The purpose of this paper is to analyze the main issues concerned with the oxidative and storage stabilities of biodiesel and how they affect different metallic and polymeric materials present in automotive parts and in biodiesel storage structures. In addition, this work presents a review of the techniques used for measuring the oxidative stability and for evaluating the degradation of metallic and polymeric materials. When biodiesel is oxidized, a series of changes in its properties occurs. These changes not only affect biodiesel quality, but also the properties of the materials that are in contact with it. Upon oxidation, biodiesel properties like the acid value, peroxide value and viscosity increase, while the iodine value and the content of methyl esters decrease. The changes in the chemical and physical properties of biodiesel can affect the integrity and stability of the material. The situation reviewed in this paper, which talks about the stability of materials, could limit the extensive use of biodiesel. Such measures have been proposed in several countries, and it is a topic of great importance for biodiesel technology.
The aim of the present work is to evaluate the impact of pure palm biodiesel fuel (B100) and biodiesel blends with 0.32% oleic, palmitic, acetic, myristic, and stearic acids on the properties of some polymeric materials used commonly in the manufacture of auto parts such as the polyamide 66 (PA66), polyoxymethylene (POM), and high-density polyethylene (HDPE). The effects of the B100 and B100–acid blends on polymeric materials were examined by comparing changes in the gain/loss of mass and by measuring the hardness, the impact strength, and the tensile strength of the materials at the end of the exposure. The characterization of the polymers was carried out before and after exposure by using differential scanning calorimetry (DSC), thermogravimetric analysis (TGA), and Fourier transform infrared spectroscopy (FTIR). After the immersion in B100–acids blends, the HDPE exhibited an increase in mass of 5%, which was very similar in all blends. The PA66 showed a small decrease in weight (2% approx.) in all mixtures. The POM presented an increase in the percentage of weight in the mixture of B100 with acetic acid of 0.3%. A decrease was observed in the crystallinity of the HDPE when exposed to blends of B100–acids. This behavior may be associated with a plasticizing effect in the HDPE exposed to the blends. The mechanical properties of POM and HDPE showed no significant changes after immersion in the fuels. On the other hand, PA66 exhibited a significant decrease in maximum stress value after immersion in B100, B100–oleic acid and B100–palmitic acid blends. The variation of the mechanical properties of the PA66 after exposure to B100 was potentiated by addition of organic acids. The assessed polymers did not undergo appreciable changes in the chemical structure of the samples after immersion in the fuels, so the variation in the mechanical properties could be explained by physical absorption of the fuel into the polymers.
In this paper, we describe the synthesis and characterization of alkoxylated TEMPO, (2,2,6,6-tetramethylpiperidin-1-yl)oxyl, radicals with potential application in organic non-aqueous redox flow batteries. The behavior of a series of TEMPO derivatives with varying lengths of alkoxy chain is analyzed in acetonitrile solutions using electrochemical techniques, electron paramagnetic resonance (EPR) spectroscopy, and measurements of permeability through three different membranes. Electrochemical redox potentials are only weakly dependent on the substituent, but, in contrast, exchange current densities derived from the data do depend on the substitution. EPR lends further insight into these properties via the determination of hyperfine splitting constant and rotational correlation time. There is a negligible effect of the substituents on those parameters among the modified TEMPO radicals. Finally, permeation rates of modified TEMPO derivatives through membranes depend significantly on both the membrane and the substitution of TEMPO, providing insights into capacity fade measurements in the literature.