The purpose of this study is to investigate the effects of process parameters on the microstructure and mechanical properties of the Hastelloy X (HX) alloy using a laser powder bed fusion (L-PBF) process. A combined experimental and numerical approach was used to evaluate the influence of the energy density distribution and temperature evolution on the microstructure, defects, and mechanical properties. After the specimens were built on SUS304 substrate by the L-PBF, the microstructure and defects in the specimens were analyzed by SEM and EBSD analysis methods, and then the hardness and the tensile tests were performed. The cooling rate under different laser conditions was obtained by the finite element method (FEM). The results show that a low volume energy density (VED) was applied to the unmelted powder particles, and a high energy density resulted in spherical defects. In addition, the microstructures were found to coarsen with increasing the energy density along with a tendency to strengthen the (001) texture orientation in both x–y and x–z planes. Compared to the parts with the thermal history from numerical results, the low cooling rate with high energy density had larger crystal grains elongated along the building direction, coarser sub-grains, resulting in a reduction in microhardness and yield strength together with an increase in elongation for the L-PBF HX alloy. The presented results provide new insights into the effects of parameters and the cooling rates. It can play an important role in optimizing the L-PBF processing parameters, identifying the cause of defects, and controlling the cooling rates for the crystallographic texture in such a way as to guide the development of better metrics for designing processing parameters with the desired mechanical properties.
20 January 2026 in Journal of Materials Research and Technology
This research aims to produce TiO2-based composite powder by growing of carbon nanotubes (CNTs) on the surface of micron-sized TiO2 particles using a chemical vapor deposition (CVD) technique. This nanocomposite powder will be further used as feedstock powder to build up as a coating using a thermal spray technique. This coating is expected to have better photocatalytic efficiency over that of pure TiO2 coating. For composite powder preparation, rutile-phase of TiO2 powder with particle size in a range of 25 – 45 µm was used as a starting powder. The powder was placed in a CVD apparatus under ethanol atmosphere as a carbon source. The best CNTs growing condition was found to be 650°C for 60 min. The starting powder and as-synthesized composite powders were characterized by scanning electron microscopy, energy dispersive spectrum, Raman spectroscopy and UV-vis spectroscopy. The results showed that CNTs were successfully grown in-situ on the surface of TiO2 particles. The photocatalytic activities under visible-light were examined based on a degradation of methylene blue. The degradation efficiency of the TiO2/CNTs composite powder was found to be higher than that of pure TiO2. It is expected that the TiO2/CNTs nanocomposite powder could be further used to fabricate various of nanocomposite products.