Purpose: The purpose of this study is to investigate the effect of electron beam surface melting (EBSM) on the properties of Plasma Transfer Arc (PTA) deposited Stellite 12 hardfacing.Design/methodology/approach: For this purpose, structural characterization and dry sliding wear tests have been conducted on the hardfacings at room temperature. The wear tracks formed on the surfaces of the hardfacings were examined by a stylus-type profilometer and a scanning electron microscope.Findings: Refinement of the matrix and the carbides following EBSM process led to about 15 per cent increment in hardness as compared to PTA state. Despite an increase in the surface hardness, EBSM’ed hardfacing exhibited about 50 per cent lower sliding wear resistance than PTA hardfacing against alumina ball. According to the worn surface examinations, reduction in the wear resistance of Stellite 12 after EBSM process has been associated with the extensive refinement of the carbides which made them easier to be removed from the matrix during the sliding contact.Originality/value: The authors of current study have applied EBSM to PTA deposited Stellite 12 hardfacing alloy to investigate if the surface structure and properties could be improved. More specifically the dry sliding wear performance of PTA and EBSM’ed hardfacings have been focused in the scope of this study. To the best of the authors’ knowledge, this approach, i.e. use of EBSM as a post deposition treatment of Stellite 12 hardfacings, has not been reported in open literature.
Aiming at additional improvements in the properties of Stellite 12 PTA hardfacing alloy deposited on 4140 steel substrate, the authors have adopted a dual approach. During PTA deposition Stellite 12 hardfacing powder was alloyed with 10 wt-% Mo, followed by laser surface melting (LSM). Addition of 10 wt-% Mo, led to an increase in the volume fraction of Co and W-rich complex carbides. Later on LSM executed on the PTA led to the development of unique microstructure near the surface, characterised by the segregation of hard Cr-rich carbides. The resultant layers were subjected to mechanical characterisation, at room temperature, e.g. hardness and wear resistance. It was concluded that combining both approaches i.e. addition of Mo during the hardfacing process followed by LSM of deposited layer gave additional improvements in mechanical properties owing to evolution of a unique carbide structure.