This paper demonstrates the application of ultra-precision cutting to the fabrication of ridged LiNbO3 waveguides for use in low-loss photonic integrated circuits. Ridged waveguides with sidewall verticality of 88° and ultra-smooth sidewalls were obtained in LiNbO3 crystals using this technique. In addition, the possibility of fabricating bent ridged waveguides via this mechanical micromachining method was examined. The root mean square surface roughness of the machined sidewall was 4.5 nm over an area of 2.5 × 10 µm, which is sufficiently low so as to minimize scattering losses of guided light. The propagation loss of the ridged waveguide produced during this work was well below 1 dB/cm at a wavelength of 1550 nm. The present technique should have significant applicability to the micromachining of ferroelectric materials and the fabrication of highly confined optical waveguides such as ridged waveguides and photonic wires.
24 May 2018 in Japanese Journal of Applied Physics
In this paper, we report room-temperature bonding of LiNbO 3 (LN) and SiO 2 /Si for the realization of a LN on insulator (LNOI)/Si hybrid wafer. We investigate the applicability of a modified surface activated bonding (SAB) method for the direct bonding of LN and a thermally grown SiO 2 layer. The modified SAB method using ion beam bombardment demonstrates the room-temperature wafer bonding of LN and SiO 2 . The bonded wafer was successfully cut into 0.5 × 0.5 mm 2 dies without interfacial debonding owing to the applied stress during dicing. In addition, the surface energy of the bonded wafer was estimated to be approximately 1.8 J/m 2 using the crack opening method. These results indicate that a strong bond strength can be achieved, which may be sufficient for device applications.
In this study, room-temperature wafer bonding of Al2O3 thin films on Si thermal oxide wafers, which were deposited using atomic layer deposition (ALD), was realized using the surface-activated bonding (SAB) method. Transmission electron microscopy (TEM) observations indicated that these room-temperature-bonded Al2O3 thin films appeared to work well as nanoadhesives that formed strong bond between thermally oxidized Si films. The perfect dicing of the bonded wafer into dimensions of 0.5 mm × 0.5 mm was successful, and the surface energy, which is indicative of the bond strength, was estimated to be approximately 1.5 J/m2. These results indicate that strong bonds can be formed, which may be sufficient for device applications. In addition, the applicability of different Al2O3 microstructures in the SAB method was investigated, and the effectiveness of applying ALD Al2O3 was experimentally verified. This successful SAB of Al2O3 thin films, which is a promising insulator material, opens the possibility of future room-temperature heterogenous integration and wafer-level packaging.
This paper focuses on the residual stress in a lithium niobate (LN) film layer of a LN-on-insulator (LNOI)/Si hybrid wafer. This stress originates from a large mismatch between the thermal expansion coefficients of the layers. A modified surface-activated bonding method achieved fabrication of a thin-film LNOI/Si hybrid wafer. This low-temperature bonding method at 100 °C showed a strong bond between the LN and SiO2 layers, which is sufficient to withstand the wafer thinning to a LN thickness of approximately 5 μm using conventional mechanical polishing. Using micro-Raman spectroscopy, the residual stress in the bonded LN film in this trilayered (LN/SiO2/Si) structure was investigated. The measured residual tensile stress in the LN film layer was approximately 155 MPa, which was similar to the value calculated by stress analysis. This study will be useful for the development of various hetero-integrated LN micro-devices, including silicon-based, LNOI-integrated photonic devices.
3 July 2017 in Japanese Journal of Applied Physics
This paper focuses on the bonding interface of LiNbO 3 and Si wafers bonded by laser irradiation. The nanostructure and composite distribution across the bonding interface were investigated. The experimental interface analysis showed that no cracks or voids were formed at the nanolevel. It was also found that the bonding interface had a disordered amorphous layer containing Nb, O, and Si. This indicates that a strong bond was achieved because fusion bonding proceeded at the interface between LiNbO 3 and Si. In addition, the effectiveness of this bonding method for the wafer-level bonding of LiNbO 3 and Si was demonstrated.
An InP substrate was directly bonded on a diamond heat spreader for efficient heat dissipation. The InP surface activated by oxygen plasma and the diamond surface cleaned with an NH3/H2O2 mixture were contacted under atmospheric conditions. Subsequently, the InP/diamond specimen was annealed at 250 °C to form direct bonding. The InP and diamond substrates formed atomic bonds with a shear strength of 9.3 MPa through an amorphous intermediate layer with a thickness of 3 nm. As advanced thermal management can be provided by typical surface cleaning processes followed by low-temperature annealing, the proposed bonding method would facilitate next-generation InP devices, such as transistors for high-frequency and high-power operations.