Koichi Kakimoto

Dr. Koichi Kakimoto


Research Focus & Metrics

Academic Career Length

4Years (2023-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
8 June 2023 in Crystals
Verified
Journal Article
Open access
PDF file
KKKei Kamada
Kei Kamada
RSRei Sasaki
Rei Sasaki
TTTaketoshi Tomida
Taketoshi Tomida
ITIsao Takahashi
Isao Takahashi
MYMasao Yoshino
Masao Yoshino
AYAkira Yoshikawa
Akira Yoshikawa
β-Ga2O3 is a well-known semiconductor material for power devices and other applications. Recently, β-Ga2O3 has also been reported as a scintillator material with a light yield of approximately 8400 ph./MeV, scintillation decay time of <1 μs, and density of 6.44 g/cm3. In this study, 45 cm diameter β-Ga2O3 single crystals were prepared via oxide crystal growth using the cold crucible (OCCC) method under various oxygen partial pressures. In the OCCC method, as in the cold crucible method, a high frequency is applied directly to the oxide materials, which are heated and melted, and the melt is held by the outermost solid material itself that is cooled by water using a copper hearth. In the OCCC method, crystal growth is performed while rotating the seed crystal, as in the Czochralski method, to increase the crystal diameter. The optical properties and radiation responses of the crystals grown under various oxygen partial pressures were evaluated.

1 May 2023 in Preprints.org
Verified
Preprint
Open access
PDF file
KKKei Kamada
Kei Kamada
RSRei Sasaki
Rei Sasaki
TTTaketoshi Tomida
Taketoshi Tomida
ITIsao Takahashi
Isao Takahashi
MYMasao Yoshino
Masao Yoshino
AYAkira Yoshikawa
Akira Yoshikawa
β-Ga2O3 is a well-known semiconductor material for power devices and other applications. Recently, β-Ga2O3 has also been reported as a scintillator material with a light yield of approximately 8400 ph./MeV, scintillation decay time of <1 μs, and density of 6.44 g/cm3. In this study, 2-inch diameter β-Ga2O3 single crystals were prepared by oxide crystal growth using the cold crucible (OCCC) method under various oxygen partial pressures. In the OCCC method, as in the cold crucible method, a high frequency is applied directly to the oxide materials, which are heated and melted, and the melt is held by the outermost solid material itself that is cooled by water using a copper hearth. In the OCCC method, crystal growth is performed while rotating the seed crystal, as in the Czochralski method, to increase the crystal diameter. The optical properties and radiation responses of the crystals grown under various oxygen partial pressures were evaluated.