In the present study, two main parameters as stirring duration and casting temperature were taken into consideration in order to determine the effect of stirring process on mechanical properties of aluminum matrix composites. AlSi7Mg0.3 aluminum alloy and silicon carbide (SiC) particles were used as matrix and reinforcement materials to produce composite samples. Firstly, stirring processes were applied as the combination of mechanical stirring and ultrasonic vibration for the various time as 3-1, 2-2 and 1-3 minutes, respectively. To determine the effect of stirring process, tensile tests were applied to whole samples and Quality Indexes (QI) were calculated by using the results of tensile tests. According to the values of QI, the produced samples with the combination of 1 minute mechanical stirring and 3 minutes ultrasonic vibration showed the maximum mechanical properties. Afterwards, the determined stirring combination was chosen to specify the appropriate molten metal temperature. Three different casting temperatures were addressed as 700˚C, 720˚C and 740˚C. According to mechanical tests results and calculations of QI and metallographic analysis, the maximum mechanical properties were obtained with aluminum composite reinforced with 1 wt. % SiC at 720˚C molten metal temperature by applying 1 minute mechanical stirring and 3 minutes ultrasonic vibration.
31 December 2020 in International Journal of Automotive Science And Technology
The aim of this study is to investigate the effect of ultrasonic treatment on the microstructural and mechanical properties of A356 aluminum al-loy. Ultrasonic treatment was applied to 2 kg and 4 kg molten metals at different melting temperatures (700 oC, 720 oC and 740 oC) for different durations (0, 60, 180 and 300 seconds). Bifilm indices of the samples were also measured after all parameters were tested. The ultimate tensile strength (UTS) and elongation values were used to calculate the Quality Index (QI) of the samples. According to the results, the amount of liquid metal directly affects the the ultrasonic intensity that is produced during the treatment. Maximum UTS and elongation results were determined at 720 oC during 300 seconds for 4 kg casting. Minimum bifilm density val-ue was measured at the same ultrasonic temperature and time.
27 September 2021 in Celal Bayar Üniversitesi Fen Bilimleri Dergisi
It is well-known that strontium addition into molten metal as a eutectic modifier increases the elongation and toughness values of the cast parts by refining the eutectic phases. However, when over-modification occurs, porosity increases due to some unwanted physical and chemical reactions that develop within the structure. On the other hand, it has been seen that high cooling rates tend to reduce the porosity of the alloy, decrease grain size and secondary dendrite arm spacing and refine eutectic silicon phase on Al-Si casting alloys. Within the scope of this project, it is aimed to investigate the effects of the cooling rate of cast part and the addition amount of strontium on the silicon modification behavior of Al A356 (AlSi7Mg) alloy parts using casting simulation environment. In order to examine the effect of strontium addition, 150, 250, 350 and 450 parts per million of strontium additions were chosen based on thermodynamic calculations. After the casting session of each Al A356 composition with different strontium amount by using special designed 5-spoke mold on casting simulation, thermal analysis was done by obtained thermocouple data from casting part’s each spoke. Obtained thermal analysis data was interpreted with the casting simulation outputs. Within all aspects, the 150 parts per million strontium addition on Al A356 alloy has been identified as the most useful simulation model in terms of casting performance.