In this study, fracture parameters of epoxy/glass functionally graded composite were determined experimentally using the digital image correlation (DIC) method. A functionally graded material (FGM) with continuous variation in elastic properties was manufactured by gravity casting in vertical template. A 30% volume fraction of glass spheres was dispersed in a low viscosity resin. A single edge crack specimen was examined in a three-point bending test under mode Ⅰ loading with cracks along the gradient tendency of the material properties. The mechanical properties of FGM were calculated according to ASTM D638. The DIC technique was adopted to obtain the deformation region around the crack tip. William's series was employed to calculate stress intensity factor and T-stress. The experimental results then verified by solving the FE model using ABAQUS program. The comparison between DIC and numerical results illustrated a largely acceptable achievement.
Surface roughness plays a vital role in determining surface integrity and function. Surface irregularities or reduced quality near the surface can contribute to material failure. Surface roughness is considered a crucial factor in estimating the fatigue life of structures welded by FSW. This study attempts to provide a deeper understanding of the nature of the surface formation and roughness of aluminum joints during FSW processes. In order to form more efficient joints, the frictional temperature generated was monitored until reaching 450 °C, where the transverse movement of the tool and the joint welding began. Hardness and tensile tests showed that the formed joints were good, which paved the way for more reliable surface roughness measurements. The surface roughness of the weld joint was measured along the weld line at three symmetrical levels using welding parameters that included a rotational speed of 1250 rpm, a welding speed of 71 mm/min, and a tilt angle of 1.5°. The average hardness in the stir zone was measured at 64 HV, compared to 50 HV in the base material, indicating a strengthening effect induced by the welding process. In terms of tensile strength, the FSW joint exhibited a maximum force of 2.759 kN. Average roughness (Rz), arithmetic center roughness (Ra), and maximum peak-to-valley height (Rt) were measured. The results showed that along the weld line and at all levels, the roughness coefficients (Rz, Ra, and Rt) gradually increased from the beginning of the weld line to its end. The roughness Rz varies from start to finish, ranging between 9.84 μm and 16.87 μm on the RS and 8.77 μm and 13.98 μm on the AS, leveling off slightly toward the end as the heat input stabilizes. The obtained surface roughness and mechanical properties can give an in-depth understanding of the joint surface forming and increase the ability to overcome cracks and defects. Consequently, this approach, using adaptive thresholding image processing coupled with grayscale histogram analysis, yielded significant understanding of the FSW joint’s surface texture.
This paper presents a robust dual-loop control strategy for the lateral motion and heading-angle regulation of an autonomous vehicle equipped with a Steer-By-Wire (SBW) system under unknown time-varying disturbances. The proposed framework comprises a fuzzy PID controller in the inner loop to generate the motor torque and track the front-wheel steering angle, and an optimal backstepping controller in the outer loop—integrated with a finite-time disturbance observer—to ensure lateral trajectory tracking and wind-disturbance rejection. The PID gains are tuned online by a Mamdani-type fuzzy inference system, while the backstepping parameters are optimized offline via a genetic algorithm. Beyond the bicycle-model-based design, the controller is evaluated through supplementary simulations using a 6-degree-of-freedom (6-DOF) vehicle model, as well as through a detailed robustness analysis that includes measurement noise and increasing lateral disturbance forces. The results demonstrate that the closed-loop system achieves precise path tracking, finite-time convergence of both tracking and estimation errors, and effective compensation of road vibrations and wind disturbances. Furthermore, the controller maintains stable performance under significant measurement noise and tolerates lateral disturbance forces up to at least 10,000 N without violating safety constraints. The effectiveness of the proposed method is consistently confirmed across both the reduced-order bicycle model and the higher-fidelity 6-DOF validation environment.
31 December 2022 in Periodicals of Engineering and Natural Sciences (PEN)
Repair of cracked pipeline under internal pressure has been investigated in the present study. To this aim, an experimental test has been done on the cracked pipeline to find failure pressure. A longitudinal crack that cut 65% thickness of pipe has been applied on the external surface. Carbon fiber reinforced polymer has been used to repair the system. Additionally, a finite element model has been developed to estimate failure pressure of the unrepaired pipes. The results show that the failure pressure in unrepaired pipes is identical to the failure pressure predicted by the standards for corroded pipes, however, the failure pressure of repaired system is lower than the predicted results of standard for corroded pipelines.
This research describes crack analysis in the functionally graded materials (FGMs) by adopting the extended element free Galerkin method (XEFGM) under mixed mode and asymmetric loading. These loads are somewhat similar to fatigue loads because, numerically, they are load values from zero and then directly to the critical load. The meshfree method can be easily simulated the fracture problems against the traditional numerical method because it is not dependent on mesh. Triangles technique in the process of numerical integration at regions of discontinuity, functions of enrichment, and as well as the appropriate support field to contain numerical points and nodes to from the shape functions are used in this study. In addition, incompatible interaction integration technique has used to determine the stress intensity factors (SIFs). Two study cases with different crack positions were studied and compared with the experimental works of the relevant reference literature, where accurate and identical results were obtained.
Welding lightweight materials such as aluminium and magnesium ensures optimal structural integrity in welded joints; this is essential for applications that require high strength and durability, as improper welding conditions can lead to defects and reduced load-bearing capacity. Friction stir spot welding (FSSW) is an effective method for joining similar and dissimilar lightweight metals, even with differences in their densities and melting points. The structural integrity of FSSW joints depends on factors such as material properties, process parameters, and tool design, which affect the mechanical performance of the joint and its fatigue resistance. This study investigates the mechanical properties of aluminium alloy EN AW 2024-T4 and magnesium alloy AZ31B, as well as their joint performance with FSSW. The study focuses on the structural integrity of welded joints through three scenarios. The first is by conducting a tensile test for the base metal of both metals to show that they are qualified in yield strength and ultimate tensile strength values. The second scenario the study includes the effect of sheet thickness on the tensile shear force of the welded joint by taking three thicknesses. The last scenario represents the effect of the shoulder-face configuration on the tensile shear force. The results show that the smaller the sheet thickness, the weaker is the weld joint. Also, a zigzag configuration for shoulder-face configuration can give the highest structural integrity, and a configuration consisting of concentric circles can lead to the worst structural integrity of the joint.