It is known that there is a correlation between hydration heat and physico-mechanical properties of wood based cement panels. Cement hydration is affected by many variables, such as chemical composition, water/cement ratio, wood/cement ratio, wood chemical properties, mineral additions and producing conditions. This study mainly aimed to investigate the effects of press temperature on some properties of three-layer cement bonded particleboard made from the particles of spruce (Picea orientalis) and poplar (Populus tremula). For this purpose, a total of 16 experimental board groups with 1200 kg/m3 target density and 1/3 wood-cement ratio were produced at the press temperatures of (20, 30, 40, 50, 60, 70 and 80) °C. As cement curing accelerator, CaCl2 was used at a rate of 5 % (cement weight basis). The physical, mechanical and thermal properties of the boards were determined. The results indicated that the press temperature substantially affected the properties of cement-bonded particleboard depending on the wood species. In the light of this study, the optimum temperatures in producing of cement-bonded particleboard were found as 40 °C for poplar wood and 60 °C for spruce wood.
The aim of this research was to investigate the physico-mechanical, thermal, and morphological properties of cement-bonded wood particleboards produced by using fly as has a partial cement replacement and spruce planer shavings. Experimental single-layer cement-bonded wood particleboards produced using a target density of 1200 kg/m3, 1/3 wood-cement ratio, a dimension of 460x460x10 mm3 and 5%, 10%, 15%, 20% fly ash as cement replacement were tested for physical and mechanical properties in accordance with EN and ASTM standards. Moreover, morphological and thermal properties of the cement-bonded wood particleboards were analysed by using the scanning electron microscope and thermogravimetric analysis-derivative thermogravimetry. Test results indicated that the fly ash enhanced both the bending strength and water-resistance of the cement-bonded wood particleboards. Internal bond and screw withdrawal strengths tended to decrease as the fly ash content increased in the cement-bonded wood particleboards, but this decrease was not statistically significant. As the fly ash increased, the weight loss of the cement-bonded wood particleboards decreased in the thermogravimetric analysis because of the pozzolonic reaction of the fly ash with calcium hydroxide. In the scanning electron microscope, it was observed that calcium silicate hydrate gel increased, whereas calcium hydroxide decreased as the usageratio of the fly ash increased in the cement-bonded wood particleboards.
1 July 2015 in Procedia - Social and Behavioral Sciences
In this study, the effects of hardener type (ammonium chloride and ammonium nitrate) and board thickness on the physical (density, thickness swelling and water absorption), mechanical (modulus of rupture, modulus of elasticity, internal bond strength, screw withdrawal resistance and surface durability) and formaldehyde content of particleboard were investigated. Three types panels were produced using 11-9% urea-formaldehyde adhesive (core and surface, respectively), with 650kg/m3 target density, 150°C pressing temperature, 20-24kg/cm2 pressure, and 6min of pressing time. The analyses revealed that use of ammonium nitrate for particleboard manufacturing resulted in improved water absorption and thickness swelling properties after 24h of immersion in water. In addition, the using ammonium nitrate has no significant effect by Modulus of rupture (MOR) and modulus of elasticity (MOE). However, internal bond strength, screw withdrawal resistance and surface durability properties were positively affected by using ammonium nitrate. Formaldehyde content value was decreased by about 5%. The study demonstrated that the boards made of ammonium nitrate meet the requirements for general standard and building materials
31 December 2019 in Journal of Anatolian Environmental and Animal Sciences
In this study, it is aimed to determine the effect of the use of different types cement and accelerator on the physico-mechanical properties of cement-bonded particleboards. Within this scope, two types of cements (calcium aluminate cement and Super white CEM I 52.5 R) and accelerators (aluminum sulfate and calcium chloride) were used in the production of boards. Therefore, CBPBs with 1200 kg/m3 target density and 1/2.75 wood-cement ratio were produced. Based on cement weight 1.5% accelerators were used. The test results obtained were evaluated according to EN 634-2 (2009). According to result, density values of the boards were changed with using depending on cement and accelerator types. The use of super white cement and calcium chloride positively affected the both mechanical properties and dimensional stability of the boards. The use of calcium aluminate cement and aluminum sulfate resulted in lower strength properties.
The effect of using duroplast sanitary ware waste as a substitute for wood materials in cement-bonded wood panels was evaluated. Utilizing these wastes can provide considerable economic and environmental benefits by reducing the use of wood materials and the deposits in landfills. Cement-bonded wood panels were produced with the replacement of spruce wood materials by the duroplast sanitary ware waste particles in 10 wt%, 20 wt%, 30 wt%, and 40 wt%. The produced panels were examined in terms of physical, thermal, mechanical, and morphological properties and compared with the related standards. Experimental findings demonstrated that water absorption, moisture content, and thickness swelling values of the panels were enhanced by the addition of duroplast sanitary ware waste. The duroplast sanitary ware waste did not affect the density of the panels. The bending strength and the modulus of elasticity of the cement-bonded wood panels can be increased up to 23 % and 5,6 %, respectively, by the addition of 10 wt% duroplast sanitary ware waste particles. However, the internal bond strength and the screw withdrawal resistance values were reduced by an increment in the use of duroplast sanitary ware waste. The scanning electron microscope observation revealed that there was no mechanical interlocking between the duroplast sanitary ware waste and cement, and the formations of voids in the panels increased with an increase in the duroplast sanitary ware waste particle content. The thermal analysis showed that the use of duroplast sanitary ware waste resulted in increased cement hydration products due to the reduction in the wood content of cement-bonded wood panels.