in Science China Technological Sciences
The research on how to reduce energy consumption and improve the efficiency of amorphous motors has extensive coverage. This study systematically investigates the influence of internal stress induced by impregnation curing and interference fit on the soft magnetic properties and loss characteristics of Fe80Co3Si3B10P1C3 (CAF4) amorphous alloy iron cores. The amorphous iron core samples undergo analysis through differential scanning calorimetry (DSC), transmission electron microscopy (TEM), X-ray diffraction (XRD), magnetic performance testing equipment, flexible pressure sensors, and magnetostriction testers. The CAF4 amorphous iron core after impregnation curing (AIC) exhibits the lowest loss of P1.2T,1.5 kHz = 22.8 W/kg when annealed at 260 °C, representing a 21% increase compared to the pre-impregnation curing (BIC) state. Within the commonly utilized interference fit range, the loss growth rate of CAF4 amorphous iron cores is lower than that of Fe80Si9B11 (1K101). Likewise, at a frequency of 50 Hz and an excitation of 1000 A/m, the magnetostriction coefficient of CAF4 is smaller than that of 1K101. Within the typical interference fit range, the magnetization performance of CAF4 amorphous iron cores surpasses that of 1K101, favoring lightweight and compact motor designs and reducing copper losses. Consequently, CAF4 amorphous iron cores exhibit significant advantages when employed in motors.